Effect of Carrier Modification on Reforming to Produce Hydrogen of Ethanol Steam Catalyzed by Ni/La2O2CO3 AITranslate
Abstract AITranslate
Zn and Ca were respectively used to modify and compound La2O2CO3 carrier,and then the catalysts of Ni/La2O2CO3(NL),Ni/La2O2CO3-ZnO(NLZ)and Ni/La2O2CO3-CaO(NLC)were prepared to catalyze reforming of ethanol steam to produce hydrogen.The crystal phase,specific surface area and comprehensive performance of the catalysts were analyzed by XRD,BET and temperature programmed reduction(TPR).The results show that compared with NL,the ethanol conversion rates of NLC and NLZ at 300℃are increased by 24.3%and 20.8%,respectively.NLC has the best low-temperature catalytic activity.The H2 selectivity of NLC and NLZ is higher than that of NL,increased by 15.23%and 14.04%respectively at 600℃.In the range of 400~700℃,the H2 selectivity of NLC is higher than that of NLZ,while the selectivity of CO2,CO and CH4 is lower than that of NLZ.NLC can better inhibit Ni coalescence and deactivation at high temperature,thus improving the efficiency of Ni catalysis for hydrogen production.
KeyWords AITranslate
1邓宇,秦疆洲,赵文军,喻兰兰,胡霞.二维生物质炭纳米片材料的合成研究进展[J].合成化学,2020,28(6):558-567. 被引量:1
2刘军瑜,肖周荣,张香文.Ru改性Ni/Ce0.8Pr0.2O2催化剂用于乙醇水蒸气重整制氢研究[J].现代化工,2019,39(7):162-166. 被引量:1
3李亮荣,丁永红,王飞,欧阳红霞,曾晶晶,孙戊辰.乙醇水蒸气重整制氢双金属催化剂Ni-Co/La_2O_2CO_3的研究[J].应用化工,2013,42(5):866-869. 被引量:7
4刘承伟,石秋杰,李彬,谌伟庆.不同载体对钌基催化剂催化乙醇水蒸气重整制氢性能的影响[J].中国稀土学报,2009,27(1):19-24. 被引量:6
5杨欢,何素芳,王云珠,罗永明.Ni-CaO-La2O3催化剂在乙醇水蒸气重整制氢中的应用[J].石油化工,2020,49(2):107-112. 被引量:3
1方书起,王毓谦,李攀,陈志勇,陈玮,白净,常春.生物油催化重整制氢研究进展[J].化工进展,2022,41(3):1330-1339. 被引量:2
2李亮荣,丁永红,邓志伟,刘艳,彭建,倪智超,熊磊.La、Ce等稀土改性重整制氢催化剂的研究进展[J].稀有金属与硬质合金,2022,50(2):45-49. 被引量:2
3李亮荣,彭建,付兵,黄玉林,姜慧,齐海霞.碳中和愿景下绿色制氢技术发展趋势及应用前景分析[J].太阳能学报,2022,43(6):508-520. 被引量:7
4李亮荣,刘艳,杨小喆,孙戊辰,邓志伟,陈镇,李炜娟.稀土改性非贵金属重整制氢催化剂载体的研究进展[J].应用化工,2023,52(4):1270-1275.
1吴珺,郭文涛,刘欣坤,赵增武,刘宝玉.温度对La_(2)O_(3)-SiO_(2)-CaO-Al_(2)O_(3)-MgO系高温熔体结构的影响[J].稀有金属与硬质合金,2022,50(6):52-58.
2王一涵.信息与通信技术在碳达峰碳中和战略中的应用研究[J].石河子科技,2023(1):46-48.
3牛永红,钱相儒,刘峥,李义科.载铈白云石基黏土陶催化松木气化研究[J].燃料化学学报(中英文),2023,51(3):340-347.
4郭旭宁,李云玲,闫佳铭,刘为锋.“双碳”战略下水循环响应与需水情势变化[J].南水北调与水利科技(中英文),2023,21(1):22-28.
5李果,张安东,万震,李志合,王绍庆,李宁,张鹏.生物油及其衍生物催化重整制氢研究进展[J].燃料化学学报(中英文),2023,51(4):444-457.
6李艳,李卓,刘恩周.NiMoO_(4)/ZnIn_(2)S_(4)S-scheme异质结的制备及光催化产氢性能增强机制[J].聊城大学学报:自然科学版,2023,36(2):1-10.
7李亮荣,梁娇,彭建,艾盛,齐海霞.基于MOFs材料光催化分解水制氢的研究进展[J].精细化工,2023,40(3):553-564.
8钟鸣.中国绿色制氢关键技术发展现状及展望[J].现代化工,2023,43(4):13-17. 被引量:1
9赵天寿,蒋浩然,李文甲.流体电池的化学工程科学问题[J].中国科学基金,2023,37(2):170-177.
10汤雪腾,马已青,史兴华,裘鹏,黄晓明,赵彪.基于软换流控制的直流变压器黑启动研究[J].浙江电力,2023,42(6):14-22.
1范思强,吴子明,朱化雷,孙士可,白振民.生物质原料加氢裂化生产高附加值燃料技术研究进展[J].工业催化,2021,29(8):13-18.
2张倩,温月丽,王斌,范鹤鸣,杨晨,宋镕鹏,张维中,黄伟.双配体CuFe@MOFs材料为前驱体的催化剂的组分调控对CO_(2)加氢制C_(2+)醇性能的影响[J].无机化学学报,2021,37(8):1390-1398. 被引量:2
3吴彦霞,王献忠,梁海龙,陈鑫,陈琛,戴长友,陈玉峰.钾盐沉积对VMoTi催化剂脱硝性能的影响[J].稀有金属材料与工程,2021,50(7):2343-2351. 被引量:2
4颜再荣,苗超,刘庆贺,韩菲,欧阳静.Ni-Ru/TiO_(2)-凹凸棒石复合材料的制备及其CO_(2)甲烷化性能[J].硅酸盐学报,2021,49(7):1377-1384. 被引量:2
5李剑,何思达,楚爽,刘近,吴冰峰,佟岩,杨丽娜,白金.纳米微晶纤维素辅助合成加氢脱芳催化剂[J].高校化学工程学报,2021,35(4):675-682. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TQ426.65[化学工程]
Citation Information:
Zn and Ca were respectively used to modify and compound La2O2CO3 carrier,and then the catalysts of Ni/La2O2CO3(NL),Ni/La2O2CO3-ZnO(NLZ)and Ni/La2O2CO3-CaO(NLC)were prepared to catalyze reforming of ethanol steam to produce hydrogen.The crystal phase,specific surface area and comprehensive performance of the catalysts were analyzed by XRD,BET and temperature programmed reduction(TPR).The results show that compared with NL,the ethanol conversion rates of NLC and NLZ at 300℃are increased by 24.3%and 20.8%,respectively.NLC has the best low-temperature catalytic activity.The H2 selectivity of NLC and NLZ is higher than that of NL,increased by 15.23%and 14.04%respectively at 600℃.In the range of 400~700℃,the H2 selectivity of NLC is higher than that of NLZ,while the selectivity of CO2,CO and CH4 is lower than that of NLZ.NLC can better inhibit Ni coalescence and deactivation at high temperature,thus improving the efficiency of Ni catalysis for hydrogen production.
quote
| GB/T 7714-2015 | [1] LI Liang-rong, SUN Wu-chen, CHEN Zu-jie, et al. Effect of Carrier Modification on Reforming to Produce Hydrogen of Ethanol Steam Catalyzed by Ni/La2O2CO3[J]. Rare Metals and Cemented Carbides, 2021(4): 50-54. |
| MLA | [1] LI Liang-rong, et al., "Effect of Carrier Modification on Reforming to Produce Hydrogen of Ethanol Steam Catalyzed by Ni/La2O2CO3." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 50-54. |
| APA | [1] LI Liang-rong, SUN Wu-chen, CHEN Zu-jie, & QI Hai-xia. (2021). Effect of Carrier Modification on Reforming to Produce Hydrogen of Ethanol Steam Catalyzed by Ni/La2O2CO3. Rare Metals and Cemented Carbides(4), 50-54. |
| IEEE | [1] LI Liang-rong, SUN Wu-chen, CHEN Zu-jie, and QI Hai-xia, "Effect of Carrier Modification on Reforming to Produce Hydrogen of Ethanol Steam Catalyzed by Ni/La2O2CO3," Rare Metals and Cemented Carbides, no. 4, pp. 50-54, 2021. keywords: {Ni catalyst;LaOCOcarrier;modification and compounding;ethanol steam;hydrogen production;ZnO;CaO} |