Application and Research Progress of WO3-Based Composite Materials in Photocatalysis AITranslate
Abstract AITranslate
The development and use of fossil energy not only promote the development of global economy,but also bring two major crises to human beings: environmental pollution and energy exhaustion. Based on this,the use of new energy,looking for green and efficient new energy conversion technology has become the focus of research. Photocatalysis,as a new green energy conversion technology,converts solar energy into chemical energy that can be directly used,which has been widely concerned by researchers. The principle of this technology is put forward by the solid energy band theory,that is,when the light with energy greater than the semiconductor band gap shines on the surface of the catalyst,the electrons in the valence band will be excited to jump to the conduction band,leaving a hole in the valence band. These holes and electrons can directly with the target molecule,can also with the catalyst surface adsorption of O2 and H2O or OH − reaction,generate reactive free radicals,and participate in the reaction. Due to the direct use of solar energy,photocatalytic technology has low consumption,clean and other innate advantages. At present,this technology has shown great application potential in the purification of environmental pollutants and the development of clean energy. In order to obtain higher conversion efficiency,the research on catalytic mechanism and structural modification of materials has become a hot topic in physical chemistry,materials science and environmental chemistry. The low e-h separation efficiency of catalyst materials is the main bottleneck hindering the practical application of photocatalytic technology. Among them,the construction of composite materials is considered to be one of the most effective ways to develop highly active photocatalysts. On the one hand,the composite catalyst can combine the advantages of different materials into one,thus significantly expanding its application range. On the other hand,the carrier can migrate to the surface of different components,which can effectively improve the separation efficiency of photogenerated charge through physical isolation.Among many semiconductor materials,tungsten trioxide (WO3) is popular because of its good visible light response (band gap around 2.70 eV) and excellent valence band hole oxidation ability. Driven by the pursuit of higher hole efficiency,a large number of WO3 based composite photocatalysts have been constructed and reported,and their applications cover many fields. In order to make the design and application of WO3 based composite photocatalytic materials more rational development,and to provide useful reference for peers,it is urgent to summarize and review relevant studies regularly. In this paper,the application and research progress of WO3 based composite in photocatalysis in recent years are systematically summarized. Starting from structural characteristics of WO3 itself,around the composite preparation methods and the characteristics of composite material structure and performance of structure-activity relationship between two hot issues were summarized,and finally expounds the existing WO3 based composite photocatalyst in the decomposition of aquatic product hydrogen,CO2 reduction,nitrogen fixation,and the application of pollutants removal in areas such as the status quo,and the prospects of the development prospect was put forward.
KeyWords AITranslate
[1]吴健豪,赵婉,陈默,刘纯希,陈金超,陈智.无铅卤化物钙钛矿可见光催化研究进展 [J].稀有金属,2022,46(1):96.
J H Wu,W Zhao,M Chen,C X Liu,J C Chen,Z Chen. Recent advance in visible-light-driven photocatalysis on lead-free halide perovskites[J].Chinese Journal of Rare Metals,2022,46(1):96.
[2]崔玉民,李慧泉,凡素华,苗慧,田志祥,郏青峰. (BiO)2CO3光催化剂的制备及性能[J].稀有金属,2014,38(6):1066.
Y M Cui,H Q Li,S H Fan,S Miao,Z X Tian,Q F Jia. Preparation and properties of (BiO)2CO3 photocatalyst[J].Chinese Journal of Rare Metals,2014,38(6):1066.
[3]孙为朋,孙明东,陈伟华,刘郁,刘继忠,李兴国. 基于Autoform Sigma的汽车门内板生产稳定性与材料性能的关系[J].锻压技术,2023,48(2):85.
W P Sun,M D Sun,W H Chen. Y Liu,J Z Liu,X G Li. Relationship between production stability and material properties on automobile door inner panel based on Autoform Sigma[J].Forging & Stamping Technology,2023,48(2):85.
[4]刘国彬,陈紫微,顾胡维,孟庆坤,戚继球.变形处理对Zn-0.75Cu-0.15Ti合金组织和力学性能的影响 [J].铜业工程,2023,(1):28.
G B Liu,Z W Chen,H W Gu,Q K Meng,J Q Qi. Microstructure and mechanical properties of Zn-0.75Cu-0.15Ti alloy with different deformation treatments[J].Copper Engineering,2023,(1):28.
[5]Claudino C H,Kuznetsova M,Rodrigues B S,Chen C Q,Wang Z Y,Sardela M, Souza J S. Facile one-pot microwave-assisted synthesis of tungsten-doped BiVO4/WO3 heterojunctions with enhanced photocatalytic activity[J].Materials Research Bulletin,2020,125:110783.
[6]祁凯,张兵,赵田丽,杨艳,张志娟,王快社,蔡军.热处理对Cu/Ti层状异质结构复合材料组织及力学性能的影响 [J].塑性工程学报,2023,30(2):160.
K Qi,B Zhang,T L Zhao,Y Yang,Z J Zhang,K S Wang,J Cai. Effect of heat treatment on microstructure and mechanical properties of Cu/Ti laminated hetero-structure composites[J].Journal of Plasticity Engineering,2023,30(2):160.
[7]Wang J,Zhang Y N,Wang X X,Su X. Simultaneous enhancements in photoactivity and anti-photocorrosion of Z-scheme Mn0.25Cd0.75S/WO3 for solar water splitting[J].Applied Catalysis B:Environmental,2020,268:118444.
[8]Alaghmandfard A,Ghandi K. A comprehensive review of graphitic carbon nitride (g-C3N4)–metal oxide-based nanocomposites:potential for photocatalysis and sensing[J].Nanomaterials,2022,12(2):294.
[9]Jiang Z C,Cheng B,Zhang Y,Wageh S,Al-Ghamdi Ahmed A,Yu J G,Wang L X. S-scheme ZnO/WO3 heterojunction photocatalyst for efficient H2O2 production[J].Journal of Materials Science & Technology,2022,124:193.
[10]He D Y,Wang C,Zhao R,Lu X F,Yang M,Qiu J,Wang K Z,Wang C. BiOX (X=Cl,Br,I)/WO3/polyacrylonitrile nanofibrous membranes for diagnostic X-ray shielding and visible-light photocatalysis[J].ACS Applied Nano Materials,2022,5(3):4157.
[11]Arunachalam P. Synthesis of BiFeWO6/WO3 nanocomposite and its enhanced photocatalytic activity towards degradation of dye under irradiation of light[J].Colloids and Surfaces A:Physicochemical and Engineering Aspects,2018,559:83.
[12]Cui Y P,Shang Y R,Shi R,Wang Z Y,Zhu Y N,Yang P. Boosting photoelectrochemical and photocatalytic performances of electronspun WO3 nanofibers by combining with biphase-Ag2WO4[J].Materials Science in Semiconductor Processing,2020,120:105285.
[13]Vemuri R S,Bharathi K K,Gullapalli S K. Effect of structure and size on the electrical properties of nanocrystalline WO3 films[J].ACS Applied Materials & Interfaces,2010,2(9):2623.
[14]Shandilya P,Sambyal S,Sharma R,Mandyal P,Fang B Z. Properties,optimized morphologies,and advanced strategies for photocatalytic applications of WO3 based photocatalysts[J].J Hazard Mater,2022,428:128218.
[15]Sun D Y,Yan G Q. Research progress in preparation and properties of anatase titanium dioxide/carbon composites by hydrothermal method[J].Synthetic Chemistry,2020,28(1):78.
[16]Wei Y L,Huang Y F,Fang Y,Zhao Y Z,Luo D,Guo Q Y,Fan L Q,Wu J H. Hollow mesoporous TiO2/WO3 sphere heterojunction with high visible-light-driven photocatalytic activity[J].Materials Research Bulletin,2019,119:110571.
[17]Cui L F,Ding X,Wang Y G,Shi H C,Huang L H,Zuo Y H,Kang S F. Facile preparation of Z-scheme WO3/g-C3N4 composite photocatalyst with enhanced photocatalytic performance under visible light[J].Applied Surface Science,2017,391:202.
[18]Priyadharsan A,Vasanthakumar V,Shanavas S,Karthikeyan S,Anbarasan P M. Crumpled sheet like graphene based WO3-Fe2O3 nanocomposites for enhanced charge transfer and solar photocatalysts for environmental remediation[J].Applied Surface Science,2019,470:114.
[19]Song B,Wang T T,Sun H G,Shao Q,Zhao J K,Song K K,Hao L H,Wang L,Guo Z H. Two-step hydrothermally synthesized carbon nanodots/WO3 photocatalysts with enhanced photocatalytic performance[J].Dalton Trans,2017,46(45):15769.
[20]Mersal M,Mohamed G G,Zedan A F. Promoted visible-light-assisted oxidation of methanol over N-doped TiO2/WO3 nanostructures[J].Optical Materials,2021,122:111810.
[21]Tran V A,Nguyen T P,Le V T. Excellent photocatalytic activity of ternary Ag@WO3@rGO nanocomposites under solar simulation irradiation[J].Journal of Science:Advanced Materials and Devices,2021,6(1):108.
[22]Li J,Du X h,Yao L,Zhang Y C. Synthesis of SnS2/WO3 nanocomposite with enhanced photocatalytic activity[J].Materials Letters,2014,121:44.
[23]He F,Yan G Q. Progress in preparation and properties of spinel ferrite hollow nanospheres by hydrothermal method[J].Synthetic Chemistry,2015,23(12):1178.
[24]Das S,Srivastava V C. An overview of the synthesis of CuO-ZnO nanocomposite for environmental and other applications[J].Nanotechnology Reviews,2018,7(3):267.
[25]Malefane M E,Feleni U,Kuvarega A T. A tetraphenylporphyrin/WO3/exfoliated graphite nanocomposite for the photocatalytic degradation of an acid dye under visible light irradiation[J].New Journal of Chemistry,2019,43(28):11348.
[26]Wang G Y,Wu C C,Song B J,Wang Y. Synthesis and photocatalylic activity of SrCu2O2 for water decomposition to hydrogen[J].Advanced Materials Research,2011,239-242:2914.
[27]Shin D,Lee D H,Lee C G,Park K. Synergistic Effects of fluorine and WO3 nanoparticles on the surface of TiO2 hollow spheres for enhanced photocatalytic activity under visible light irradiation[J].ACS Omega,2021,6(46):30942.
[28]Zhang Z Y,Zhu Q J,Ding J,Dai W L,Zong B N. Effect of support on the structural evolution and catalytic performance of WO3-supported catalysts in the synthesis of adipic acid[J].Acta Physico-Chimica Sinica,2014,30(8):1527.
[29]Palanisamy G,Bhuvaneswari K,Bharathi G,Nataraj D,Pazhanivel T. Enhanced photocatalytic properties of ZnS-WO3 nanosheet hybrid under visible light irradiation[J].Chemistry Select,2018,3(32):9422.
[30]邹爽,赵金松,陈驰. 静电纺丝技术的影响因素及应用研究综述[J].河南科技,2019,(5):75.
S Zou,J S Zhao,C Chen. Review on the influencing factors and application of electrospinning technology[J].Henan Science and Technology,2019,(5):75.
[31]Liu Y,Ding H,Si D C. A review on preparation of catalyst layers for proton exchange membrane fuel cell by electrospinning[J].The Electrochemical,2018,24(6):639.
[32]Bachs-herrera A,YousefzadE O,Del valle L J. Melt electrospinning of polymers:blends,nanocomposites,additives and applications[J].Applied Sciences,2021,11(4):1808.
[33]Han X,Yao B,Li K,Zhu W J,Zhang X Y. Preparation and photocatalytic performances of WO3/TiO2 composite nanofibers[J].Journal of Chemistry,2020,2020:1.
[34]Wei L J,Zhang H M,Cao J. Electrospinning of Ag/ZnWO4/WO3 composite nanofibers with high visible light photocatalytic activity[J].Materials Letters,2019,236:171.
[35]Rong F,Wang Q Y,Lu Q F. Rational fabrication of hierarchical Z-scheme WO3/Bi2WO6 nanotubes for superior photoelectrocatalytic reaction[J].ChemistrySelect,2019,4(9):2676.
[36]Zhou M,Tian X M,Yu H,Wang Z H,Ren C G,Zhou L M,Lin Y W,Dou L. WO3/Ag2CO3 mixed photocatalyst with enhanced photocatalytic activity for organic dye degradation[J].ACS Omega,2021,6(40):26439.
[37]周梅,田雪梅,王中华. WO3/Ag3PO4复合物的制备及其光催化性能研究[J].西华师范大学学报(自然科学版),2022,43(3):301.
M Zhou,X M Tian,Z H Wang. Preparation and photocatalytic properties of WO3/Ag3PO4 composites[J].Journal of China West Normal University (Natural Science Edition),2022,43(3):301.
[38]Omrani N,Nezamzadeh-Ejhieh A. A novel quadripartite Cu2O-CdS-BiVO4-WO3 visible-light driven photocatalyst:brief characterization and study the kinetic of the photodegradation and mineralization of sulfasalazine[J].Journal of Photochemistry and Photobiology A:Chemistry,2020,400:112726.
[39]Isari A A,Mehregan M,Mehregan S,Hayati Farzan,Kalantary R R,Kakavandi B. Sono-photocatalytic degradation of tetracycline and pharmaceutical wastewater using WO3/CNT heterojunction nanocomposite under US and visible light irradiations:a novel hybrid system[J].J Hazard Mater,2020,390:122050.
[40]Cordero-Garcia A,Palomino G,Hinojosa-Reyes L,Guzmán-Mar J,Maya-Teviño L,Hernández-Ramírez A. Photocatalytic behaviour of WO3/TiO2-N for diclofenac degradation using simulated solar radiation as an activation source[J].Environ Sci Pollut Res Int,2017,24(5):4613.
[41]Sangchay W. WO3-doped TiO2 coating on charcoal activated with increase photocatalytic and antibacterial properties synthesized by microwave-assisted sol-gel method[J].Journal of Nanotechnology,2017,2017:1.
[42]Luévano-Hipólito E,Martínez-de L A C A,López-Cuellar E,Yu Q L,Brouwers H J H. Synthesis,characterization and photocatalytic activity of WO3/TiO2 for NO removal under UV and visible light irradiation[J].Materials Chemistry and Physics,2014,148(1–2):208.
[43]Dong Y Z,Xue Y S,Yang W W,You H M,Su Y. Visible light driven CdS/WO3 inverse opals with enhanced RhB degradation activity[J].Colloids and Surfaces A:Physicochemical and Engineering Aspects,2019,561:381.
[44]Zhang S,Wang J M,Chen S T,Li R J,Peng T Y. Construction of Ag2S/WO3 direct Z-Scheme photocatalyst for enhanced charge separation efficiency and H2 generation activity[J].Industrial & Engineering Chemistry Research,2019,58(32):14802.
[45]Mao J,Li P W,Wang J M,Wang H T,Zhang Q,Zhang L X,Li H,Zhang W,Peng T. Insights into photocatalytic inactivation mechanism of the hypertoxic site in aflatoxin B1 over clew-like WO3 decorated with CdS nanoparticles[J].Applied Catalysis B:Environmental,2019,248:477.
[46]Li H,Zhang Y L,Zhang Q,Wang Y F,Fan Y P,Gao X,Niu J. Boosting visible-light photocatalytic degradation of indomethacin by an efficient and photostable Ag3PO4/NG/WO3 composites[J].Applied Surface Science,2019,490:481.
[47]Shi H X,Yang S Z,Han C,Niu Z J,Li H S,Huang X B,Ma J C. Fabrication of Ag/Ag3PO4/WO3 ternary nanoparticles as superior photocatalyst for phenol degradation under visible light irradiation[J].Solid State Sciences,2019,96:105967.
[48]Li Q Y,Wang F L,Hua Y X,Luo Y T,Liu X H. Deposition-precipitation preparation of Ag/Ag3PO4/WO3 nanocomposites for efficient visible-light degradation of rhodamine B under strongly acidic/alkaline conditions[J].J Colloid Interface Sci,2017,506:207.
[49]Jian J X,Sun J W. A review of recent progress on silicon carbide for photoelectrochemical water splitting[J].Solar RRL,2020,4(7):111.
[50]Fakhri H,Bagheri H. Highly efficient Zr-MOF@WO3/graphene oxide photocatalyst:synthesis,characterization and photodegradation of tetracycline and malathion[J].Materials Science in Semiconductor Processing,2020,107:104815.
[51]Nawaz A,Goudarzi S,Zarrin H,Saravanan P. S-scheme/type-1 heterostructure stimulated WO3/g-C3N4-WS2 ternary photocatalyst with improved charge transfer mechanism for full solar spectrum photocatalysis[J].Journal of Alloys and Compounds,2022,903:163951.
[52]Wu W,Ma X D,Li D,Xuan Y W,Meng S C,Chen M. Assembly of WO3 nanosheets/Bi24O31Br10 nanosheets composites with superior photocatalytic activity for degradation of tetracycline hydrochloride[J].Journal of Materials Science,2018,53(23):15804.
[53]Han W M,Wu T,Wu Q S. Fabrication of WO3/Bi2MoO6 heterostructures with efficient and highly selective photocatalytic degradation of tetracycline hydrochloride[J].J Colloid Interface Sci,2021,602:544.
[54]Xu T,Wang Y,Zhou X F,Zheng X L,Xu Q,Chen Z M,Ren Y M,Yan B. Fabrication and assembly of two-dimensional TiO2/WO3·H2O heterostructures with type II band alignment for enhanced photocatalytic performance[J].Applied Surface Science,2017,403:564.
[55]Markhabayeva A A,Moniruddin M,Dupre R. Designing of WO3@Co3O4 heterostructures to enhance photoelectrochemical performances[J].J Phys Chem A,2020,124(3):486.
[56]Wei P C,Wen Y,Lin K F,Li X. 2D/3D WO3/BiVO4 heterostructures for efficient photoelectrocatalytic water splitting[J].International Journal of Hydrogen Energy,2021,46(54):27506.
[57]Ma H Q,Yang W Y,Gao S,Lin Z F,Mo Z Y,Li C,Shang J K,Li Q. Photoirradiation-induced capacitance enhancement in the h-WO3/Bi2WO6 submicron rod heterostructure under simulated solar illumination and its postillumination capacitance enhancement retainment from a photocatalytic memory effect[J].ACS Appl Mater Interfaces,2021,13(48):57214.
[58]Basumatary B,Basumatary R,Ramchiary A,Konwar D. Evaluation of Ag@TiO2/WO3 heterojunction photocatalyst for enhanced photocatalytic activity towards methylene blue degradation[J].Chemosphere,2022,286(Pt 2):131848.
[59]Akhlaghian F,Najafi A. CuO/WO3/TiO2 photocatalyst for degradation of phenol wastewater[J].Scientia Iranica,2018,0(0)。
[60]Singh P,Priya B,Shandilya P,Raizada P,Singh N,Pare B,Jonnalagadda S B. Photocatalytic mineralization of antibiotics using 60%WO3/BiOCl stacked to graphene sand composite and chitosan[J].Arabian Journal of Chemistry,2019,12(8):4627.
[61]Lee J Y,Jo W K. Heterojunction-based two-dimensional N-doped TiO2/WO3 composite architectures for photocatalytic treatment of hazardous organic vapor[J].Journal of Hazardous Materials,2016,314:22.
[62]Keereeta Y,Thongtem S,Thongtem T. Enhanced photocatalytic degradation of methylene blue by WO3/ZnWO4 composites synthesized by a combination of microwave-solvothermal method and incipient wetness procedure[J].Powder Technology,2015,284:85.
[63]Ali H,Guler A,Masar M. Solid-state synthesis of direct Z-scheme Cu2O/WO3 nanocomposites with enhanced visible-light photocatalytic performance[J].Catalysts,2021,11(2):293.
[64]Chen J Y,Xiao X Y,Wang Y,Ye Z H. Fabrication of hierarchical sheet-on-sheet WO3/g-C3N4 composites with enhanced photocatalytic activity[J].Journal of Alloys and Compounds,2019,777:325.
[65]Wang W Z,Huang H W,Ke X,Liu X,Yang S H,Wang K Q,Huang L,Tu C,Zheng Z Q,Luo D X,Zhang M L. Morphology- and size-dependent FAPbBr3/WO3 Z-scheme photocatalysts for the controllable photo-oxidation of benzyl alcohol[J].Materials & Design,2022,215:110502.
[66]Singh J,Arora A,Basu S. Synthesis of coral like WO3/g-C3N4 nanocomposites for the removal of hazardous dyes under visible light[J].Journal of Alloys and Compounds,2019,808:151734.
[67]Wang L P,Huang T T,Yang G P,Lu C Y,Dong F L,Li Y L,Guan W S. The precursor-guided hydrothermal synthesis of CuBi2O4/WO3 heterostructure with enhanced photoactivity under simulated solar light irradiation and mechanism insight[J].J Hazard Mater,2020,381:120956.
[68]Yao J C,Zhang M,Yin H F,Luo Y T,Liu X H. Improved photocatalytic activity of WO3/C3N4:by constructing an anchoring morphology with a Z-scheme band structure[J].Solid State Sciences,2019,95:105926.
[69]Zheng D Y,Jiang X F,Liu M Y,Zhao X,Wang W C,Sun G Y. Three-dimensional Si/ITO/WO3 photoelectrode with micropost array structure for photocatalysis enhancement[J].IOP Sciences,2017,95:1361.
[70]Wang W C,Chen S Y,Yang P X,Duan C G,Wang L W. Si:WO3 heterostructure for Z-scheme water splitting:an ab initio study[J].J. Mater. Chem. A,2013,1,1078.
[71]Chen J Y,Xiao X Y,Wang Y,Ye Z H. Ag nanoparticles decorated WO3/g-C3N4 2D/2D heterostructure with enhanced photocatalytic activity for organic pollutants degradation[J].Applied Surface Science,2019,467-468:1000.
[72]Jia J K,Jiang C Y,Zhang X R,Li P J,Xiong J X,Zhang Z,Wu T,Wang Y P. Urea-modified carbon quantum dots as electron mediator decorated g-C3N4/WO3 with enhanced visible-light photocatalytic activity and mechanism insight[J].Applied Surface Science,2019,495:143524.
[73]Tahir M,Siraj M,Tahir B,Umer M,Alias H,Othman N. Au-NPs embedded Z–scheme WO3/TiO2 nanocomposite for plasmon-assisted photocatalytic glycerol-water reforming towards enhanced H2 evolution[J].Applied Surface Science,2020,503:5781.
[74]Zhao L Y,Liu Y S,Xi X,Shen Y G,Wang J Y,Liu Y N,Nie Z. Bi/Bi2O3/WO3 composite:a bifunctional plasmonic heterostructure for detection and degradation pollutions in wastewater[J].Journal of Environmental Chemical Engineering,2022,10(3):107643.
[75]Wang Y,Chen D,Hu Y,Qin L,Liang J,Sun X,Huang Y. An artificially constructed direct Z-scheme heterojunction:WO3 nanoparticle decorated ZnIn2S4 for efficient photocatalytic hydrogen production[J].Sustainable Energy & Fuels,2020,4(4):1681.
[76]Fu J,Xu Q,Low J,Jiang C,Yu J. Ultrathin 2D/2D WO3/g-C3N4 step-scheme H2-production photocatalyst[J].Applied Catalysis B:Environmental,2019,243:556.
[77]Liu C,Mao S,Wang H L,Wu Y,Wang F Y,Xia M Z,Chen Q.. Peroxymonosulfate-assisted for facilitating photocatalytic degradation performance of 2D/2D WO3/BiOBr S-scheme heterojunction[J].Chemical Engineering Journal,2022,430:132806.
[78]董永浩,马爱琼,李金叶,李宏飞,高云琴. 热剥离法制备含缺陷g-C3N4纳米片及光催化性能[J].稀有金属,2021,45(1):47.
Y H Dong,A Q Ma,J Y Li,H F Li,Y Q Gao. Preparation of defective g-C3N4 nanosheets by thermal stripping and photocatalytic properties [J].Chinese Journal of Rare Metals,2021,45(1):47.
[79]Akhter P,Hussain M,Saracco G,Russo N. Novel nanostructured-TiO2 materials for the photocatalytic reduction of CO2 greenhouse gas to hydrocarbons and syngas[J].Fuel,2015,149:55.
[80]Zhou W,Guo J K,Shen S,Pan J B,Tang J,Chen L,Au C T,Yin S F. Progress in photoelectrocatalytic reduction of carbon dioxide[J].Acta Physico-Chimica Sinica,2020,36(3):1906048.
[81]Lin N S,Lin Y,Qian X J,Wang X X,Su W Y. Construction of a 2D/2D WO3/LaTiO2N direct Z-Scheme photocatalyst for enhanced CO2 reduction performance under visible light[J].ACS Sustainable Chemistry & Engineering,2021,9(40):13686.
[82]Xie Z K,Xu Y Y,Li D,Chen L J,Meng S C,Jiang D L,Chen M. Construction of CuO quantum Dots/WO3 nanosheets 0D/2D Z-scheme heterojunction with enhanced photocatalytic CO2 reduction activity under visible-light[J].Journal of Alloys and Compounds,2021,858:157668.
[83]Zhang M M,Zhao K,Xiong J Y,Wei Y,Han C,Li W J,Cheng. A 1D/2D WO3 nanostructure coupled with a nanoparticulate CuO cocatalyst for enhancing solar-driven CO2 photoreduction:the impact of the crystal facet[J].Sustainable Energy & Fuels,2020,4(5):2593.
[84]Chen Q,Lan X F,Chen K S,Ren Q Q,Shi J S. Construction of WO3/CsPbBr3 S-scheme heterojunction via electrostatic self-assembly for efficient and long-period photocatalytic CO2 reduction[J].J Colloid Interface Sci,2022,616:253.
[85]Shi W N,Guo X W,Wang J C,Li Y,Liu L,Hou Y X,Li Y,Lou H H. Enhanced photocatalytic 3D/2D architecture for CO2 reduction over cuprous oxide octahedrons supported on hexagonal phase tungsten oxide nanoflakes[J].Journal of Alloys and Compounds,2020,830:154683.
[86]Yee W T,Yien W G,Xin Y K,Ng B J,Yong S T,Chai S P. Fabrication of Bi2WO6/Cu/WO3 all‐solid‐state Z‐scheme composite photocatalyst to improve CO2 photoreduction under visible light irradiation[J].ChemCatChem,2019,11(24):6431.
[87]Tang Z,Wang C,He W. The Z-scheme g-C3N4/3DOM-WO3 photocatalysts with enhanced activity for CO2 photoreduction into CO[J].Chinese Chemical Letters,2022,33(2):939.
[88]Dong Y J,Jiang Y,Liao J F,Chen H Y,Kuang D B,Su C Y. Construction of a ternary WO3/CsPbBr3/ZIF-67 heterostructure for enhanced photocatalytic carbon dioxide reduction[J].Science China Materials,2022,21:1962.
[89]Das R,Sarkar S,Kumar R. Noble-metal-free heterojunction photocatalyst for selective CO2 reduction to methane upon induced strain relaxation[J].ACS Catalysis,2021,12(1):687.
[90]Zhao X F,Yi X B,Zhang J,Liu B X,Yu S M,Liu X C. Z-scheme polyimide/tungsten trioxide aerogel photocatalyst for enhanced photocatalytic CO2 reduction under visible light[J].Nanotechnology,2021,32(31):315714.
[91]Li B,Sun L,Bian J. Controlled synthesis of novel Z-scheme iron phthalocyanine/porous WO3 nanocomposites as efficient photocatalysts for CO2 reduction[J].Applied Catalysis B:Environmental,2020,270:118849.
[92]Raza A,Shen H,Haidry A A. Studies of Z-scheme WO3-TiO2/Cu2ZnSnS4 ternary nanocomposite with enhanced CO2 photoreduction under visible light irradiation[J].Journal of CO2 Utilization,2020,37:260.
[93]Nguyen C T K,Tran N Q,Seo S,Hwang H,Oh S,Yu J M,Lee J S,Le T A,Hwang J,Kim M R,Lee H Y. Highly efficient nanostructured metal-decorated hybrid semiconductors for solar conversion of CO2 with almost complete CO selectivity[J].Materials Today,2020,35:25.
[94]Zhu Z,Huang W R,Chen C Y,Wu R J. Preparation of Pd–Au/TiO2–WO3 to enhance photoreduction of CO2 to CH4 and CO[J].Journal of CO2 Utilization,2018,28:247.
[95]冯亚杰,段有雨,邹函君,马江平,周楷,周小元. 单原子催化剂在光催化分解水制氢中的研究现状[J].稀有金属,2021,45(5):551.
Y J Feng,Y Y Duan,H J Zou,J P Ma,K Zhou,X Y Zhou. Research status of monatomic catalysts in photocatalytic decomposition of water to produce hydrogen[J].Chinese Journal of Rare Metals,2021,45(5):551.
[96]Hong J W,Wi D H,Lee S U,Han S W. Metal-semiconductor heteronanocrystals with desired configurations for plasmonic photocatalysis[J].J Am Chem Soc,2016,138(48):15766.
[97]于晶晶,廖斌,张旭,周福增,伏开虎,吴先映. 热氧化法在泡沫铜上制备CuO纳米线及其光催化性能研究[J].稀有金属,2016,40(10):1021.
J J Yu,B Liao,X Zhang,F Z Zhou,K H Fu,X Y Wu. Preparation of CuO nanowires on copper foam by thermal oxidation and their photocatalytic properties[J].Chinese Journal of Rare Metals,2016,40(10):1021.
[98]Lu Y,Li Y,Wang Y Y,Zhang J Y. Two-photon induced NIR active core-shell structured WO3/CdS for enhanced solar light photocatalytic performance[J].Applied Catalysis B:Environmental,2020,272:118979.
[99]Wang D,Liu J Z,Zhang M,Song Y T,Zhang Z H,Wang J. Construction of ternary annular 2Z-scheme+1heterojunction CuO/WO3/CdS/ photocatalytic system for methylene blue degradation with simultaneous hydrogen production[J].Applied Surface Science,2019,498:143843.
[100]Qian Y T,Yang M K,Zhang F F,Du J M,Li K D,Lin X L,Zhu X R,Lu Y Y,Wang W M,Kang D J. A stable and highly efficient visible-light-driven hydrogen evolution porous CdS/WO3/TiO2 photocatalysts[J].Materials Characterization,2018,142:43.
[101]Tahir M B,Asiri A M,Nabi G,Rafique M,Sagir M. Fabrication of heterogeneous photocatalysts for insight role of carbon nanofibre in hierarchical WO3/MoSe2 composite for enhanced photocatalytic hydrogen generation[J].Ceramics International,2019,45(5):5547.
[102]Oh W-C,Na J D,Biswas M R U D. CVD technique assisted,advanced synthesis of WO3-G composites for enhanced photocatalytic H2 generation under visible light illumination[J].Fullerenes,Nanotubes and Carbon Nanostructures,2019,27(10):762.
[103]Zhang M,Piao C C,Wang D,Liu Z Y,Liu J Z,Zhang Z H,Wang J,Song Y T. Fixed Z-scheme TiO2|Ti|WO3 composite film as recyclable and reusable photocatalyst for highly effective hydrogen production[J].Optical Materials,2020,99:109545.
[104]RamÍrez-Ortega D,Guerrero-Araque D,Acevedo-peÑa P,Lartundo-Rojas L,Zanella R. Effect of Pd and Cu co-catalyst on the charge carrier trapping,recombination and transfer during photocatalytic hydrogen evolution over WO3–TiO2 heterojunction[J].Journal of Materials Science,2020,55(35):16641.
[105]Zhou Y,Sun M,Yu T T,Wang J. 3D g-C3N4/WO3/biochar/Cu2+-doped carbon spheres composites:synthesis and visible-light-driven photocatalytic hydrogen production[J].Materials Today Communications,2022,30:103804.
[106]Mallikarjuna K,Kumar M K,Kim H. Synthesis of oxygen-doped-g-C3N4/WO3 porous structures for visible driven photocatalytic H2 production[J].Physica E:Low-dimensional Systems and Nanostructures,2021,126:114428.
[107]He F,Meng A Y,Cheng B,Ho W K,Yu J G. Enhanced photocatalytic H2-production activity of WO3/TiO2 step-scheme heterojunction by graphene modification[J].Chinese Journal of Catalysis,2020,41(1):9.
[108]Liu D,Zhang S,Wang J M,Peng T Y,Li R J. Direct Z-scheme 2D/2D photocatalyst based on ultrathin g-C3N4 and WO3 nanosheets for efficient visible-light-driven H2 generation[J].ACS Appl Mater Interfaces,2019,11(31):27913.
[109]Bilal T M,Nadeem R K,Asiri A M. Boosting the performance of visible light‐driven WO3/g‐C3N4 anchored with BiVO4 nanoparticles for photocatalytic hydrogen evolution[J].International Journal of Energy Research,2019,43(11):5747.
[110]Gong H M,Hao X Q,Jin Z L,Ma Q X. WP modified S-scheme Zn0.5Cd0.5S/WO3 for efficient photocatalytic hydrogen production[J].New Journal of Chemistry,2019,43(48):19159.
[111]Han X,Xu D Y,An L,Hou C Y,Li Y G,Zhang Q H,Wang H Z. WO3/g-C3N4 two-dimensional composites for visible-light driven photocatalytic hydrogen production[J].International Journal of Hydrogen Energy,2018,43(10):4845.
[112]崔玉民,张文保. WO3/TiO2薄膜光催化降解ARB性能研究[J].稀有金属,2008,32(4):489.
Y M Cui,W B Zhang. Photocatalytic degradation of ARB by WO3/TiO2 thin films[J].Chinese Journal of Rare Metals,2008,32(4):489.
[113]Ibrahim Y O,Gondal M A,Alaswad A,Moqbel R A,Hassan M,Cevik E, Qahtan T F,Dastageer M A,Bozkurt A. Laser-induced anchoring of WO3 nanoparticles on reduced graphene oxide sheets for photocatalytic water decontamination and energy storage[J].Ceramics International,2020,46(1):444.
[114]Mendoza J A,Lee D H,Kang J H. Photocatalytic removal of gaseous nitrogen oxides using WO3/TiO2 particles under visible light irradiation:effect of surface modification[J].Chemosphere,2017,182:539.
[115]Shi R,Zhang Z,Luo F. N-doped graphene-based CuO/WO3/Cu composite material with performances of catalytic decomposition 4-nitrophenol and photocatalytic degradation of organic dyes[J].Inorganic Chemistry Communications,2020,121:108408.
[116]Zhu W Y,Liu J C,Yu S Y,Zhou Y,Yan X L. Ag loaded WO3 nanoplates for efficient photocatalytic degradation of sulfanilamide and their bactericidal effect under visible light irradiation[J].J Hazard Mater,2016,318:407.
[117]Guo R,Han G N,Yan A G,He Y,Su N,Liu X W,Yi T F. Epitaxial growth of metastable phase α-Ag2MoO4 on WO3 surface:visible light-driven photocatalysis,sterilization,and reaction mechanism[J].Journal of Alloys and Compounds,2020,814:152255.
[118]Zheng J J,Chang F,Jiao M Z,Xu Q,Deng B Q,Hu X F. A visible-light-driven heterojuncted composite WO3/Bi12O17Cl2:synthesis,characterization,and improved photocatalytic performance[J].J Colloid Interface Sci,2018,510:20.
[119]Li J J,Weng B,Cai S C,Chen J,Jia P,Xu Y J. Efficient promotion of charge transfer and separation in hydrogenated TiO2/WO3 with rich surface-oxygen-vacancies for photodecomposition of gaseous toluene[J].J Hazard Mater,2018,342:661.
[120]Govindaraj T,Mahendran C,Marnadu R,Mohd S,Manikandan V. S. The remarkably enhanced visible-light-photocatalytic activity of hydrothermally synthesized WO3 nanorods:an effect of Gd doping[J].Ceramics International,2021,47(3):4267.
[121]Wang C,Luo S Y,Liu C Y,Chen C S. WO3 quantum dots enhanced the photocatalytic performances of graphene oxide/TiO2 films under flowing dye solution[J].Inorganic Chemistry Communications,2020,115:107875.
[122]He K L,Shen R C,Hao L,Li Y J,Zhang P,Jiang J Z,Li X. Advances in nanostructured silicon carbide photocatalysts[J].Acta Physico Chimica Sinica,2022,(11):21.
[123]Qi P,Gao X X,Wang J,Liu H M,He D H,Zhang Q J. A minireview on catalysts for photocatalytic N2 fixation to synthesize ammonia[J].RSC Advances,2022,12(3):1244.
[124]Zhang K,Deng L Q,Huang M L,Tu H Y,Kong Z,Liang Z Y,Shao Y L,Hao X P,Wu Y Z. Energy band matching WO3/B-doped g-C3N4 Z-scheme photocatalyst to fix nitrogen effectively[J].Colloids and Surfaces A:Physicochemical and Engineering Aspects,2022,633:127830.
[125]Guo H R,Zhang H T,Zhao J Y,Yuan P F,Li Y Y,Zhang Y ,Li L,Wang S,Song R. Two-dimensional WO3-transition-metal dichalcogenide vertical heterostructures for nitrogen fixation:a photo(electro) catalysis theoretical strategy[J].The Journal of Physical Chemistry C,2022,126(6):3043.
Basic Information:
DOI:10.13373/j.cnki.cjrm.XY22050043
Chinese Library Classification Number:
Citation Information:
The development and use of fossil energy not only promote the development of global economy,but also bring two major crises to human beings: environmental pollution and energy exhaustion. Based on this,the use of new energy,looking for green and efficient new energy conversion technology has become the focus of research. Photocatalysis,as a new green energy conversion technology,converts solar energy into chemical energy that can be directly used,which has been widely concerned by researchers. The principle of this technology is put forward by the solid energy band theory,that is,when the light with energy greater than the semiconductor band gap shines on the surface of the catalyst,the electrons in the valence band will be excited to jump to the conduction band,leaving a hole in the valence band. These holes and electrons can directly with the target molecule,can also with the catalyst surface adsorption of O2 and H2O or OH − reaction,generate reactive free radicals,and participate in the reaction. Due to the direct use of solar energy,photocatalytic technology has low consumption,clean and other innate advantages. At present,this technology has shown great application potential in the purification of environmental pollutants and the development of clean energy. In order to obtain higher conversion efficiency,the research on catalytic mechanism and structural modification of materials has become a hot topic in physical chemistry,materials science and environmental chemistry. The low e-h separation efficiency of catalyst materials is the main bottleneck hindering the practical application of photocatalytic technology. Among them,the construction of composite materials is considered to be one of the most effective ways to develop highly active photocatalysts. On the one hand,the composite catalyst can combine the advantages of different materials into one,thus significantly expanding its application range. On the other hand,the carrier can migrate to the surface of different components,which can effectively improve the separation efficiency of photogenerated charge through physical isolation.Among many semiconductor materials,tungsten trioxide (WO3) is popular because of its good visible light response (band gap around 2.70 eV) and excellent valence band hole oxidation ability. Driven by the pursuit of higher hole efficiency,a large number of WO3 based composite photocatalysts have been constructed and reported,and their applications cover many fields. In order to make the design and application of WO3 based composite photocatalytic materials more rational development,and to provide useful reference for peers,it is urgent to summarize and review relevant studies regularly. In this paper,the application and research progress of WO3 based composite in photocatalysis in recent years are systematically summarized. Starting from structural characteristics of WO3 itself,around the composite preparation methods and the characteristics of composite material structure and performance of structure-activity relationship between two hot issues were summarized,and finally expounds the existing WO3 based composite photocatalyst in the decomposition of aquatic product hydrogen,CO2 reduction,nitrogen fixation,and the application of pollutants removal in areas such as the status quo,and the prospects of the development prospect was put forward.
quote
| GB/T 7714-2015 | [1] Xue Zhang, Qingfeng Dong, Yandong Sun, et al. Application and Research Progress of WO3-Based Composite Materials in Photocatalysis[J]. Chinese Journal of Rare Metals, 2024, 48(9): 1306-1321. DOI:10.13373/j.cnki.cjrm.XY22050043. |
| MLA | [1] Xue Zhang, et al., "Application and Research Progress of WO3-Based Composite Materials in Photocatalysis." Chinese Journal of Rare Metals, vol. 48, no. 9, 2024, pp. 1306-1321, https://doi.org/10.13373/j.cnki.cjrm.XY22050043. |
| APA | [1] Xue Zhang, Qingfeng Dong, Yandong Sun, Ziqi Zhang, Boxiong Shen, & Shengqi Guo. (2024). Application and Research Progress of WO3-Based Composite Materials in Photocatalysis. Chinese Journal of Rare Metals, 48(9), 1306-1321. https://doi.org/10.13373/j.cnki.cjrm.XY22050043 |
| IEEE | [1] Xue Zhang, Qingfeng Dong, Yandong Sun, Ziqi Zhang, Boxiong Shen, and Shengqi Guo, "Application and Research Progress of WO3-Based Composite Materials in Photocatalysis," Chinese Journal of Rare Metals, vol. 48, no. 9, pp. 1306-1321, 2024, doi: 10.13373/j.cnki.cjrm.XY22050043. keywords: {WO;;composite materials;;photocatalysis;;CO reduction;;hydrogen generation;;pollutant degradation} |