Study on Arc Erosion Behavior of a New Type of Ag-Ti_2AlN Electrical Contact Material AITranslate

State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals;State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals,Kunming Institute of precious Metals
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A new type of Ag-Ti2AlN electrical contact materials were prepared by high energy ball milling and powder metallurgy.The arc erosion behavior and mechanism of the contact materials were studied.The surface microstructure of the contact after arc erosion was analyzed by scanning electron microscopy.The results show that Ti2AlN reinforcement has obvious advantages in improving the arc time,arc energy and welding resistance of Ag-matrix electrical contact materials.The average arc time,arc energy and welding strength of Ag-Ti2AlN contacts are 5.61 ms,59.8 mJ and 15 cN respectively in 70 000 on-off cycle tests. Under the action of vapor arc,the corrosion pit centers such as lava and sweat droplets are formed in the cathode of electric contacts.The Ti2 AlN reinforcement particles are fused into the silver melting pool by the diffusion of titanium and aluminum,which can improve the viscosity of the melt,and then enhance the arc erosion resistance.In addition,because of the preferential oxidation mechanism of Al element,the formed Al2O3 absorbs a lot of heat during vaporization,which reduces the mass gain of the anode and the height of the anode bulge,and effectively improves the reliability of electrical contact materials.

KeyWords AITranslate

composite Ag-matrix electrical contact material Ti2 AlN reinforcement electrical conductivity arc erosion

1杨天足,杜作娟,古映莹,邱晓勇,江名喜,楚广.Preparation of flake AgSnO_2 composite powders by hydrothermal method[J].中国有色金属学会会刊:英文版,2007,17(2):434-438. 被引量:7

2闫程科,周延春.Ti_2SnC颗粒增强铜基复合材料的力学性能[J].金属学报,2003,39(1):99-103. 被引量:19

1吴新合,沈涛,杨辉,祁更新,穆成法,陈晓.环保型氧化物增强银基电接触功能复合材料研究进展[J].贵金属,2021,42(1):79-87. 被引量:3

1黄秋玲,李肖瑶,张晓,肖红新.铅试金-重量法测定银钨合金中的银[J].材料研究与应用,2022,16(2):311-315. 被引量:1

2胡钟元,王开旭,周馨,高林辉,李跃.Bi_(2)Sn_(2)O_(7)含量对改性Ag/SnO_(2)电接触复合材料微观结构及性能的影响[J].稀有金属材料与工程,2022,51(10):3808-3818.

3滕汶宋,周晓龙,胡晨,于杰,刘满门,王立惠.ZnO含量对AgCuOIn_(2)O_(3)SnO_(2)ZnO材料电接触性能的影响[J].功能材料,2023,54(2):2159-2166.

1原涛,赵跃文.水热-共还原法制备电气用W/Cu复合粉末的组织和侵蚀性能研究[J].热加工工艺,2018,47(24):109-111.

2张文毓.铜基复合材料的研究现状与应用[J].铜加工,2019,0(1):11-15.

3伍玉鑫,王阳明,杨泽锋,许潘,吴广宁.电弧作用下浸铜碳材料烧蚀过程的数值模拟[J].电工技术学报,2019,34(6):1119-1126. 被引量:10

4臧恒佳.2018年地球上的10个惊人变化[J].大科技:天才少年图说百科(B),2019,0(3):28-29.

5银-金属氧化物电触头材料的制备方法、装置以及应用[J].电工材料,2019,0(1):47-48.

6张耀东,李程,姬瑞磊,樊国祥.PTFE复合体系电弧作用机理探讨及电气性能研究[J].湖北电力,2018,42(5):29-33. 被引量:3

7姚秋实,李进兴,方明学,李鹏,方广民.不同温度下阀控电池失水方式分析[J].蓄电池,2019,56(1):35-37. 被引量:1

8夏谷林,邓军,丁卫东,钱凯洋,王育佳.电弧作用下SF_6分解固体产物的实验研究[J].高压电器,2018,54(6):223-228. 被引量:4

9张立群,张晓冉,张静轩,胡靖宇,许艺颖,赵振宇,于东超.改性橡胶骨料混凝土的抗氯离子渗透性能及抗冲击性能研究[J].混凝土与水泥制品,2019(3):10-13. 被引量:5

10李维刚,郑全新.电弧的形成机制与灭弧原理研究[J].通信电源技术,2019,36(2):21-22. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146[金属学及工艺—金属材料]

Citation Information:

A new type of Ag-Ti2AlN electrical contact materials were prepared by high energy ball milling and powder metallurgy.The arc erosion behavior and mechanism of the contact materials were studied.The surface microstructure of the contact after arc erosion was analyzed by scanning electron microscopy.The results show that Ti2AlN reinforcement has obvious advantages in improving the arc time,arc energy and welding resistance of Ag-matrix electrical contact materials.The average arc time,arc energy and welding strength of Ag-Ti2AlN contacts are 5.61 ms,59.8 mJ and 15 cN respectively in 70 000 on-off cycle tests. Under the action of vapor arc,the corrosion pit centers such as lava and sweat droplets are formed in the cathode of electric contacts.The Ti2 AlN reinforcement particles are fused into the silver melting pool by the diffusion of titanium and aluminum,which can improve the viscosity of the melt,and then enhance the arc erosion resistance.In addition,because of the preferential oxidation mechanism of Al element,the formed Al2O3 absorbs a lot of heat during vaporization,which reduces the mass gain of the anode and the height of the anode bulge,and effectively improves the reliability of electrical contact materials.

quote

GB/T 7714-2015 [1] JIA Hai-long, ZHU Gang, XIE Ming, et al. Study on Arc Erosion Behavior of a New Type of Ag-Ti_2AlN Electrical Contact Material[J]. Rare Metals and Cemented Carbides, 2019(1): 26-30.
MLA [1] JIA Hai-long, et al., "Study on Arc Erosion Behavior of a New Type of Ag-Ti_2AlN Electrical Contact Material." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 26-30.
APA [1] JIA Hai-long, ZHU Gang, XIE Ming, LI Ai-kun, LIU Man-men, WU Di, & WU Xian-yue. (2019). Study on Arc Erosion Behavior of a New Type of Ag-Ti_2AlN Electrical Contact Material. Rare Metals and Cemented Carbides(1), 26-30.
IEEE [1] JIA Hai-long, ZHU Gang, XIE Ming, LI Ai-kun, LIU Man-men, WU Di, and WU Xian-yue, "Study on Arc Erosion Behavior of a New Type of Ag-Ti_2AlN Electrical Contact Material," Rare Metals and Cemented Carbides, no. 1, pp. 26-30, 2019. keywords: {composite;Ag-matrix electrical contact material;Ti2 AlN reinforcement;electrical conductivity;arc erosion}