Effect of Biomimetic Preset Crystal Seeds on Hydroxyapatite Coatings Prepared by Electrodeposition on Titanium Substrate AITranslate

School of Chemical Engineering and Light Industry,Guangdong University of Technology;School of Chemical Engineering and Light Industry,Guangdong University of Technology;School of Chemical Engineering and Light Industry,Guangdong University of Technology;School of Chemical Engineering and Light Industry,Guangdong University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

HAP seeds were constructed on Ti substrate by biomimetic preset crystal seeds method to provide nucleation points for the formation of HAP coating,and then HAP coating was obtained by electrodeposition at low temperature.The microstructures of HAP coating prepared by electrodeposition with biomimetic preset crystal seeds were studied by scanning electron microscopy,X-ray diffraction,infrared spectroscopy and Raman spectroscopy,and the cytotoxicity of HAP coating was tested by MTT method.The results show that the surface morphology of HAP coatings prepared by electrodeposition changed from three-dimensional network structure to honeycomb structure as the time of biomimetic preset crystal seeds prolonged from 24 h to 48 h.Compared with the HAP coating prepared by electrodeposition without seeds, the HAP coating prepared by electrodeposition after presetting crystal seeds is more uniform and corn,pact, 3 and has higher bonding strength with the matrix,also is more conducive to the proliferation,metabolism and growth of osteoblasts.

KeyWords AITranslate

biomimetic preset crystal seeds Ti substrate HAP coating electrodeposition network structure cytotpxicity

1陈彰旭.咪唑-1-乙酸壳聚糖支架仿生合成羟基磷灰石[J].化工新型材料,2017,45(6):230-232. 被引量:3

2Na YIN,Shi-yan CHEN,Yang OUYANG,Lian TANG,Jing-xuan YANG,Hua-ping WANG.Biomimetic mineralization synthesis of hydroxyapatite bacterial cellulose nanocomposites[J].自然科学进展·国际材料:英文版,2011,21(6):472-477. 被引量:7

3付涛,徐可为.仿生法沉积磷灰石层的研究进展[J].生物医学工程学杂志,2001,18(1):116-118. 被引量:25

1王冉,祁涛.多级孔纳米ZSM-5分子筛的制备及其催化芳构化性能研究[J].化工管理,2017(28):83-85.

2曾晗,吴宏,周承商,刘咏,刘彬.烧结温度对高速钢颗粒增强钛基复合材料组织与性能的影响[J].粉末冶金材料科学与工程,2019,24(1):68-74.

3刘林涛,李争显,王彦峰,李宏战.纯钛表面多步合成Ti-Al梯度抗氧化涂层[J].钛工业进展,2018,35(6):26-30. 被引量:2

4王伟,周海雄,王庆娟,王成,孙亚玲,邹武.石墨烯增强钛基复合材料的摩擦学性能研究[J].兵器材料科学与工程,2019,42(1):26-32. 被引量:8

5王欢,陈雪梅.晶种法制备高长径比纳米银线的研究[J].人工晶体学报,2019,48(1):1-7. 被引量:3

6李孟星,孟祥海,马涛,张宏博,李欣,徐鸣悦,李运刚.电流对电沉积制备Fe-Ni功能材料的影响研究[J].有色金属:冶炼部分,2019(2):51-54. 被引量:3

7宋袁曾,刘立君,齐超琪,李亚萍,高转妮.飞机襟翼滑轨用钛合金表面激光熔注WC/TC4复合涂层微观组织分析[J].焊接,2018(11):44-49. 被引量:2

8孙宏丽,王腾蛟,许军,李帅,王颖,李晓莉,袁小先.云母片上单层石墨烯的制备及拉曼光谱研究[J].河北大学学报:自然科学版,2019,39(1):23-28. 被引量:1

9齐海东,周宗熠,温林洁,张丽楠,李运刚,杨海丽.电沉积制备Ni-Fe/TiO_2复合电极及其析氢催化性能[J].钢铁钒钛,2019,40(1):47-52. 被引量:2

10许玲萍,刘希豪,邵东强,朱义.汽车覆盖件冷冲压模具激光熔覆强化技术[J].锻压技术,2019,44(2):135-140. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

HAP seeds were constructed on Ti substrate by biomimetic preset crystal seeds method to provide nucleation points for the formation of HAP coating,and then HAP coating was obtained by electrodeposition at low temperature.The microstructures of HAP coating prepared by electrodeposition with biomimetic preset crystal seeds were studied by scanning electron microscopy,X-ray diffraction,infrared spectroscopy and Raman spectroscopy,and the cytotoxicity of HAP coating was tested by MTT method.The results show that the surface morphology of HAP coatings prepared by electrodeposition changed from three-dimensional network structure to honeycomb structure as the time of biomimetic preset crystal seeds prolonged from 24 h to 48 h.Compared with the HAP coating prepared by electrodeposition without seeds, the HAP coating prepared by electrodeposition after presetting crystal seeds is more uniform and corn,pact, 3 and has higher bonding strength with the matrix,also is more conducive to the proliferation,metabolism and growth of osteoblasts.

quote

GB/T 7714-2015 [1] ZHOU Hao, CHENG Xiao-ling, HUANG Lu-yin, et al. Effect of Biomimetic Preset Crystal Seeds on Hydroxyapatite Coatings Prepared by Electrodeposition on Titanium Substrate[J]. Rare Metals and Cemented Carbides, 2019(1): 31-35.
MLA [1] ZHOU Hao, et al., "Effect of Biomimetic Preset Crystal Seeds on Hydroxyapatite Coatings Prepared by Electrodeposition on Titanium Substrate." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 31-35.
APA [1] ZHOU Hao, CHENG Xiao-ling, HUANG Lu-yin, & PAN Guang-min. (2019). Effect of Biomimetic Preset Crystal Seeds on Hydroxyapatite Coatings Prepared by Electrodeposition on Titanium Substrate. Rare Metals and Cemented Carbides(1), 31-35.
IEEE [1] ZHOU Hao, CHENG Xiao-ling, HUANG Lu-yin, and PAN Guang-min, "Effect of Biomimetic Preset Crystal Seeds on Hydroxyapatite Coatings Prepared by Electrodeposition on Titanium Substrate," Rare Metals and Cemented Carbides, no. 1, pp. 31-35, 2019. keywords: {biomimetic preset crystal seeds;Ti substrate;HAP coating;electrodeposition;network structure;cytotpxicity}