Preparation of Nano TiC Reinforced Ti-matrix Composite Powder by Mechanical Alloying AITranslate
Abstract AITranslate
Nano TiC reinforced Ti-matrix composite powder was prepared by mechanical alloying.The phase,morphology,crystal structure and element distribution of the powder were characterized by XRD, SEM,TEM and EDS.The effects of milling speed,ball-to-powder mass ratio and milling time on phase and morphology of the composite powder were investigated.The results show that milling efficiency has no significant difference when milling speed reaches 300 r/min or higher,and ball-to-powder mass ratio reaches 20 :1 or higher.TiC phase in the powder is obvious when milling time reaches 10 h,and nano TiC reinforcement phase is obtained when milling time is extended to 20 h.Under the conditions of 300 r/min milling speed,20 :1 ball-to-powder mass ratio and 20 h milling time,nano TiC reinforced Ti-matrix composite powder can be obtained,and part of the powder is amorphous,where a large number of nano TiC particles are dispersed.
KeyWords AITranslate
1倪月娥,柯昌明,韩兵强,李楠.纳米晶尖晶石-碳复合粉体的机械合金化法制备[J].硅酸盐学报,2012,40(1):137-144. 被引量:3
2李晓杰,孙伟,闫鸿浩,刘凯欣,王小红,罗宁.纯铜表面纳米氧化铝弥散强化覆层的制备研究[J].稀有金属材料与工程,2012,41(S2):32-34. 被引量:1
3张厚安,胡小平,黄文哲,毛征宇.机械合金化制备Al-Pb粉末[J].粉末冶金技术,2000,18(4):270-273. 被引量:9
4丁睿谦,杨英丽,吴金平,杨帆.TA2钛合金表面激光熔覆金属钽探索实验研究[J].稀有金属与硬质合金,2017,45(3):36-40. 被引量:2
5MENG Jie JIA Chengchang HE Qing.Characteristics of mechanical alloyed Ni-Al powder for sintering[J].稀有金属:英文版,2007,26(4):372-376. 被引量:1
6冯黛丽,冯妍卉,袁思伟,张欣欣.颗粒团聚对纳米尺度熔化行为的影响[J].工程热物理学报,2015,36(2):397-401. 被引量:13
7张亚萍,鲁玉祥,郭进.球磨环境对机械合金化合成纳米TiC的影响[J].石油大学学报:自然科学版,2005,29(2):136-140. 被引量:6
8武万良,李学伟,刘万辉,郭子玉.TiC增强钛基复合材料激光熔覆层显微组织及形成机理[J].稀有金属材料与工程,2006,35(9):1363-1366. 被引量:22
9冉广,周敬恩,席生岐,王永芳.机械合金化制备纳米晶与非晶Al-Pb系粉末[J].稀有金属材料与工程,2005,34(10):1617-1621. 被引量:8
1吴琼,肖震东,侯纪新,周巍,阴雅雯,夏志新.机械合金化法制备Ti_(50)Ni_(15)Cu_(28)Sn_7非晶合金粉末[J].热加工工艺,2019,48(4):36-38. 被引量:1
2张坤淑.正当防卫时间性问题研究[J].天津检察,2019,0(1):17-20.
3徐海健,沙孝春,孟劲松,李凡,王文仲,康超,吕铮.15Cr-ODS钢的微观组织及力学性能[J].材料热处理学报,2019,40(1):107-111. 被引量:2
4谢锐,吕铮,王晴,刘春明.热等静压制备9Cr氧化物弥散强化钢的组织性能[J].新技术新工艺,2019(3):7-12. 被引量:3
5王婧,张蕾.任务前准备时间与语言复杂性对英语学习者复述故事的影响研究[J].佳木斯职业学院学报,2018,34(11):297-298. 被引量:1
6刘萌萌,白亚平,李建平,郭永春,杨忠,罗佳佳,成超.干摩擦与边界润滑下SiC/Al复合材料的摩擦磨损性能[J].轻合金加工技术,2019,47(3):65-71. 被引量:3
7李庆文,吴琼,刘志豪,杨占鑫,魏玉冬,刘源淼,刘成,齐国超.真空烧结法层状Ti_3SiC_2材料的制备研究[J].陶瓷,2019(3):41-45. 被引量:1
8李琪,王瑞峰.基于KH算法的高速列车ATO控制策略优化研究[J].铁道标准设计,2019,63(3):165-168. 被引量:3
9董至恒,郭楠,石瑞文,包小妹,王玉华,张烨,关海滨.温度诱导对鼠李糖乳杆菌cspc mRNA基因表达和生长速率的影响[J].食品工业科技,2019,40(6):137-140.
10饶永明,张延孔,谢文军,刘璐,刘新月,罗月童.交通事故时空模式可视分析方法[J].计算机科学,2019,46(4):14-21. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
Nano TiC reinforced Ti-matrix composite powder was prepared by mechanical alloying.The phase,morphology,crystal structure and element distribution of the powder were characterized by XRD, SEM,TEM and EDS.The effects of milling speed,ball-to-powder mass ratio and milling time on phase and morphology of the composite powder were investigated.The results show that milling efficiency has no significant difference when milling speed reaches 300 r/min or higher,and ball-to-powder mass ratio reaches 20 :1 or higher.TiC phase in the powder is obvious when milling time reaches 10 h,and nano TiC reinforcement phase is obtained when milling time is extended to 20 h.Under the conditions of 300 r/min milling speed,20 :1 ball-to-powder mass ratio and 20 h milling time,nano TiC reinforced Ti-matrix composite powder can be obtained,and part of the powder is amorphous,where a large number of nano TiC particles are dispersed.
quote
| GB/T 7714-2015 | [1] FANG Chao, YAO Zheng-jun, DU Wen-bo, et al. Preparation of Nano TiC Reinforced Ti-matrix Composite Powder by Mechanical Alloying[J]. Rare Metals and Cemented Carbides, 2019(1): 19-25. |
| MLA | [1] FANG Chao, et al., "Preparation of Nano TiC Reinforced Ti-matrix Composite Powder by Mechanical Alloying." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 19-25. |
| APA | [1] FANG Chao, YAO Zheng-jun, DU Wen-bo, YIN Chun-sheng, & LIU Qi. (2019). Preparation of Nano TiC Reinforced Ti-matrix Composite Powder by Mechanical Alloying. Rare Metals and Cemented Carbides(1), 19-25. |
| IEEE | [1] FANG Chao, YAO Zheng-jun, DU Wen-bo, YIN Chun-sheng, and LIU Qi, "Preparation of Nano TiC Reinforced Ti-matrix Composite Powder by Mechanical Alloying," Rare Metals and Cemented Carbides, no. 1, pp. 19-25, 2019. keywords: {Ti-matrix composite powder;nano TiC;mechanical alloying;dispersive distribution;phase;morphology} |