Research on the Microstructure of Tungsten Oxides AITranslate

Chenzhou Diamond Tungsten Products Co., Ltd.;Zhuzhou Hard Alloy Group Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The microstructure of tungsten oxides was investigated by using scanning electron microscopy, transmission electron microscopy and so on. The results show that different tungsten oxides, including violet tungsten oxide,blue tungsten oxide and yellow tungsten oxide, are of different microstructure. Especially,violet tungsten oxide is of particular monocrystal bar structure and suitable for producing fine tungsten powders.

KeyWords AITranslate

tungsten oxide microstucture violet tungsten oxide blue tungsten oxide yellow tungsten oxide

1张克从 张乐漶.晶体生长科学与技术[M].北京:科学出版社,1997..

2陈响明,施超波,易丹青.紫钨生产的亚微米级钨粉和碳化钨粉的形貌[J].硬质合金,2002,19(2):65-69. 被引量:18

1项培云,张华民.紫钨晶型对超细碳化钨粉粒度的影响[J].稀有金属与硬质合金,2018,46(5):75-78. 被引量:6

1姜春辉.装舟量及还原时间对氧化钨物相形貌的影响[J].福建冶金,2019,48(2):35-37.

2张璐,陆必志,徐涛.超细碳化钨制备关键技术及评价方法研究的新进展[J].硬质合金,2019,36(6):460-471. 被引量:13

3喻相标,肖杰,郭少毓,肖义钰,廖春发,姜平国.蓝钨氢还原制备钨粉工艺研究[J].有色金属科学与工程,2021,12(3):35-41. 被引量:4

4谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2

5潘锋,刘家义,杜占,朱庆山.超细碳化钨制备过程及机理研究进展[J].化工学报,2021,72(11):5455-5467. 被引量:4

6魏庭民,李志锋,林钊,张永会,陈伟豪.紫色氧化钨制备工艺研究[J].世界有色金属,2022(20):163-165.

1姜文伟,陈响明.氧化钨微观结构的研究[J].江西有色金属,2010,24(3):105-108. 被引量:6

2张立.硬质合金中WC晶粒内部微孔形成原因探讨[J].粉末冶金技术,1995,13(3):181-185. 被引量:2

3王长基,刘鸿,谢璐,杜香珍,李军,华娟霞,龙水秀.钨制品的扫描电镜分析[J].中国钨业,2012,27(5):36-39. 被引量:1

4傅练英.APT煅烧工艺对WC质量的影响[J].硬质合金,2006,23(1):15-20. 被引量:5

5黄新,孙亚丽,刘清才,颜杰,金永中.WC粉末中的生长孪晶[J].中国钨业,2005,20(6):27-30. 被引量:1

6钟毓斌,孙娟,涂洁,郝立伟.超细、纳米晶硬质合金的原料制备研究[J].中国钨业,2016,31(6):35-40. 被引量:6

7廖寄乔,黄志锋,吕海波,陈绍衣,邹志强.不同氧化钨氢还原制取超细钨粉[J].中南工业大学学报,2000,31(1):51-55. 被引量:27

8雷纯鹏,唐建成,刘刚,吴爱华.W粉末的形貌结构对板状晶硬质合金的组织与性能的影响[J].稀有金属材料与工程,2016,45(8):2146-2149. 被引量:4

9张立,陈泳华,刘汝模.以蓝钨为原料制取的粗颗粒W粉、WC粉特性的研究[J].硬质合金,1994,11(4):200-204. 被引量:4

10雷纯鹏,刘刚,唐建成,张方.氧化钨形貌结构对纳米WC粉及其烧结性能的影响[J].稀有金属与硬质合金,2013,41(2):53-57. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

The microstructure of tungsten oxides was investigated by using scanning electron microscopy, transmission electron microscopy and so on. The results show that different tungsten oxides, including violet tungsten oxide,blue tungsten oxide and yellow tungsten oxide, are of different microstructure. Especially,violet tungsten oxide is of particular monocrystal bar structure and suitable for producing fine tungsten powders.

quote

GB/T 7714-2015 [1] JIANG Wen-wei, CHEN Xiang-ming. Research on the Microstructure of Tungsten Oxides[J]. Rare Metals and Cemented Carbides, 2009(3): 8-11.
MLA [1] JIANG Wen-wei, and CHEN Xiang-ming. "Research on the Microstructure of Tungsten Oxides." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 8-11.
APA [1] JIANG Wen-wei, & CHEN Xiang-ming. (2009). Research on the Microstructure of Tungsten Oxides. Rare Metals and Cemented Carbides(3), 8-11.
IEEE [1] JIANG Wen-wei and CHEN Xiang-ming, "Research on the Microstructure of Tungsten Oxides," Rare Metals and Cemented Carbides, no. 3, pp. 8-11, 2009. keywords: {tungsten oxide;microstucture;violet tungsten oxide;blue tungsten oxide;yellow tungsten oxide}