Research on Synthesizing Bi_2S_3 Nanorods by Complex Solvothermal Process AITranslate
Abstract AITranslate
Large-scale Bi2S3 nanorods were synthesized by the complex solvothermal process using copper reagent (sodium diethyldithiocarbamate) as sulfur source,bismuth nitrate as bismuth source,and glycerolwater system as solvent. The product was investigated by X-ray powder diffraction (XRD),transmission electron microscopy (TEM),field emission scanning electron microscopy (FESEM) and so on. The results show that the prepared sample is purely of orthorhombic crystal phase. The well-dispersed single-crystal nanorods are obtained, having the lateral sizes of 30-50 nm and the axial sizes of several microns. The formation mechanism of Bi2S3 nanorods is also discussed. It is concluded that both the complex solvent of glycerol-water and the surfactant of PVP have important influences on the morphology and size of Bi2 S3 single -crystal nanorods.
KeyWords AITranslate
1Shen G Z,Chen D,Tang K B,et al.Self-sacrificing template route to novel patterns of radially aligned Bi2(Se,S)3 nanorods and Bi2Se3 flakes[J].Nanotechnology,2004,15(11):1 530-1 534.
2Zhu J J,Liu S W,Palchik O,et al.Shape-controlled synthesis of silver nanoparticles by pulse sonoelectrochemical methods[J].Langmuir,2000,16(16):6 396-6 399.
3Cui H M,Liu H,Wang J Y,et al.Sonochemical synthesis of bismuth selenide nanobelts at room temperature[J].J Cryst Growth,2004,271(3-4):456-461.
4Li X X,Cheng F Y,Guo B,et al.Template-synthesized LiCoO2,LiMn2O4,and LiNi0.8Co0.2O2nanotubes as the cathode materials of lithium ion batteries[J].J Phys Chem B,2005,109(29):14 017-14 024.
5Wu Y Y,Yang P D.Germanium nanowire growth via simple vapor transport[J].Chem Mater,2000,12(3):605-607.
6Jia C J,Sun L D,Yan Z G,et al.Single-crystalline iron oxide nanotubes[J].Angew Chem,2005,117(28):4 402-4 407.
7Xia Y N,Yang P D,Sun Y G,et al.One-dimensional nanostructures:synthesis,characterization,and applications[J].Adv Mater,2003,15(5):353-389.
8Tang K B,Qian Y T,Zeng J H,et al.Solvothermal route to semiconductor nanowires[J].Adv Mater,2003,15(5):448-450.
9Nayak B B,Achya H N,Mitra G B,et al.Structural characterization of Bi2-xSbxS3 films prepared by the dip-dry method[J].Thin Solid Films,1983,105(1):17-24.
10Boudjouk P,Remington M P,Grier D G,et al.Tris(benzylthiolato)bismuth efficient precursor to phase-pure polycrystalline Bi2S3[J].J Inorg Chem,1998,37(3):3 538-3 547.
1陈渊,杨家添,谢祖芳,韦庆敏,朱立刚,刘国聪.蛋挞状Bi_2WO_6催化剂的制备及其光催化性能[J].人工晶体学报,2014,43(2):380-387. 被引量:7
2罗昉星,汤化伟,袁新松.硫化铋单晶纳米棒的模板法合成研究[J].广东化工,2016,43(9):112-113.
3张鸿羽,王爱军,袁耀.不同溶剂对钨酸铋形貌及可见光催化性能的影响[J].广州化工,2017,45(9):81-84. 被引量:1
4陈渊,杨家添,韦庆敏,周科朝,刘国聪.PVP辅助混合溶剂热法制备高可见光催化活性的花状Bi_2WO_6催化剂[J].中国有色金属学报,2014,24(8):2090-2099. 被引量:2
1董兴安,熊伟,遇丽.N掺杂Bi_2O_2CO_3/氧化石墨烯分级结构的合成及其可见光催化性能研究[J].人工晶体学报,2015,44(6):1675-1682. 被引量:2
2梁敏,莫创荣,张金莲,王馨蔚.复合磁性光催化剂Co_(0.5)Zn_(0.5)Fe_2O_4/Bi_2WO_6的制备及其光催化性能[J].化工环保,2016,36(2):183-188. 被引量:2
3陈渊,杨家添,韦庆敏,晏全,黎中良,秦颖瑜.方形花状Bi_2WO_6可见光催化降解制革废水[J].广西师范大学学报:自然科学版,2016,34(4):60-69. 被引量:4
4张鸿羽,王爱军,袁耀.不同溶剂对钨酸铋形貌及可见光催化性能的影响[J].广州化工,2017,45(9):81-84. 被引量:1
5鲁珍,王亚珍,刘晓烨,何丹.不同碱液调节pH水热制备钨酸铋及其光催化性能研究[J].江汉大学学报:自然科学版,2019,47(1):41-45. 被引量:1
6崔家民,杨艳青,靳虎芳,邓钏,张卫珂.凹凸棒/Bi2WO6光催化复合材料的制备及性能[J].复合材料学报,2019,0(9):2119-2130. 被引量:3
7王蕊,徐梅,谢家文,叶盛英,宋贤良.水热反应条件对多孔球状Bi2WO6光催化剂结构及性能的影响[J].高等学校化学学报,2020,41(6):1320-1328. 被引量:3
8逄显娟,王新胜.钨酸铋的制备及其光降解有机污染物的研究进展[J].化工新型材料,2021,49(3):225-229. 被引量:3
9牛凯莉,孙冰,刘宇,朱小梅.钨酸铋光催化剂在四环素废水处理中的应用研究进展[J].工业水处理,2021,41(11):9-15. 被引量:4
1罗昉星,汤化伟,袁新松.硫化铋单晶纳米棒的模板法合成研究[J].广东化工,2016,43(9):112-113.
2刘淑玲,李红霖,闫路.二氧化锡微球的制备、表征及其性能研究[J].陕西科技大学学报:自然科学版,2013,31(5):70-73. 被引量:6
3廖学红,郑坚.微波合成半导体CuS纳米粒子和Bi_2S_3纳米棒[J].黄冈师范学院学报,2002,22(6):26-27. 被引量:2
4吕燕飞,吴希俊,吴大雄.乙醇/水复合溶剂中纳米CaF_2的沉淀制备及表征[J].功能材料,2006,37(7):1108-1109. 被引量:13
5韩璐,曹栋,杜鹏,张锐.Bi_2S_3纳米棒的可控合成和表征[J].河北科技师范学院学报,2011,25(2):4-7.
6碳纳米管[J].粉末冶金技术,2016,34(6):460-460.
7郑佳,沙建超.碳纳米管技术专利分析[J].新材料产业,2014(9):60-65. 被引量:2
8李强,杜卫民.大规模合成近乎单分散的镍三维纳米结构及其催化性能研究(英文)[J].稀有金属材料与工程,2009,38(12):2080-2084. 被引量:1
9韦东远.我国碳纳米管发展及应用[J].创新科技,2011(3):18-19. 被引量:1
10梅丹丹,张林.压缩喷射制冷循环射流泵轴向尺寸设计计算[J].制冷空调与电力机械,2008,29(2):47-50.
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
Large-scale Bi2S3 nanorods were synthesized by the complex solvothermal process using copper reagent (sodium diethyldithiocarbamate) as sulfur source,bismuth nitrate as bismuth source,and glycerolwater system as solvent. The product was investigated by X-ray powder diffraction (XRD),transmission electron microscopy (TEM),field emission scanning electron microscopy (FESEM) and so on. The results show that the prepared sample is purely of orthorhombic crystal phase. The well-dispersed single-crystal nanorods are obtained, having the lateral sizes of 30-50 nm and the axial sizes of several microns. The formation mechanism of Bi2S3 nanorods is also discussed. It is concluded that both the complex solvent of glycerol-water and the surfactant of PVP have important influences on the morphology and size of Bi2 S3 single -crystal nanorods.
quote
| GB/T 7714-2015 | [1] YUAN Xin-song, HAO Jian-wen, ZHU Jin-miao, et al. Research on Synthesizing Bi_2S_3 Nanorods by Complex Solvothermal Process[J]. Rare Metals and Cemented Carbides, 2009(3): 5-7. |
| MLA | [1] YUAN Xin-song, et al., "Research on Synthesizing Bi_2S_3 Nanorods by Complex Solvothermal Process." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 5-7. |
| APA | [1] YUAN Xin-song, HAO Jian-wen, ZHU Jin-miao, ZHOU A-yang, & ZHOU Tao. (2009). Research on Synthesizing Bi_2S_3 Nanorods by Complex Solvothermal Process. Rare Metals and Cemented Carbides(3), 5-7. |
| IEEE | [1] YUAN Xin-song, HAO Jian-wen, ZHU Jin-miao, ZHOU A-yang, and ZHOU Tao, "Research on Synthesizing Bi_2S_3 Nanorods by Complex Solvothermal Process," Rare Metals and Cemented Carbides, no. 3, pp. 5-7, 2009. keywords: {complex solvothermal process;Bi2 S3;nanorod;glycerol-water;PVP} |