Characteristics of β_2 Phase in the Casting Alloy Ti-47Al-2Cr-2Nb and its Effect on the Alloy Thermal Stability AITranslate

School of Materials Science and Engineering, Beijing University of Aeronautics and Astronautics;School of Materials Science and Engineering, Beijing University of Aeronautics and Astronautics;School of Materials Science and Engineering, Beijing University of Aeronautics and Astronautics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The characteristics of β2phase and its effects on the alloy thermal stability were investigated in the casting alloy Ti-47Al-2Cr-2Nb with industrial application value. The results show that β2 phase is with high Cr content and of dispersive distribution and continuous linear morphology in the TiAl alloy lamellar microstrueture. No strict coherent orientation of a2 and 7 phase is kept in β2 phase. By aging treatment (1 150℃ and 48 h),the lamellar structure is dissolved and coarsened preferentially at the phase interface between β2 and (a2+γ). During the heating process of (a2+γ) phase region,a2 particles are also precipitated and grown preferentially at the boundary. Accordingly,the addition of β2 phase is harmful for the thermal stability of TiAl alloy.

KeyWords AITranslate

TiAl alloy β2 phase thermal stability

1Kim Y W.Ordered intermetallic alloys (part Ⅲ)[J].JOM,1994,46(7):30-39.

2Chen G L,Zhang W J,Liu Z C,et al.Microstructure and properties of high Nb containing TiAl alloys[A].Nathal M V,Daralia,Liu C T,et al.Structural Inter-metallics[C].Warrendale PA:TMS,1997.371-380.

3唐兆麟,王福会.Cr对TiAl金属间化合物抗循环氧化性能的影响[J].中国有色金属学报,1998,8(2):245-249. 被引量:6

4李臻熙,曹春晓.添加微量硼对TiAl合金持久性能的影响[J].中国有色金属学报,2005,15(6):836-841. 被引量:6

5Maziasz P J,Ramanujan R V,Liu C T,et al.Effects of B and W alloying additions on the formation and stability of lamellar[J].Intermetallics,1997,5(2):83-96.

6郑运荣,汪小平,阮中慈,马书伟.Cr、Al含量对铸造TiAl基合金显微组织的影响[J].航空材料学报,1995,15(4):8-14. 被引量:3

7Maria A Munoz-Morris,I Gil,David G Morris.Microstructural stability of γ-based TiAl intermetallics containing β phase[J].Intermetalics,2005,13(9):929-936.

8周兰章,郭建亭,周兰章,肖旋,V.Lupinc,M.Maldini.金属间化合物TiAl(W,Si,B)合金的组织稳定性及其蠕变性能[J].金属学报,2002,38(11):1175-1180. 被引量:5

9Ramanujan R V,Maziasz P J,Liu C T.The thermal stability of the microstructure of γ-based titanium aluminides[J].Acta Mater,1996,44(7):2 611-2 642.

10Sharma G,Ramanujan R V,Tiwari G P.The mechanisms of thermal instabilities in lamellar microstructures[J].Acta Mater,2000,48(4):875-889.

1李德发,梁宝珠,王世森,董汉雄.消除应力热处理对15MnNiNbDR特厚板组织和力学性能的影响[J].热加工工艺,2016,45(14):239-240. 被引量:1

2周亦胄,郭敬东,王宝全,何冠虎,单以银.脉冲电流对低碳微合金钢力学性能的影响[J].材料研究学报,2002,16(3):243-246. 被引量:13

3于庆波,李子林,韦玄,于爱民.低碳合金钢变形奥氏体的相变研究[J].材料热处理学报,2007,28(4):83-87. 被引量:4

4王悔改,何春娜,李云月,李科杰,任少凯,王文哲.TA15钛合金棒材在加热和冷却过程中的相转变[J].金属热处理,2015,40(7):111-114.

5陈勋,范群波,杨学文.TC6钛合金加热和冷却过程中的相转变研究[J].稀有金属材料与工程,2012,41(12):2123-2126. 被引量:5

6庄宝潼,江海涛,唐荻,米振莉,蒯振.汽车用Q&P钢中的残留奥氏体[J].金属热处理,2012,37(5):11-15. 被引量:4

7车成卫,张志明,田锡唐.Pr激光表面合金化对Ti-6A1-4V组织热稳定性的影响[J].机械工程学报,1995,31(6):97-101. 被引量:1

8贾海龙,于浩杰.计算机用镁合金的组织热稳定性及力学性能[J].热加工工艺,2015,44(8):187-190. 被引量:1

9盛晓菲,杨文超,汪明朴,李周,龚静,彭诚.人工时效对6005A铝合金晶间腐蚀性能的影响[J].中国有色金属学报,2012,22(8):2174-2180. 被引量:13

10祁小红,邓运来,刘胜胆,张云崖,张新明.微量Sc对7085铝合金淬火敏感性的影响[J].中国有色金属学报,2013,23(3):666-672. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

The characteristics of β2phase and its effects on the alloy thermal stability were investigated in the casting alloy Ti-47Al-2Cr-2Nb with industrial application value. The results show that β2 phase is with high Cr content and of dispersive distribution and continuous linear morphology in the TiAl alloy lamellar microstrueture. No strict coherent orientation of a2 and 7 phase is kept in β2 phase. By aging treatment (1 150℃ and 48 h),the lamellar structure is dissolved and coarsened preferentially at the phase interface between β2 and (a2+γ). During the heating process of (a2+γ) phase region,a2 particles are also precipitated and grown preferentially at the boundary. Accordingly,the addition of β2 phase is harmful for the thermal stability of TiAl alloy.

quote

GB/T 7714-2015 [1] ZHAO Yong, PEI Yan-ling, MA Yue. Characteristics of β_2 Phase in the Casting Alloy Ti-47Al-2Cr-2Nb and its Effect on the Alloy Thermal Stability[J]. Rare Metals and Cemented Carbides, 2009(3): 12-15.
MLA [1] ZHAO Yong, et al., "Characteristics of β_2 Phase in the Casting Alloy Ti-47Al-2Cr-2Nb and its Effect on the Alloy Thermal Stability." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 12-15.
APA [1] ZHAO Yong, PEI Yan-ling, & MA Yue. (2009). Characteristics of β_2 Phase in the Casting Alloy Ti-47Al-2Cr-2Nb and its Effect on the Alloy Thermal Stability. Rare Metals and Cemented Carbides(3), 12-15.
IEEE [1] ZHAO Yong, PEI Yan-ling, and MA Yue, "Characteristics of β_2 Phase in the Casting Alloy Ti-47Al-2Cr-2Nb and its Effect on the Alloy Thermal Stability," Rare Metals and Cemented Carbides, no. 3, pp. 12-15, 2009. keywords: {TiAl alloy;β2 phase;thermal stability}