Sub-Micrometer Ag Particles Boost Luminescence and Thermal Stability of Perovskite Quantum Dot Phosphors for Light-Emitting Diodes AITranslate

AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Perovskite quantum dots (QDs) have been considered as promising emitters for lighting and display applications, but they suffer from poor thermal stability under operation. Herein, we introduce sub-micrometer Ag particles to simultaneously enhance the luminescence intensity and thermal stability of perovskite QDs. The CsPbBr3/Ag (CPB/Ag) hybrid phosphors are synthesized via an in situ solid-phase method. We find that nano-sized Ag particles quench perovskite QD emission, and their discontinuous structure also disrupts thermal conduction pathways, thereby sacrificing the benefit of metal particles. Relatively, sub-micrometer Ag particles enable the hybrid phosphors a 2.2-fold increase in PL intensity compared to pristine CsPbBr3 by leveraging the strong light scattering. Furthermore, benefitting from the high thermal conductivity of sub-micrometer Ag particles, the hybrid phosphors retain 75.6% of their initial PL intensity at 85°C, significantly higher than that of 24.8% for pristine CsPbBr3. As a result, a CPB/Ag-based white LED (WLED) retains 83.5% of its initial luminance after 1000 h of operation, which is much higher than that of 30.3% for a pristine CsPbBr3-based WLED. This study demonstrates the crucial role of sub-micrometer Ag particles in enhancing the brightness and thermal stability of perovskite phosphor and their potential for enabling reliable, high-performance WLEDs.

KeyWords AITranslate

Ag particles light scattering perovskite QDs thermal stabilities white light-emitting diodes
No data

Basic Information:

DOI:

Chinese Library Classification Number:

Citation Information:

Perovskite quantum dots (QDs) have been considered as promising emitters for lighting and display applications, but they suffer from poor thermal stability under operation. Herein, we introduce sub-micrometer Ag particles to simultaneously enhance the luminescence intensity and thermal stability of perovskite QDs. The CsPbBr3/Ag (CPB/Ag) hybrid phosphors are synthesized via an in situ solid-phase method. We find that nano-sized Ag particles quench perovskite QD emission, and their discontinuous structure also disrupts thermal conduction pathways, thereby sacrificing the benefit of metal particles. Relatively, sub-micrometer Ag particles enable the hybrid phosphors a 2.2-fold increase in PL intensity compared to pristine CsPbBr3 by leveraging the strong light scattering. Furthermore, benefitting from the high thermal conductivity of sub-micrometer Ag particles, the hybrid phosphors retain 75.6% of their initial PL intensity at 85°C, significantly higher than that of 24.8% for pristine CsPbBr3. As a result, a CPB/Ag-based white LED (WLED) retains 83.5% of its initial luminance after 1000 h of operation, which is much higher than that of 30.3% for a pristine CsPbBr3-based WLED. This study demonstrates the crucial role of sub-micrometer Ag particles in enhancing the brightness and thermal stability of perovskite phosphor and their potential for enabling reliable, high-performance WLEDs.

quote

GB/T 7714-2015 [1] Sub-Micrometer Ag Particles Boost Luminescence and Thermal Stability of Perovskite Quantum Dot Phosphors for Light-Emitting Diodes[J]. Rare Metals, 2026(3).
MLA [1] "Sub-Micrometer Ag Particles Boost Luminescence and Thermal Stability of Perovskite Quantum Dot Phosphors for Light-Emitting Diodes." Rare Metals, no. 3, 2026.
APA [1] (2026). Sub-Micrometer Ag Particles Boost Luminescence and Thermal Stability of Perovskite Quantum Dot Phosphors for Light-Emitting Diodes. Rare Metals(3).
IEEE [1] "Sub-Micrometer Ag Particles Boost Luminescence and Thermal Stability of Perovskite Quantum Dot Phosphors for Light-Emitting Diodes," Rare Metals, no. 3, 2026. keywords: {Ag particles;light scattering;perovskite QDs;thermal stabilities;white light-emitting diodes}