daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ammonium Salt Assisted Crystallization for High Performance Two-Dimensional Lead-Free Perovskite Photodetector Ammonium Salt Assisted Crystallization for High Performance Two-Dimensional Lead-Free Perovskite Photodetector AITranslate

P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences;University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences; P. R. China|University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional Ruddlesden–Popper lead-free perovskites show promising prospects for application in optoelectronic devices due to their tunable optoelectronic properties and environmental friendliness. However, their carrier mobility and stability are limited by the crystal morphology and lattice direction, which hinder the improvement of their optoelectronic device performance. Here, we introduce a convenient ammonium assistance method to improve the crystallinity and lattice orientation of 2D perovskite films, through which carrier mobility and stability of 2D perovskites can be significantly improved. Oriented crystals, increased grain size, and improved crystal quality contribute to the high performance of lateral photodetectors. The champion device exhibits high Responsivity, External Quantum Efficiency, and Detectivity (938 A/W, 34714%, and 3.70 × 1014 Jones, respectively), as well as outstanding stability. This work reveals the potential of ammonium assistance 2D perovskite in developing high-performance and stable optoelectronic devices.

KeyWords AITranslate

2D perovskite leadfree perovskite ammonium chloride crystallization photodetector
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00058

Chinese Library Classification Number:

Citation Information:

Two-dimensional Ruddlesden–Popper lead-free perovskites show promising prospects for application in optoelectronic devices due to their tunable optoelectronic properties and environmental friendliness. However, their carrier mobility and stability are limited by the crystal morphology and lattice direction, which hinder the improvement of their optoelectronic device performance. Here, we introduce a convenient ammonium assistance method to improve the crystallinity and lattice orientation of 2D perovskite films, through which carrier mobility and stability of 2D perovskites can be significantly improved. Oriented crystals, increased grain size, and improved crystal quality contribute to the high performance of lateral photodetectors. The champion device exhibits high Responsivity, External Quantum Efficiency, and Detectivity (938 A/W, 34714%, and 3.70 × 1014 Jones, respectively), as well as outstanding stability. This work reveals the potential of ammonium assistance 2D perovskite in developing high-performance and stable optoelectronic devices.

quote

GB/T 7714-2015 [1] Tao Huang, Ruiyan Li, Xuhang Chen, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00058.
MLA [1] Tao Huang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00058.
APA [1] Tao Huang, Ruiyan Li, Xuhang Chen, Ying Li, Yulei Chang, Wei Li, & Weili Yu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00058
IEEE [1] Tao Huang, Ruiyan Li, Xuhang Chen, Ying Li, Yulei Chang, Wei Li, and Weili Yu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00058. keywords: {2D perovskite leadfree perovskite ammonium chloride crystallization photodetector}