(Tetrafluorovinylphenyl)carbazole as a Multifunctional Material for OLED Applications (Tetrafluorovinylphenyl)carbazole as a Multifunctional Material for OLED Applications AITranslate

Lviv Polytechnic National University;Lviv Polytechnic National University;Lviv Polytechnic National University;Lviv Polytechnic National University;Lviv Polytechnic National University; Kaunas University of Technology; Kaunas University of Technology; University Savoie Mont Blanc; Bohdan Khmelnytsky National University; Linköping University;Research Institute for Physical Chemical Problems of the Belarusian State University;Research Institute for Physical Chemical Problems of the Belarusian State University; Kaunas University of Technology; Linköping University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The multifunctional materials for application in organic light-emitting devices (OLEDs) based on a single structural motif are very desired but quite rare species. Such structures allow simplifying the chemical variety within OLED heterostructures and thus reducing their cost, manufacturing time, and logistic efforts. In this paper, we report the 9-(2,3,5,6-tetrafluoro-4-vinylphenyl)carbazole molecule (Cz4FS) utilized as a fluorescent emitter, host material for quantum dot based OLEDs (QLEDs), acceptor part of the exciplex active layer, and monomer that can be used for the preparation of emissive polymers and copolymers. The external quantum efficiency (EQE) of the corresponding fluorescent OLED based on a Cz4FS single emitter doped into a 1,3-bis(carbazol-9-yl)benzene matrix is 4.2%, which is close to the theoretical limit and maximum brightness at the level of 3600 cd/m2. An OLED based on exciplex emission obtained utilizing Cz4FS as an acceptor demonstrates higher efficiency (5.3%) and much higher brightness near 25 000 cd/m2. A QLED based on Cz4FS as a host for CdSeS/ZnS core–shell quantum dots demonstrates excellent energy transfer from the Cz4FS matrix that results in a clear spectrum of quantum dots with an EQE of 2.3%, maximum of 19 000 cd/m2, and narrow spectral distribution. An OLED based on a Cz4FS-based polymer and copolymer demonstrates not extraordinary efficiency but low-efficiency roll-off in a wide range of current densities.

KeyWords AITranslate

exciplex OLED fluorescence polymer quantum dots charge transfer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00047

Chinese Library Classification Number:

Citation Information:

The multifunctional materials for application in organic light-emitting devices (OLEDs) based on a single structural motif are very desired but quite rare species. Such structures allow simplifying the chemical variety within OLED heterostructures and thus reducing their cost, manufacturing time, and logistic efforts. In this paper, we report the 9-(2,3,5,6-tetrafluoro-4-vinylphenyl)carbazole molecule (Cz4FS) utilized as a fluorescent emitter, host material for quantum dot based OLEDs (QLEDs), acceptor part of the exciplex active layer, and monomer that can be used for the preparation of emissive polymers and copolymers. The external quantum efficiency (EQE) of the corresponding fluorescent OLED based on a Cz4FS single emitter doped into a 1,3-bis(carbazol-9-yl)benzene matrix is 4.2%, which is close to the theoretical limit and maximum brightness at the level of 3600 cd/m2. An OLED based on exciplex emission obtained utilizing Cz4FS as an acceptor demonstrates higher efficiency (5.3%) and much higher brightness near 25 000 cd/m2. A QLED based on Cz4FS as a host for CdSeS/ZnS core–shell quantum dots demonstrates excellent energy transfer from the Cz4FS matrix that results in a clear spectrum of quantum dots with an EQE of 2.3%, maximum of 19 000 cd/m2, and narrow spectral distribution. An OLED based on a Cz4FS-based polymer and copolymer demonstrates not extraordinary efficiency but low-efficiency roll-off in a wide range of current densities.

quote

GB/T 7714-2015 [1] Khrystyna Ivaniuk, Pavlo Stakhira, Iryna Yaremchuk, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00047.
MLA [1] Khrystyna Ivaniuk, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00047.
APA [1] Khrystyna Ivaniuk, Pavlo Stakhira, Iryna Yaremchuk, Stepan Kutsiy, Tetiana Bulavinets, Dmytro Volyniuk, Ivan Klymenko, Galyna Sych, Nataliya KaraushKarmazin, Amjad Ali, Aliaksei Vaitusionak, Sergei V. Kostjuk, Juozas Vidas Grazulevicius, & Glib V. Baryshnikov. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00047
IEEE [1] Khrystyna Ivaniuk, Pavlo Stakhira, Iryna Yaremchuk, Stepan Kutsiy, Tetiana Bulavinets, Dmytro Volyniuk, Ivan Klymenko, Galyna Sych, Nataliya KaraushKarmazin, Amjad Ali, Aliaksei Vaitusionak, Sergei V. Kostjuk, Juozas Vidas Grazulevicius, and Glib V. Baryshnikov, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00047. keywords: {exciplex OLED fluorescence polymer quantum dots charge transfer}