The Latest Development of Multiphase La-Mg-Ni Hydrogen Storage Alloy on Preparation Technology AITranslate
Abstract AITranslate
The microstructure and electrochemical property of multiphase La-Mg-Ni hydrogen storage alloy are influenced by its preparation techniques.The latest development in this area is reviewed.The microstructure of the La-Mg-Ni alloy plays a decisive role on its electrochemical parameters.Based on this view,the advantages and disadvantages of different preparation techniques are compared to provide ideas and basis for preparing hydrogen storage alloy of excellent electrode performance.
KeyWords AITranslate
1朱春玲,阎汝煦,王大辉,康龙,章应,罗永春.表面包覆镍处理La_(0.67)Mg_(0.33)Ni_(2.5)Co_(0.5)贮氢合金电极的电化学性能[J].稀有金属材料与工程,2006,35(4):573-576. 被引量:11
2张羊换,赵栋梁,董小平,祁焱,郭世海,王新林.Effects of rapid quenching on structure and electrochemical characteristics of La_(0.5)Ce_(0.2)Mg_(0.3)Co_(0.4)Ni_(2.6-x)Mn_x(x=0-0.4) electrode alloys[J].中国有色金属学会会刊:英文版,2009,19(2):364-371. 被引量:3
3DONG Xiaoping Lü Fanxiu ZHANG Yanghuan YANG Liying FENG Meng WANG Xinlin.Effects of rapid quenching on structure and cycle stability of La-Mg-Ni-Co type hydrogen storage alloy[J].稀有金属:英文版,2006(z1):207-212. 被引量:4
4康龙,田晓光,罗永春,阎汝煦.La-Mg-Ni系A_2B_7型贮氢合金表面包覆铜及其电化学性能[J].兰州理工大学学报,2008,34(4):1-5. 被引量:6
5安富强,李平,郑雪萍,曲选辉.用SPS技术制备La-Mg-Ni储氢合金的工艺探究[J].稀有金属材料与工程,2007,36(5):907-909. 被引量:11
6吴彦军,王大辉,罗永春,康龙,闫汝煦.快速凝固制备La_2Mg_(0.9)Ni_(7.5)Co_(1.5)Al_(0.1)贮氢合金的相结构及电化学性能[J].稀有金属材料与工程,2007,36(10):1856-1860. 被引量:3
7安富强,李平,曲选辉,郑雪萍.一种改善La-Mg-Ni贮氢电极合金性能的方法[J].北京科技大学学报,2008,30(3):263-266. 被引量:6
8董小平,吕反修,张羊换,杨丽颖,王新林.Effect of annealing temperature on microstructure and electrochemical performance of La_(0.75)Mg_(0.25)Ni_(3.5)Co_(0.2) hydrogen storage electrode alloy[J].稀土学报:英文版,2008,26(1):99-104. 被引量:8
9斯庭智,张庆安,刘 宁.Phase structure and electrochemical properties of laser sintered La_2MgNi_9 hydrogen storage electrode alloys[J].稀土学报:英文版,2008,26(4):598-603. 被引量:3
1蔡鑫,魏范松,胥小丽,肖佳宁,魏范娜.退火温度对La_4MgNi_(17.5)Co_(1.5)贮氢合金结构和性能的影响[J].金属功能材料,2015,22(4):16-20. 被引量:1
1朱凡红,魏范松,肖佳宁,蔡鑫,高旭红.快速凝固LaMg_(0.25)Ni_(4.0-x)Co_(0.75)Al_x(x=0~0.3)合金的相结构与电化学性能[J].金属功能材料,2015,22(6):34-38.
1吕东显,李青华,董小平.复相La-Mg-Ni系贮氢合金的退火研究进展[J].金属热处理,2009,34(12):68-72.
2董小平,杨丽颖,王青,林玉芳,赵栋梁,张羊换.热处理La-Mg-Ni系贮氢合金微观结构研究进展[J].中国材料进展,2010,29(3):44-48.
3吴静然.贮氢合金La-Mg-Ni系的贮氢性能[J].承德石油高等专科学校学报,2011,13(2):39-41.
4张羊换,董小平,王国清,郭世海,任江远,王新林.铸态及快淬态La-Mg-Ni系(PuNi_3型)贮氢合金的循环稳定性[J].中国有色金属学报,2005,15(5):705-710. 被引量:9
5张羊换,董小平,郭世海,冯猛,任江远,王新林.硼及快淬工艺对La-Mg-Ni系贮氢合金的微观结构及电化学容量的影响[J].包头钢铁学院学报,2006,25(1):27-31.
6张羊换,董小平,郭世海,王国清,任江远,王新林.快淬工艺对La-Mg-Ni系贮氢合金微观结构及电化学性能的影响[J].稀有金属材料与工程,2006,35(3):467-471.
7张羊换,董小平,王国清,任江远,郭世海,王新林.铸态及快淬态La_2Mg(Ni_(0.85)Co_(0.15))_9Cr_x(x=0~0.2)电极合金的微观结构及电化学性能[J].稀有金属材料与工程,2006,35(6):876-879. 被引量:3
8张羊换,李保卫,任慧平,董小平,赵小龙,王新林.添加硼对La-Mg-Ni系(PuNi_3-型)贮氢合金微观结构及电化学性能的影响[J].中南大学学报:自然科学版,2007,38(2):218-224. 被引量:1
9赵小龙,张羊换,董小平,任江远,冯猛,王新林.元素替代在制备La-Mg-Ni系贮氢电极合金中的应用[J].金属功能材料,2006,13(6):26-31. 被引量:3
10张羊换,董小平,郭世海,冯猛,任江远,王新林.铸态及快淬态La_2Mg(Ni_(0.85)Co_(0.15))_9B_x(x=0~0.2)贮氢合金的微观结构与电化学容量(英文)[J].功能材料,2006,37(3):500-504. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.454[金属学及工艺—金属材料]
Citation Information:
The microstructure and electrochemical property of multiphase La-Mg-Ni hydrogen storage alloy are influenced by its preparation techniques.The latest development in this area is reviewed.The microstructure of the La-Mg-Ni alloy plays a decisive role on its electrochemical parameters.Based on this view,the advantages and disadvantages of different preparation techniques are compared to provide ideas and basis for preparing hydrogen storage alloy of excellent electrode performance.
quote
| GB/T 7714-2015 | [1] DONG Xiao-ping, YANG Li-ying, CHEN Rong, et al. The Latest Development of Multiphase La-Mg-Ni Hydrogen Storage Alloy on Preparation Technology[J]. Rare Metals and Cemented Carbides, 2010(3): 57-62. |
| MLA | [1] DONG Xiao-ping, et al., "The Latest Development of Multiphase La-Mg-Ni Hydrogen Storage Alloy on Preparation Technology." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 57-62. |
| APA | [1] DONG Xiao-ping, YANG Li-ying, CHEN Rong, & LIN Yu-fang. (2010). The Latest Development of Multiphase La-Mg-Ni Hydrogen Storage Alloy on Preparation Technology. Rare Metals and Cemented Carbides(3), 57-62. |
| IEEE | [1] DONG Xiao-ping, YANG Li-ying, CHEN Rong, and LIN Yu-fang, "The Latest Development of Multiphase La-Mg-Ni Hydrogen Storage Alloy on Preparation Technology," Rare Metals and Cemented Carbides, no. 3, pp. 57-62, 2010. keywords: {multiphase La-Mg-Ni alloy series;preparation technology;microstructure;electrochemical property} |