The Latest Development of Pyrometallurgical Technology for Processing Anode Slime AITranslate
Abstract AITranslate
The latest development at home and abroad of anode slime pyrometallurgical treatment process is briefly reviewed from its technology and equipment in the three process steps of reducing smelting,oxidation refining,and comprehensive recovery of valuable metals.The gap between domestic and foreign anode slime pyrometallurgical processes is analyzed and studied.Oxygen-enriched air smelting and process subdivision comprehensive recovery based on automatic control are the development direction of the anode slime pyrometallurgy.
KeyWords AITranslate
1周洪武.铅阳极泥冶炼技术简评和电热连续熔炼的可行性[J].有色冶炼,2002,31(4):7-11. 被引量:12
2刘宏伟.三段熔炼法处理低品位阳极泥的研究与实践[J].有色矿冶,1998,14(5):23-27. 被引量:3
3杨茂才.铅阳极泥综合利用工艺技术进展[J].贵金属,1998,19(3):55-58. 被引量:18
1李怀仁,陈家辉,徐庆鑫,和晓才,翟中标.氯化浸出铅阳极泥回收金的研究[J].昆明理工大学学报:自然科学版,2011,36(5):14-19. 被引量:10
2程利振,李翔翔,张三佩,袁廷刚,田庆华.我国铜阳极泥分银渣综合回收利用研究进展[J].金属材料与冶金工程,2011,39(4):40-43. 被引量:18
3尹久发,张启旺,张敏,卢红波.锡阳极泥锡锑分离硫化挥发工艺试验研究[J].矿冶,2012,21(4):58-62. 被引量:6
4张启旺.高锑低银锡阳极泥焙烧脱锑工艺研究[J].有色金属:冶炼部分,2013(12):8-10. 被引量:3
5许帅,宋冰宜,蒋文龙,杨斌.铜铅银合金真空蒸馏回收银的研究[J].真空科学与技术学报,2015,35(8):1011-1016. 被引量:5
6张二军,杨天足,谢兆凤.从含银烟灰中回收氯化银[J].湿法冶金,2016,35(4):316-319. 被引量:1
7周君祺,张善辉,崔家友,赵祝鹏,侯绍彬.铜、铅阳极泥混配处理技术研究及应用实践[J].世界有色金属,2018,43(2):20-21. 被引量:1
8张燕,邢晓钟,曹杰义,庞燕,张发军,陈虎.阳极泥加压酸浸渣碳热还原动力学研究[J].世界有色金属,2019,0(20):1-4.
9董准勤.碱性氧压体系下高砷锑烟灰分离砷的工艺研究[J].有色金属:冶炼部分,2020(9):110-114. 被引量:2
10伊家飞,程珂珂,查国正,范凯,孔祥峰,杨斌,刘大春,徐宝强.铅阳极泥真空氧化−气化挥发脱除As、Sb和Te[J].中国有色金属学报,2022,32(1):251-261. 被引量:1
1戈保梁.2011年云南选矿年评[J].云南冶金,2012,41(2):19-32. 被引量:1
2谢刚.2011年云南冶金年评[J].云南冶金,2012,41(2):45-55. 被引量:2
3谢刚,田林.2012年云南冶金年评[J].云南冶金,2013,42(2):42-55.
4马婷,袁功启,易回阳.氯化钠-自动电位滴定法测定分银渣中银含量[J].冶金分析,2013,33(4):52-56. 被引量:11
5熊建军.分银炉渣铜铋工业试验[J].科技风,2013(11):19-20. 被引量:1
6杨德香,杨继生,白家福,马子辉,周先辉,周丽.高铋高银低金银阳极泥的处理[J].有色金属:冶炼部分,2013(6):34-36. 被引量:2
7卢红波,尹久发,张启旺,张敏.锡阳极泥硫化焙烧分离锑的热力学研究[J].稀有金属,2013,37(5):845-850. 被引量:5
8张启旺.高锑低银锡阳极泥焙烧脱锑工艺研究[J].有色金属:冶炼部分,2013(12):8-10. 被引量:3
9杨德香,袁龙飞,杨继生,白家福,马子辉.响应曲面法优化银阳极泥氯化提金工艺[J].矿冶,2014,23(1):61-63. 被引量:3
10柯剑华,郭旦奇,覃用宁,满露梅.脆硫铅锑矿中Pb-Sb预分离新工艺研究[J].有色金属:冶炼部分,2014(7):4-7. 被引量:3
1李卫锋,张晓国,郭学益,张传福.铅阳极泥中提炼白银及有价金属技术进展[J].中国贵金属,2010(10):64-67. 被引量:2
2倪飞.电炉技术新进展述评[J].马钢技术,1996(2):32-35.
3邹志毅.铁矿烧结技术新进展[J].烧结球团,1992,17(5):50-54. 被引量:1
4银瑰.我国电解金属锰生产技术新进展[J].中国锰业,1998,16(4):40-42. 被引量:1
5姚建明.铜浮渣火法处理工艺的研究现状及发展[J].有色冶金节能,2015,31(2):14-17. 被引量:9
6何俊范.钢铁材料的近形连铸连轧技术新进展[J].四川冶金,1995,17(3):37-40. 被引量:1
7彭金辉,张利波,张世敏.等离子体活化烧结技术新进展[J].云南冶金,2000,29(3):42-44. 被引量:13
8黄海泉,蒋秀魁.顽金矿石提金的技术新进展[J].湖南冶金,1996,24(5):63-64.
9朱孔林.COREX炼铁技术新进展[J].上海宝钢工程设计,2000,14(3):36-37.
10梁学民,于家谋,冯绍忠,冷正旭.九十年代我国铝电解技术新进展[J].轻金属,2000(2):33-38. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF81[冶金工程—有色金属冶金]
Citation Information:
The latest development at home and abroad of anode slime pyrometallurgical treatment process is briefly reviewed from its technology and equipment in the three process steps of reducing smelting,oxidation refining,and comprehensive recovery of valuable metals.The gap between domestic and foreign anode slime pyrometallurgical processes is analyzed and studied.Oxygen-enriched air smelting and process subdivision comprehensive recovery based on automatic control are the development direction of the anode slime pyrometallurgy.
quote
| GB/T 7714-2015 | [1] LI Wei-feng, ZHANG Xiao-guo, GUO Xue-yi, et al. The Latest Development of Pyrometallurgical Technology for Processing Anode Slime[J]. Rare Metals and Cemented Carbides, 2010(3): 63-67. |
| MLA | [1] LI Wei-feng, et al., "The Latest Development of Pyrometallurgical Technology for Processing Anode Slime." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 63-67. |
| APA | [1] LI Wei-feng, ZHANG Xiao-guo, GUO Xue-yi, & ZHANG Chuan-fu. (2010). The Latest Development of Pyrometallurgical Technology for Processing Anode Slime. Rare Metals and Cemented Carbides(3), 63-67. |
| IEEE | [1] LI Wei-feng, ZHANG Xiao-guo, GUO Xue-yi, and ZHANG Chuan-fu, "The Latest Development of Pyrometallurgical Technology for Processing Anode Slime," Rare Metals and Cemented Carbides, no. 3, pp. 63-67, 2010. keywords: {anode slime;pyrometallurgical technology;oxygen-enriched air smelting;automatic control;process subdivision comprehensive recovery} |