Determination of Trace Arsenic in Molybdenum Metal by Hydride Generation Flame Atomic Absorption Spectrometry AITranslate

Ningxia Oriental Tantalum Co., Ltd. Analysis and Testing Center;Ningxia Oriental Tantalum Co., Ltd. Analysis and Testing Center
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The molybdenum metal samples were dissolved with hydrogen peroxide and then their trace arsenic contents were determined by hydride generation flame atomic absorption spectrometry.The results show that the above method is of good accuracy and precision with 91.8%~102.0% standardized recovery,9.96% RSD,0.28 μg/L arsenic detection limit.

KeyWords AITranslate

arsenic determination hydride generation flame atomic absorption spectrometry molybdenum metal

1钟俊华.火焰原子吸收光谱法测定钼、铋精矿中的银[J].上海有色金属,1996,17(4):176-180. 被引量:1

2乐爱山,赵收创,何学文,卢玉琦.石墨炉原子吸收光谱法测定高纯二硫化钼中铜铅[J].冶金分析,2004,24(3):51-53. 被引量:6

3李岩.氢化物发生原子荧光光谱法测定钼精矿中砷和铋[J].光谱实验室,2001,18(1):107-111. 被引量:8

1新催化剂使合成烯异构体成为可能[J].中国科技信息,2011(9):3-3.

2蔡铁军,邓谦,黄德发,彭振山,龙云飞,陈亚中.过渡金属钼钒砷杂多化合物的合成与TPR,TPD研究[J].无机化学学报,2002,18(6):602-606. 被引量:7

3新催化剂使合成烯异构体成可能[J].光机电信息,2011,28(4):68-68.

4侯列奇,李洁.电感耦合等离子体原子发射光谱法测定金属钼中10种微量元素[J].理化检验:化学分册,2009,45(2):148-150. 被引量:11

5李汉超.ICP–AES法测定金属钼中微量Fe,Ni[J].化学分析计量,2014,23(4):73-75. 被引量:3

6钼矿[J].资源与人居环境,2008(3):26-27.

7石晓波,李春根,汪德先,傅海萍.过渡金属钼钒砷酸盐纳米微粒的固相合成与表征[J].化学研究与应用,2004,16(5):619-622. 被引量:2

8苑洁,霍韬光,王艳蕾,郭婧潭,焦雪鑫,张颖花,袁媛,高岚岳,姜泓.HG-FAAS法测定雄黄染毒小鼠肝及肾脏中的砷含量[J].化学研究,2015,26(1):61-63. 被引量:3

9徐志贤,方秋生,张贵云.三溴偶氮胂直接光度法测定钼中镧[J].稀有金属与硬质合金,2008,36(3):45-47. 被引量:7

10蔡铁军,邓谦,彭振山,龙云飞,邓彤彤,宾艳娥.碱金属碱土金属钼钒砷杂多酸盐的合成与表征[J].湘潭师范学院学报:社会科学版,2000,21(6):3-6. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:O657.31[理学—分析化学]

Citation Information:

The molybdenum metal samples were dissolved with hydrogen peroxide and then their trace arsenic contents were determined by hydride generation flame atomic absorption spectrometry.The results show that the above method is of good accuracy and precision with 91.8%~102.0% standardized recovery,9.96% RSD,0.28 μg/L arsenic detection limit.

quote

GB/T 7714-2015 [1] ZHANG Jun-feng, ZHANG Hong-mei. Determination of Trace Arsenic in Molybdenum Metal by Hydride Generation Flame Atomic Absorption Spectrometry[J]. Rare Metals and Cemented Carbides, 2010(3): 54-56.
MLA [1] ZHANG Jun-feng, and ZHANG Hong-mei. "Determination of Trace Arsenic in Molybdenum Metal by Hydride Generation Flame Atomic Absorption Spectrometry." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 54-56.
APA [1] ZHANG Jun-feng, & ZHANG Hong-mei. (2010). Determination of Trace Arsenic in Molybdenum Metal by Hydride Generation Flame Atomic Absorption Spectrometry. Rare Metals and Cemented Carbides(3), 54-56.
IEEE [1] ZHANG Jun-feng and ZHANG Hong-mei, "Determination of Trace Arsenic in Molybdenum Metal by Hydride Generation Flame Atomic Absorption Spectrometry," Rare Metals and Cemented Carbides, no. 3, pp. 54-56, 2010. keywords: {arsenic determination;hydride generation flame atomic absorption spectrometry;molybdenum metal}