Recent Development Prospect of Separation of Scattered Metals with Solvent-impregnated Resins Process AITranslate

Department of Environmental Science and Engineering, Harbin Institute of Technology;School of Environmental Science and Engineering, Shanghai Jiaotong University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The current situation and prospect of separating scattered metals using solvent-impregnated resins(SIRs)process have been reviewed according to the types of SIRs.Such SIRs contain neutral organophosphorus extractants or acidic organophosphorus ones.The mechanism of SIR sorption is basically similar to the case of solvent extraction. The effective separation of scattered metals can be obtained under properly-controlled conditions.More study is required in respect of the improvement of the intensity and stability of the solvent-impregnated resin,separating mechanism,mass transfer mathematical model so as to provide theoretical criteria for its industrial application.The said technology will open up a new approach for the separation of scattered metals.

KeyWords AITranslate

separation solvent-impregnated resins rare metals

1宋金如,龚治湘,丁红芳.P_(350)萃淋树脂分离微量镓的性能研究[J].华东地质学院学报,1997,20(2):135-140. 被引量:5

2汤淑芳,赵春雷,蒋新宇.N235萃取色谱法分离锗的研究[J].有色金属:冶炼部分,2001(1):36-38. 被引量:5

3刘军深,何争光,贾淑华,蔡伟民.CL-P204萃淋树脂吸萃铟(Ⅲ)的离子交换动力学[J].稀有金属,2003,27(1):104-107. 被引量:8

4邹家炎,陈少纯.稀散金属产业的现状与展望[J].中国工程科学,2002,4(8):86-92. 被引量:18

5陈建荣,林建军,钟依均,董训杰,寿凯胜.N_(503)萃淋树脂吸萃铟的研究[J].高等学校化学学报,1996,17(8):1169-1172. 被引量:12

6何焕杰,王连英,徐勤.中性磷萃淋树脂吸附铼的性能和机理研究──Ⅴ.CL-P_(350)-KReO_4-H_2SO_4体系[J].化工冶金,1994,15(2):146-151. 被引量:1

7林建军,钟依均,陈建荣,许峰,胡建华.N503萃淋树脂吸附镓的研究[J].中国有色金属学报,1996,6(1):40-43. 被引量:6

8刘军深,周保学,杨子超,王秀山,阎居梅.CL-P_(204)萃淋树脂分离铟(Ⅲ)镓(Ⅲ)锌(Ⅱ)[J].应用化学,1999,16(3):76-78. 被引量:11

9刘建,闫英桃,胡小玲.CL-TBP萃淋树脂吸附镓的性能及应用研究[J].稀有金属,2000,24(2):157-160. 被引量:9

10高浩其,苏元复.萃淋树脂法吸附分离铟和锌[J].离子交换与吸附,1989,5(5):333-338. 被引量:5

1陈松,王培,张力,罗岁斌,郎书玲.萃取色层法净化钴溶液制备高纯钴的研究[J].稀有金属,2010,34(4):595-600. 被引量:3

2王荣耕,李学平,翟学良.离子交换树脂回收钴镍技术进展[J].无机盐工业,2005,37(11):11-13. 被引量:15

3刘军深,宋文芹,李桂华,刘春萍,陈学颖.分离提取铟的几种新方法[J].广州化工,2005,33(5):17-20. 被引量:4

4刘军深,李桂华.螯合树脂法分离回收镓和铟的研究进展[J].稀有金属与硬质合金,2005,33(4):42-45. 被引量:14

5刘军深,李桂华,宋文芹,刘春萍.螯合树脂法从酸性溶液中分离回收铟和镓[J].有色金属:冶炼部分,2006(3):32-35. 被引量:9

6丁健刚,焦利敏,王安,廖学品.磷酸化胶原纤维对Cu^(2+)的吸附特性研究[J].皮革科学与工程,2007,17(5):7-11. 被引量:2

7马军,王小华,贾永忠,徐跃伟.铟的富集与回收工艺、技术[J].盐湖研究,2008,16(3):44-51. 被引量:7

8王生军,梅毅,梁雪松,吴礼定.黄磷电炉电尘灰中镓的提取可能性[J].云南化工,2008,35(5):73-76. 被引量:4

9刘军深,袁延旭.P507萃淋树脂在盐酸介质中吸附铟(Ⅲ)的性能[J].稀有金属与硬质合金,2008,36(4):1-4. 被引量:11

10袁延旭,刘军深,王海燕.浸渍树脂自盐酸介质中吸附铟(Ⅲ)的性能[J].材料研究与应用,2009,3(2):93-96. 被引量:5

1叶竞华,蓝桥发,柯兆华,邱小英.CL-P507树脂吸附Nd^(3+)过程热力学及动力学研究[J].冶金管理,2022(1):25-27. 被引量:1

2诸爱士,徐亮,沈芬芳,成忠.钴与镍的分离技术研究综述[J].浙江科技学院学报,2007,19(3):169-174. 被引量:17

3诸爱士,成忠,沈芬芳,徐亮.Co、Ni离子分离研究[J].高校化学工程学报,2008,22(3):412-417. 被引量:7

4陈松,王培,张力,罗岁斌,郎书玲.萃取色层法净化钴溶液制备高纯钴的研究[J].稀有金属,2010,34(4):595-600. 被引量:3

5叶茂松,俎建华,王浦银,唐方东,何林锋.弱碱性阴离子交换树脂的合成及其对铼离子的吸附解吸行为研究[J].离子交换与吸附,2015,31(2):107-114. 被引量:3

6何虹,诸爱士.分光光度法测定混合液中Co(Ⅱ)、Ni(Ⅱ)含量分析[J].中国测试技术,2007,33(6):19-21. 被引量:2

7李玲,黄松涛,温建康,武名麟,刘美林.亚氨基二乙酸树脂对镍和镁离子的吸附性能研究[J].金属矿山,2008(5):44-48. 被引量:4

8韦文宾,何启贤.从湿法炼锌浸出渣中回收镓的试验研究[J].湿法冶金,2008,27(2):103-105. 被引量:5

9王生军,梅毅,梁雪松,吴礼定.黄磷电炉电尘灰中镓的提取可能性[J].云南化工,2008,35(5):73-76. 被引量:4

10李玲,温建康,阮仁满.离子交换法分离回收溶液中镍的研究进展[J].贵金属,2007,28(S1):75-79. 被引量:8

1张瑞华,戴明,吴耀华.用液膜技术分离水溶液中的铜[J].江西有色金属,1992,6(1):10-12. 被引量:6

2方秀君,李运刚.提高高炉风口使用寿命的研究现状及展望[J].金属材料与冶金工程,2008,36(4):55-59. 被引量:6

3邓敬石,阮仁满,温建康,孙雪南.中等嗜热菌浸出硫化矿的研究现状及展望[J].矿产综合利用,2002(2):33-38. 被引量:15

4耿佃桥,雷洪,陈芝会,赫冀成,黄健,李秉强.RH真空精炼过程数值模拟的研究现状及展望[J].过程工程学报,2010,10(S1):271-276. 被引量:5

5朱立光,胡斌,王杏娟,马坤霞,韩毅华.连铸保护渣析晶行为的研究现状及展望[J].材料导报,2013,27(11):77-82. 被引量:10

6邓三才,肖志瑜,陈进,许阳,关航健.粉末冶金高速压制技术的研究现状及展望[J].粉末冶金材料科学与工程,2009,14(4):213-217. 被引量:8

7李华昌,周春山,符斌.铂族金属溶剂萃取分离新进展[J].稀有金属,2001,25(4):297-302. 被引量:23

8李耀威,古国榜.活化-溶剂萃取技术分离铑的研究进展[J].稀有金属,2004,28(5):912-916. 被引量:10

9罗吉束.矿浆电解的研究现状及展望[J].黄金科学技术,2003,11(6):36-43. 被引量:6

10刘祥萱,杨文斌,杨绪杰,陆路德,汪信.酸性含磷萃取剂萃铟机理及性能规律研究[J].有色金属:冶炼部分,1998(4):33-36. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF843[冶金工程—有色金属冶金]

Citation Information:

The current situation and prospect of separating scattered metals using solvent-impregnated resins(SIRs)process have been reviewed according to the types of SIRs.Such SIRs contain neutral organophosphorus extractants or acidic organophosphorus ones.The mechanism of SIR sorption is basically similar to the case of solvent extraction. The effective separation of scattered metals can be obtained under properly-controlled conditions.More study is required in respect of the improvement of the intensity and stability of the solvent-impregnated resin,separating mechanism,mass transfer mathematical model so as to provide theoretical criteria for its industrial application.The said technology will open up a new approach for the separation of scattered metals.

quote

GB/T 7714-2015 [1] LIU Jun-shen, CAI Wei-min. Recent Development Prospect of Separation of Scattered Metals with Solvent-impregnated Resins Process[J]. Rare Metals and Cemented Carbides, 2003(4): 36-39.
MLA [1] LIU Jun-shen, and CAI Wei-min. "Recent Development Prospect of Separation of Scattered Metals with Solvent-impregnated Resins Process." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 36-39.
APA [1] LIU Jun-shen, & CAI Wei-min. (2003). Recent Development Prospect of Separation of Scattered Metals with Solvent-impregnated Resins Process. Rare Metals and Cemented Carbides(4), 36-39.
IEEE [1] LIU Jun-shen and CAI Wei-min, "Recent Development Prospect of Separation of Scattered Metals with Solvent-impregnated Resins Process," Rare Metals and Cemented Carbides, no. 4, pp. 36-39, 2003. keywords: {separation;solvent-impregnated resins;rare metals}