daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation and Treatment of High-density Alloy Powder AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation of metal powders,composite powders and alloy powders of high density alloy is reviewed.The process flowsheet and characteristics of various powders are introduced.The treatment of tungsten powder is also introduced.

KeyWords AITranslate

high-density alloy powder preparation

1张丽英,吴成义,汪志勇,晏洪波,吴庆华.硬质合金用纳米级(W,Ni,Fe,V)系复合氧化物粉末的制备[J].金属学报,1999,35(2):152-154. 被引量:25

2陈绍衣.紫色氧化钨制取钨粉[J].中南矿冶学院学报,1994,25(5):607-611. 被引量:19

3范景莲,黄伯云,曲选辉,李益民.W-Ni-Fe高比重合金纳米晶预合金粉的制备[J].粉末冶金技术,1999,17(2):89-93. 被引量:40

4陈进,黄伯云.我国金属粉末及其制备工艺的发展[J].材料导报,1994(2):15-18. 被引量:5

5曹茂盛,李文彬,秦柏.Fe-Ni-Co合金超细粉的制备[J].金属科学与工艺,1991,10(3):43-46. 被引量:4

6姜文伟,普崇恩.等离子喷雾法制取球形钨粉工艺探讨[J].硬质合金,2000,17(2):85-88. 被引量:19

7张丽英,吴成义,李刚,胡剑辉,吴庆华.纳米级W-Ni-Fe-Y系硬质合金复合氧化物粉末的制备[J].粉末冶金工业,1998,8(6):23-26. 被引量:18

8Haer.,ST,李金平.对泰勒法制备的高比重钨合金固相烧结预合金粉并随后冷变形[J].国外金属加工,1998(3):30-36. 被引量:1

9Chen.,RF.快速冷凝钨合金粉末[J].钨钼材料,1993(2):4-9. 被引量:1

10刘正春,王志法,李方,姜国圣.钨粉的等离子体球化[J].稀有金属与硬质合金,1999,27(3):7-10. 被引量:12

1李泽全,胡玲,卢姣,刘楠,韩梅.熔盐电脱氧法制备合金时物质间相互影响的研究进展[J].稀有金属,2016,40(11):1169-1176. 被引量:3

2张家润,刘智勇,刘志宏,李启厚.高纯铼及其化合物的制备与应用研究进展[J].粉末冶金材料科学与工程,2020,25(4):273-279. 被引量:6

3李晶,闫峰,左羽飞,王宇晴,王锦,王娜,党晓明,刘东新,刘晓辉.铼资源、市场及技术进展[J].中国钼业,2023,47(2):8-15.

1焦芸芬,王旭,廖春发,孙强超,蔡伯清,汤浩.Na3AlF6-AlF3-LiF-MgF2-Al2O3-Sm2O3熔盐体系表面张力的研究[J].稀有金属,2018,42(1):75-82. 被引量:1

2陈征,赵兴科.致密ZrO2陶瓷板表面金属层的熔盐电解法制备[J].稀有金属,2018,42(2):175-181. 被引量:3

3贾雷,严红燕,李慧,刘畅,张帅.熔盐电脱氧法制备金属及合金的研究进展[J].矿产综合利用,2020(3):69-77. 被引量:3

4周小彬,沈婕,原慷,王芦燕.铼酸铵及铼粉制备典型工艺中碳杂质去除研究[J].有色金属工程,2021,11(9):11-16.

5房孟钊,宁瑞,李伟.4N级铼酸铵的工艺研究及应用[J].硫酸工业,2021(8):5-8. 被引量:3

6邱林飞,丁波,刘红旭,胡宝群,王战永,肖柯相.川北广元田坝子剖面含铀沥青脉的发现及其地质意义[J].地质论评,2022,68(1):335-347.

7宋文平,邬莉婷,李自强,封永斌,裴玲芳,何泽彬.稀有金属元素铼的测定方法探究[J].科技创新与应用,2022,12(4):114-116. 被引量:1

8陈昆昆,李林波,操齐高,孟晗琪.从沉钨钼后液中制备高纯铼酸铵[J].稀有金属材料与工程,2022,51(8):3049-3056.

9李晶,闫峰,左羽飞,王宇晴,王锦,王娜,党晓明,刘东新,刘晓辉.铼资源、市场及技术进展[J].中国钼业,2023,47(2):8-15.

1肖英龙.日本合金粉末生产技术的新进展[J].四川冶金情报,1991(7):7-8.

2О.,ПН,杨杉.冶金企业采用金属粉未制品的前景[J].国外金属材料,1990(1):29-30.

3王洪海.合金粉末的生产与应用[J].粉末冶金工业,1994,4(2):52-57.

4刘曼朗.Sm—Fr—N系列合金粉末及其制造方法[J].粉末冶金工业,2003,13(1):46-46.

5郭品河.钙在钢和合金生产中的应用[J].长城技术,1990(2):11-20. 被引量:1

6郝斌.高密度烧结钛合金产品的开发[J].钛工业进展,1995(5):24-25.

7吴敢生.耐磨合金粉末碳弧堆焊法及其应用[J].中国建材装备,1991(2):31-34.

8范景莲,黄伯云,曲选辉.PIM高密度合金在液相烧结过程中的变形[J].中南工业大学学报,2000,31(1):47-50. 被引量:4

9尚文智.机械合金化法制取微晶弥散的Cu—Ti合金粉末[J].工程设计与应用研究,1994(2):20-22.

10曹勇家.苏联铁基粉末及合金粉末生产概况[J].粉末冶金通讯,1990(2):17-21.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.71[冶金工程—粉末冶金]

Citation Information:

The preparation of metal powders,composite powders and alloy powders of high density alloy is reviewed.The process flowsheet and characteristics of various powders are introduced.The treatment of tungsten powder is also introduced.

quote

GB/T 7714-2015 [1] HUANG Jing-song, ZHOU Ji-cheng, LIU Wen-sheng, et al. Preparation and Treatment of High-density Alloy Powder[J]. Rare Metals and Cemented Carbides, 2003(4): 40-44.
MLA [1] HUANG Jing-song, et al., "Preparation and Treatment of High-density Alloy Powder." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 40-44.
APA [1] HUANG Jing-song, ZHOU Ji-cheng, LIU Wen-sheng, & HUANG Bo-yun. (2003). Preparation and Treatment of High-density Alloy Powder. Rare Metals and Cemented Carbides(4), 40-44.
IEEE [1] HUANG Jing-song, ZHOU Ji-cheng, LIU Wen-sheng, and HUANG Bo-yun, "Preparation and Treatment of High-density Alloy Powder," Rare Metals and Cemented Carbides, no. 4, pp. 40-44, 2003. keywords: {high-density alloy;powder;preparation}