Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor AITranslate
Abstract AITranslate
In the paper are summarized the market development of tantalum and niobium electrolytic capacitors and progress on the development and manufacturing of Ta/Nb capacitors both at home and abroad.
KeyWords AITranslate
1伍尊中,姚卫东,袁坤阳.氧含量对钽电解电容器阳极氧化膜形成及漏电流的影响[J].稀有金属与硬质合金,2006,34(2):32-34. 被引量:17
2刘莲云,马春红,黄凯,朱鸿民.热处理时间和压制密度对氮化钽粉电性能的影响[J].有色金属:冶炼部分,2012(10):34-37. 被引量:6
3封雪,焦瑞祥,张弛.片式钽电容器的耐焊接热性能与可靠性[J].科技创新导报,2019,16(14):101-101. 被引量:2
1刘勇刚,易金锋.成形烧结过程对固体电解质钽电容器电性能的影响[J].稀有金属与硬质合金,2008,36(4):17-19. 被引量:6
2李仲香,郑金风,张健康,包玺芳.影响电容器钽阳极漏电流因素分析[J].宁夏工程技术,2010,9(2):108-110. 被引量:7
3刘莲云,马春红,黄凯,朱鸿民.热处理时间和压制密度对氮化钽粉电性能的影响[J].有色金属:冶炼部分,2012(10):34-37. 被引量:6
4高路.掺氮及氮化钽粉的研究进展[J].广州化工,2013,41(3):15-17. 被引量:1
5李军义,孙本双,王东新,任晓,何季麟.氧含量对FFC法制备钽粉形貌和电容的影响[J].稀有金属材料与工程,2013,42(4):849-852. 被引量:3
6帅柱军,余琨,何坤池.电容器钽粉镁处理降氧工艺探究[J].硬质合金,2013,30(2):86-90. 被引量:2
7石维,杨邦朝,张选红,方鸣,马建华,李玮,王兴伟.电化学Ta_2O_5薄膜漏电流机理的研究进展[J].化工进展,2013,32(4):832-836.
8高路,刘莲云,黄凯,朱鸿民.纳米氮化钽粉末的后处理[J].有色金属工程,2013,3(6):27-29.
9张卜升,许万祥,陈姝晖,马光.含钽合金渣中钽的回收[J].有色金属:冶炼部分,2014(9):47-50. 被引量:2
10张学清,郭顺,杨国启,谢群力,左婧懿,罗文.煅烧工艺对钽粉微观结构和电性能的影响[J].稀有金属,2018,42(1):67-74. 被引量:3
1欧阳一凤,李荐,姜翠玲,钟海云,刘建清,王德全.钽、铌电解电容器工艺研究进展(续)[J].稀有金属与硬质合金,2004,32(1):52-55. 被引量:1
2铌电解电容器将成替代品[J].国际电子变压器,2005(5).
3张荣详.中频技术的发展及其市场动态[J].电工技术交流,1993(1):35-39.
4亚洲钽电解电容器市场动态[J].电子元件与材料,1998,17(5):44-45.
5钟晖,李荐,戴艳阳,钟海云.铌电解电容器最新研究发展动态[J].稀有金属,2002,26(2):139-142. 被引量:10
6卢云,蒋美莲,杨邦朝.铌电解电容器研究动态[J].材料导报,2005,19(5):23-25. 被引量:3
7刘春娜.国内光伏发电市场动态[J].电源技术,2011,35(2):133-135. 被引量:2
8温晓立,袁宁峰,王丹鹏,张庆生.铌电容器及其性能[J].有色冶炼,2002,31(6):99-101.
9康涵昌,王贵欣,陈妙,郭和一,李成佳,刘睿,闫康平.磷酸铁锂的最新研究现状[J].贵州化工,2012,37(5):21-23.
10张辉,邸永江,晁明明,侯强.YAG:Ce^(3+)荧光粉的溶胶-凝胶法制备工艺研究进展[J].中国照明电器,2014(6):5-7.
Basic Information:
DOI:
Chinese Library Classification Number:TM535.1[电气工程—电器]
Citation Information:
In the paper are summarized the market development of tantalum and niobium electrolytic capacitors and progress on the development and manufacturing of Ta/Nb capacitors both at home and abroad.
quote
| GB/T 7714-2015 | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, et al. Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor[J]. Rare Metals and Cemented Carbides, 2003(4): 32-35. |
| MLA | [1] OU Yang-yi-feng, et al., "Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 32-35. |
| APA | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, ZHONG Hai-yun, LIU Jian-qing, & WANG De-quan. (2003). Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor. Rare Metals and Cemented Carbides(4), 32-35. |
| IEEE | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, ZHONG Hai-yun, LIU Jian-qing, and WANG De-quan, "Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor," Rare Metals and Cemented Carbides, no. 4, pp. 32-35, 2003. keywords: {niobium electrolytic capacitor;tantalum electrolytic capacitor;technological study;market trend} |