daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Intelligent safety management technology for power and energy storage batteries: Advancements and trends AITranslate

1.School of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100083, China
2.Shunde Innovation School, University of Science and Technology Beijing, Foshan, Guangdong 528000, China
3.Warwick Manufacturing Group, University of Warwick, Coventry CV4 7AL, United Kingdom
4.Research Center for Fire Safety Engineering, The Hong Kong Polytechnic University, HongKong, China
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The increasing reliance on batteries in transportation and energy storage sectors plays a pivotal role in addressing the challenges of energy security and grid power instability. However, the recurrent occurrence of battery safety incidents has emerged as the primary obstacle to their more extensive deployment. This necessitates the implementation of precise and efficient battery safety management technology to enhance the safety of batteries throughout their lifecycle, safeguarding the users’ assets and optimizing energy utilization. This article explores battery safety management technologies for power and energy batteries, starting with an overview of battery technology and then reviewing battery applications, failure mechanisms, and the analysis of existing intelligent safety management technologies. Finally, the paper consolidates current advancements, pinpoints gaps, and projects future trends in intelligent safety management technologies for power and energy-storage batteries. The insights presented will serve as a valuable reference and guideline for future research and development of battery safety management technology.

KeyWords AITranslate

power battery energy storage battery fault mechanism safety management technology advancement and trend

[1]D. Qiao, X. Wei, W. Fan, B. Jiang, X. Lai, Y. Zheng, X. Tang, and H. Dai, "Toward safe carbon–neutral transportation: Battery internal short circuit diagnosis based on cloud data for electric vehicles," Applied Energy, vol. 317, p. 119168, 2022.

[2]Z. Cheng, B. Zhong, Z. Ni, Z. Y. Cheng, B. L. Zhong, Z. X. Ni, W. Q. Jing, S. Q. Zhang, and J. Liu, "Research progress on simultaneous control of mechanical and magnetic properties of high-strength non-oriented silicon steel for new energy vehicle driving motors," Chinese Journal of Engineering, vol. 45, no. 09, pp. 1482–1492, 2023.

[3]X. Lei, X. Liang, R. Yang, F. Zhang, C. Wang, C. S. Lee, and Y. Tang, "Rational design strategy of novel energy storage systems: Toward high‐performance rechargeable magnesium batteries," Small, vol. 18, no. 22, p. 2200418, 2022.

[4]H. Yaqoob, Y. H. Teoh, T. S. Goraya, F. Sher, M. A. Jamil, and T. Rashid, "Energy evaluation and environmental impact assessment of transportation fuels in Pakistan," Case Studies in Chemical and Environmental Engineering, vol. 3, p. 100081, 2021.

[5]A. Joshi, "Review of vehicle engine efficiency and emissions," SAE International Journal of Advances and Current Practices in Mobility, vol. 4, no. 2022-01-0540, pp. 1704–1733, 2022.

[6]L. Qi, J. Zhao, Q. Li, S. Su, Y. Lai, F. Deng, H. Man, X. Wang, Y Lin, Y. Ding, and H. Liu, "Primary organic gas emissions from gasoline vehicles in China: Factors, composition and trends," Environmental Pollution, vol. 290, p. 117984, 2021.

[7]A. Ghosh, "Possibilities and challenges for the inclusion of the electric vehicle (EV) to reduce the carbon footprint in the transport sector: A review," Energies, vol. 13, no. 10, p. 2602, 2020.

[8]P. Ahmadi and A. Khoshnevisan, "Dynamic simulation and lifecycle assessment of hydrogen fuel cell electric vehicles considering various hydrogen production methods," International Journal of Hydrogen Energy, vol. 47, no. 62, pp. 26758–26769, 2022.

[9]X. Lai, J. Yao, C. Jin, H. Wang, C. Xu, and Y. Zheng, "A review of lithium-ion battery failure hazards: Test standards, accident analysis, and safety suggestions," Batteries, vol. 8, no. 11, p. 248, 2022.

[10]M. A. Hannan, S. B. Wali, P. J. Ker, M.S. Abd Rahman, M. Mansor, V. K. Ramachandaramurthy, K. M. Muttaqi, T. M. I. Mahlia, and Z. Y. Dong, "Battery energy-storage system: A review of technologies, optimization objectives, constraints, approaches, and outstanding issues," Journal of Energy Storage, vol. 42, p. 103023, 2021.

[11]C. Zhang, Y. L. Wei, P. F. Cao, and M. C. Lin, "Energy storage system: Current studies on batteries and power condition system," Renewable and Sustainable Energy Reviews, vol. 82, pp. 3091–3106, 2018.

[12]X. Fan, B. Liu, J. Liu, J. Ding, X. Han, Y. Deng, X. Lv, Y. Xie, B. Chen, W. Hu, and C. Zhong, "Battery technologies for grid-level large-scale electrical energy storage," Transactions of Tianjin University, vol. 26, pp. 92–103, 2020.

[13]B. Dunn, H. Kamath, and J. M. Tarascon, "Electrical energy storage for the grid: a battery of choices," Science, vol. 334, no. 6058, pp. 928–935, 2011.

[14]J. Hong, Z. Wang, C. Qu, Y. Zhou, T. Shan, J. Zhang, and Y. Hou, "Investigation on overcharge-caused thermal runaway of lithium-ion batteries in real-world electric vehicles," Applied Energy, vol. 321, p. 119229, 2022.

[15]S. Verma, S. Mishra, A. Gaur S. Chowdhury, S. Mohapatra, G. Dwivedi, and P. Verma, "A comprehensive review on energy storage in hybrid electric vehicle," Journal of Traffic and Transportation Engineering (English Edition), vol. 8, no. 5, pp. 621–637, 2021.

[16]K. Detka and K. Górecki, "Selected Technologies of Electrochemical Energy Storage—A Review," Energies, vol. 16, no. 13, p. 5034, 2023.

[17]M. Tawalbeh, A. Farooq, R. Martis, and A. Al-Othman, "Optimization techniques for electrochemical devices for hydrogen production and energy storage applications," International Journal of Hydrogen Energy, vol. 52, pp. 1058–1092, 2023.

[18]S. Cheng, G. Zhao, M. Gao, Y. Shi, M. Huang, and M. Marefati, "A new hybrid solar photovoltaic/phosphoric acid fuel cell and energy storage system; Energy and Exergy performance," International Journal of Hydrogen Energy, vol. 46, no. 11, pp. 8048–8066, 2021.

[19]C. C. Chan, E. W. C. Lo, and W. S. Shen, "The available capacity computation model based on artificial neural network for lead–acid batteries in electric vehicles," Journal of power sources, vol. 87, no. 1–2, pp. 201–204, 2000.

[20]D. Qiao, X. Wang, Lai X, Y. Zheng, X. Wei, and H. Dai, "Online quantitative diagnosis of internal short circuit for lithium-ion batteries using incremental capacity method," Energy, vol. 243, p. 123082, 2022.

[21]J. Hong, K. Li, F. Liang, H. Yang, C. Zhang, Q. Yang, and J. Wang, "A novel state of health prediction method for battery system in real-world vehicles based on gated recurrent unit neural networks," Energy, vol. 289, p. 129918, 2024.

[22]A. A. Kebede, T. Coosemans, M. Messagie, T. Jemal, H. A. Behabtu, J. Van Mierlo, and M. Berecibar, "Techno-economic analysis of lithium-ion and lead-acid batteries in stationary energy storage application," Journal of Energy Storage, vol. 40, p. 102748, 2021.

[23]Z. Šimić, D. Topić, G. Knežević, and D. Pelin, "Battery energy storage technologies overview," International Journal of Electrical and Computer Engineering Systems, vol. 12, no. 1, pp. 53–65, 2021.

[24]M. F. Tahir, C. Haoyong, and H. Guangze, "A comprehensive review of 4E analysis of thermal power plants, intermittent renewable energy and integrated energy systems," Energy Reports, vol. 7, pp. 3517–3534, 2021.

[25]A. A. Kebede, Kalogiannis T, J Van Mierlo, and M. Berecibar, "A comprehensive review of stationary energy storage devices for large scale renewable energy sources grid integration," Renewable and Sustainable Energy Reviews, vol. 159, p. 112213, 2022.

[26]H. W. Schiffer, "Flexible operation of coal-fired power plants in Germany under the renewable energy background," Cornerstone, vol. 2, no. 4, pp. 26–31, 2014.

[27]H. Zsiborács, G. Pintér, A. Vincze, Z. Birkner, and N. H. Baranyai, "Grid balancing challenges illustrated by two European examples: Interactions of electric grids, photovoltaic power generation, energy storage and power generation forecasting," Energy Reports, vol. 7, pp. 3805–3818, 2021.

[28]X. Zhang, Z. Li, L. Luo, Y. Fan, and Z. Du, "A review on thermal management of lithium-ion batteries for electric vehicles," Energy, vol. 238, p. 121652, 2022.

[29]Z. Cui, L. Kang, L. Li, L. Wang, and K. Wang, "A combined state-of-charge estimation method for lithium-ion battery using an improved BGRU network and UKF," Energy, vol. 259, p. 124933, 2022.

[30]S. Li, K. Wang, G. Zhang, S. Li, Y. Xu, X. Zhang, X. Zhang, S. Zheng, X. Sun, and Y. Ma, "Fast charging anode materials for lithium‐ion batteries: Current status and perspectives," Advanced Functional Materials, vol. 32, no. 23, p. 2200796, 2022.

[31]M. A. Hannan, S. B. Wali, P. J. Ker, M. S. Abd Rahman, M. Mansor, V. K. Ramachandaramurthy, K. M. Muttaqi, T. M. I. Mahlia, and Z. Y. Dong, "Battery energy-storage system: A review of technologies, optimization objectives, constraints, approaches, and outstanding issues," Journal of Energy Storage, vol. 42, p. 103023, 2021.

[32]J. Wen, D. Zhao, and C. Zhang, "An overview of electricity powered vehicles: Lithium-ion battery energy storage density and energy conversion efficiency," Renewable Energy, vol. 162, pp. 1629–1648, 2020.

[33]F. M. N. U. Khan, M. G. Rasul, A. S. M. Sayem, and N. K. Mandal, "Design and optimization of lithium-ion battery as an efficient energy storage device for electric vehicles: A comprehensive review," Journal of Energy Storage, vol. 71, p. 108033, 2023.

[34]G. Ruan, C. Yu, X. Hu, and J. Hua, "Simulation and optimization of a new energy vehicle power battery pack structure," Journal of Theoretical and Applied Mechanics, vol. 59, no. 4, 2021

[35]G. Memmel and A. Memmel, "Chassis control system combines comfort and stability in electric buses," ATZheavy Duty worldwide, vol. 15, no. 2, pp. 34–37, 2022.

[36]A. Tansini, J. Pavlovic, and G. Fontaras, "Quantifying the real-world CO2 emissions and energy consumption of modern plug-in hybrid vehicles," Journal of Cleaner Production, vol. 362, p. 132191, 2022.

[37]J. Dižo, M. Blatnický, S. Semenov, E. Mikhailov, M. Kostrzewski, P. Droździel, and P. Šťastniak, "Electric and plug-in hybrid vehicles and their infrastructure in a particular European region," Transportation Research Procedia, vol. 55, pp. 629–636, 2021.

[38]L. Guo, X. Zhang, Y. Zou, N. Guo, J. Li, and G. Du, "Cost-optimal energy management strategy for plug-in hybrid electric vehicles with variable horizon speed prediction and adaptive state-of-charge reference," Energy, vol. 232, p. 120993, 2021.

[39]P. V. Chombo and Y. Laoonual, "A review of safety strategies of a Li-ion battery," Journal of Power Sources, vol. 478, p. 228649, 2020.

[40]L. Wang, X. Wang, and W. Yang, "Optimal design of electric vehicle battery recycling network–From the perspective of electric vehicle manufacturers," Applied Energy, vol. 275, p. 115328, 2020.

[41]C. A. O. Wenjiong, L. E. I. Bo, S. H. I. Youjie, D. O. N. G. Ti, P. E. N. G. Peng, and F. J. Y. D. Zheng, "Ponderation over the recent safety accidents of lithium-ion battery energy storage stations in South Korea," Energy Storage Science and Technology, vol. 9, no. 5, p. 1539, 2020.

[42]M. Liu, X. Cao, C. Cao, P. Wang, C. Wang, J. Pei, H. Lei, X. Jiang, R. Li, and J. Li, "A review of power conversion systems and design schemes of high-capacity battery energy storage systems," IEEE Access, vol. 10, pp. 52030–52042, 2022.

[43]S. Van der Linden, "Bulk energy storage potential in the USA, current developments and future prospects," Energy, vol. 31, no. 15, pp. 3446–3457, 2006.

[44]X. Li, L. Chen, F. Sun, Y. Hao, X. Du, and S. Mei, "Share or not share, the analysis of energy storage interaction of multiple renewable energy stations based on the evolution game," Renewable Energy, vol. 208, pp. 679–692, 2023.

[45]K. Uddin, R. Gough, J. Radcliffe, J. Marco, and P. Jennings, “Techno-economic analysis of the viability of residential photovoltaic systems using lithium-ion batteries for energy storage in the United Kingdom,” Applied Energy, vol. 206, pp. 12–21, 2017.

[46]B. D. Olaszi and J. Ladanyi, "Comparison of different discharge strategies of grid-connected residential PV systems with energy storage in perspective of optimal battery energy storage system sizing," Renewable and Sustainable Energy Reviews, vol. 75, pp. 710–718, 2017

[47]Response, Automated Demand, "The Missing Link in the Electricity Value Chain, A. McKane, I. Rhyne, A. Lekov, L. Thompson, and MA Piette." ACEEE Summer Study on Energy Efficiency in Buildings. 2008.

[48]J. Figgener, P. Stenzel, K. P. Kairies, J. Linßen, D. Haberschusz, O. Wessels, and G. Angenendt, "The development of stationary battery storage systems in Germany–A market review,” Journal of Energy Storage, vol. 29, p. 101153, 2020.

[49]H. Dai, B. Jiang, X. Hu, X. Lin, X. Wei, and M. Pecht, "Advanced battery management strategies for a sustainable energy future: Multilayer design concepts and research trends,” Renewable and Sustainable Energy Reviews, vol. 138, p. 110480, 2021.

[50]Z. P. Wang, C. G. Yuan, and X. Y. Li, "An analysis on challenge and development trend of safety management technologies for traction battery in new energy vehicles,” Automotive Engineering, vol. 42, no. 12, pp. 1606–1620, 2020.

[51]C. Ashtiani, "Analysis of battery safety and hazards' risk mitigation,” ECS Transactions, vol. 11, no. 19, p. 1, 2008.

[52]E. Cabrera-Castillo, F. Niedermeier, and A. Jossen, "Calculation of the state of safety (SOS) for lithium-ion batteries,” Journal of Power Sources, vol. 324, pp. 509–520, 2016.

[53]H. Yin, S. Ma, H. Li, G. Wen, S. Santhanagopalan, and C. Zhang, "Modeling strategy for progressive failure prediction in lithium-ion batteries under mechanical abuse,” ETransportation, vol. 7, p. 100098, 2021.

[54]G. Wang, X. Guo, J. Chen, G. Wen, and C. Zhang, "Safety performance and failure criteria of lithium-ion batteries under mechanical abuse," Energies, vol. 16, no. 17, p. 6346, 2023.

[55]B. Liu, Y. Jia, C. Yuan, L. Wang, X. Gao, S. Yin, and J. Xu, "Safety issues and mechanisms of lithium-ion battery cell upon mechanical abusive loading: A review,” Energy Storage Materials, vol. 24, pp. 85–112, 2020.

[56]Zhang J, Li X, Zhang G, J. Guo, Q. Huang, C. Wang, D. Zhou, and D. Wei, "Experimental investigation on the essential cause of the degrading performances for an overcharging ternary battery,” International Journal of Energy Research, vol. 44, no. 4, pp. 3134–3147, 2020.

[57]C. Zhao, T. Wang, Z. Huang, J. Wu, H. Zhou, M. Ma, J. Xu, Z. Wang, H. Li, J. Sun, and Q. Wang, "Experimental study on thermal runaway of fully charged and overcharged lithium-ion batteries under adiabatic and side-heating test,” Journal of Energy Storage, vol. 38, p. 102519, 2021.

[58]G. Zhang, X. Wei, S. Chen, J. Zhu, G. Han, X. Tang, W. Hua, H. Dai, and J. Ye, "Comprehensive investigation of a slight overcharge on degradation and thermal runaway behavior of lithium-ion batteries,” ACS Applied Materials & Interfaces, vol. 13, no. 29, pp. 35054–35068, 2021.

[59]J. Hong, Z. Wang, C. Qu, Y. Zhou, T. Shan, J. Zhang, and Y. Hou, "Investigation on overcharge-caused thermal runaway of lithium-ion batteries in real-world electric vehicles,” Applied Energy, vol. 321, p. 119229, 2022.

[60]Xiao Y, Yang F, Gao Z, M. Liu, J. Wang, Z. Kou, Y. Lin, Y. Li, L. Gao, Y. Chen, S. Ren, and X. Li, "Review of mechanical abuse related thermal runaway models of lithium-ion batteries at different scales,” Journal of Energy Storage, vol. 64, p. 107145, 2023.

[61]D. Qiao, X. Wei, B. Jiang, W. Fan, X. Lai, Y. Zheng, and H. Dai, "Quantitative diagnosis of internal short circuit for lithium-ion batteries using relaxation voltage," IEEE Transactions on Industrial Electronics, Early Access, 2024, DOI: 10.1109/TIE.2023.3342289

[62]J. Conzen, S. Lakshmipathy, A. Kapahi, S. Kraft, and M. DiDomizio, "Lithium ion battery energy storage systems (BESS) hazards,” Journal of Loss Prevention in the Process Industries, vol. 81, p. 104932, 2023.

[63]Y. Liu, P. Sun, S. Lin, H. Niu, and X. Huang“Self-heating ignition of open-circuit cylindrical Li-ion battery pile: Towards fire-safe storage and transport,” Journal of Energy Storage, vol. 32, p. 101842, 2020

[64]J. Tian, Y. Wang, C. Liu, and Z. Chen, "Consistency evaluation and cluster analysis for lithium-ion battery pack in electric vehicles,” Energy, vol. 194, p. 116944, 2020.

[65]C. Chang, X. P. Zhou, J. Jiang, Y. Gao, Y. Jiang, and T. Wu, "Micro-fault diagnosis of electric vehicle batteries based on the evolution of battery consistency relative position,” Journal of Energy Storage, vol. 52, p. 104746, 2022.

[66]R. Xiong, W. Sun, Q. Yu, and F. Sun, "Research progress, challenges and prospects of fault diagnosis on battery system of electric vehicles,” Applied Energy, vol. 279, p. 115855, 2020.

[67]L. Huang, L. Liu, L. Lu, X. Feng, X. Han, W. Li, M. Zhang, D. Li, X. Liu, D. U. Sauer, and M. Ouyang, "A review of the internal short circuit mechanism in lithium‐ion batteries: Inducement, detection and prevention,” International Journal of Energy Research, vol. 45, no. 11, pp. 15797–15831, 2021.

[68]P. Sun, R. Bisschop, H. Niu, and X. Huang. "A review of battery fires in electric vehicles,” Fire Technology, vol. 56, pp. 1361–1410, 2020.

[69]Y. Li, X. Liu, L. Wang, X. Feng, D. Ren, Y. Wu, G. Xu, L. Lu, J. Hou, W. Zhang, et al., "Thermal runaway mechanism of lithium-ion battery with LiNi0.8Mn0.1Co0.1O2 cathode materials,” Nano Energy, vol. 85, p. 105878, 2021.

[70]C. Ghenai, L. A. Husein, M. Al Nahlawi, A. K. Hamid, and M. Bettayeb. "Recent trends of digital twin technologies in the energy sector: A comprehensive review,” Sustainable Energy Technologies and Assessments, vol. 54, p. 102837, 2022.

[71]M. Dubarry, D. Howey, and B. Wu, "Enabling battery digital twins at the industrial scale,” Joule, vol. 7, no. 6, pp. 1134–1144, 2023.

[72]V. Talele, U. Moralı, M. S. Patil, S. Panchal, R. Fraser, M. Fowler, P. Thorat, and Y. P. Gokhale, "Computational modelling and statistical evaluation of thermal runaway safety regime response on lithium-ion battery with different cathodic chemistry and varying ambient condition,” International Communications in Heat and Mass Transfer, vol. 146, p. 106907, 2023.

[73]Z. Wang, J. Yuan, X. Zhu, H. Wang, L. Huang, Y. T. Wang, S. Q. Xu, "Overcharge-to-thermal-runaway behavior and safety assessment of commercial lithium-ion cells with different cathode materials: A comparison study,” Journal of Energy Chemistry, vol. 55, pp. 484–498, 2021.

[74]H. Cheng, J. G. Shapter, Y. Li, and G. Gao, "Recent progress of advanced anode materials of lithium-ion batteries,” Journal of Energy Chemistry, vol. 57, pp. 451–468, 2021.

[75]X. Jiang, Y. Chen, X. Meng, W. Cao, C. Liu, Q. Huang, N. Naik, V. Murugadoss, M. Huang, and Z. Guo, "The impact of electrode with carbon materials on safety performance of lithium-ion batteries: A review,” Carbon, vol. 191, pp. 448–470, 2022.

[76]Z. H. Wu, A. C. Huang, Y. Tang, Y. P. Yang, Y. C. Liu, Z. P. Li, H. L. Zhou, C. F. Huang, Z. X. Xing, C. M. Shu, and J. C. Jiang, "Thermal effect and mechanism analysis of flame-retardant modified polymer electrolyte for lithium-ion battery," Polymers, vol. 13, no. 11, p. 1675, 2021.

[77]X. Chen, S. Yan, T. Tan, P. Zhou, J. Hou, X. Feng, H. Dong, P. Wang, D. Wang, B. Wang, and M. G. Ouyang, "Supramolecular ‘flame-retardant’ electrolyte enables safe and stable cycling of lithium-ion batteries," Energy Storage Materials, vol. 45, pp. 182–190, 2022.

[78]L. Han, C. Liao, Y. Liu, H. Yu, S. Zhang, Y. Zhu, Z. Li, X. Li, Y. Kan, and Y. Hu, "Non-flammable sandwich-structured TPU gel polymer electrolyte without flame retardant addition for high performance lithium ion batteries," Energy Storage Materials, vol. 52, pp. 562–572, 2022.

[79]J. Zhu, X. Zhang, E. Sahraei, and T. Wierzbicki, "Deformation and failure mechanisms of 18650 battery cells under axial compression," Journal of Power Sources, vol. 336, pp. 332–340, 2016.

[80]D. Ouyang, J. Weng, M. Chen, and J. Wang, "What a role does the safety vent play in the safety of 18650-size lithium-ion batteries?" Process Safety and Environmental Protection, vol. 159, pp. 433–441, 2022.

[81]X. Zhang, Q. Sun, C. Zhen, Y. Niu, Y. Han, G. Zeng, D. Chen, C. Feng, N. Chen, W. Lv, and W. He, "Recent progress in flame-retardant separators for safe lithium-ion batteries." Energy Storage Materials, vol. 37, pp. 628–647, 2021.

[82]Q. Arooj and U. A. Khan, "An improved hybrid DC circuit breaker with battery banks for energy storage in HVDC system."2022 19th International Bhurban Conference on Applied Sciences and Technology (IBCAST), IEEE, pp. 603–608, 2022.

[83]Y. Lu, J. Wang, F. Liu, Y. Liu, F. Wang, N. Yang, D. Lu, and Y. Jia, "Performance optimisation of Tesla valve-type channel for cooling lithium-ion batteries," Applied Thermal Engineering, vol. 212, pp. 118583, 2022.

[84]H. Zhou, F. Zhou, S. Shi, W. Yang, and Z. Song, "Influence of working temperature on the electrochemical characteristics of Al2O3-coated LiNi0.8Co0.1Mn0.1O2 cathode materials for Li-ion batteries," Journal of Alloy and Compounds, vol. 847, p. 156412, 2020.

[85]Z. Liu, Y. Jiang, Q. Hu, S. Guo, L. Yu, Q. Li, Q. Liu, and X. Hu, "Safer lithium‐ion batteries from the separator aspect: Development and future perspectives," Energy & Environmental Materials, vol. 4, no. 3, pp. 336–362, 2021.

[86]X. Li, K. Liu, Y. Yan, J. Yu, N. Dong, B. Liu, G. Tian, S. Qi, and D. Wu, "Thermostable and nonflammable polyimide/zirconia compound separator for lithium-ion batteries with superior electrochemical and safe properties," Journal of Colloid and Interface Science, vol. 625, pp. 936–945, 2022.

[87]Y. Song, X. Liu, D. Ren, H. Liang, L. Wang, Q. Hu, H. Cui, H. Xu, J. Wang, C. Zhao, X. Zuo, and G. L. Xu, "Simultaneously blocking chemical crosstalk and internal short circuit via gel‐stretching derived nanoporous non‐shrinkage separator for safe lithium‐ion batteries," Advanced Materials, vol. 34, no. 2, p. 2106335, 2022.

[88]D. Wu, N. Dong, R. Wang, S. Qi, B. Liu, and D. Wu, "In situ construction of high-safety and non-flammable polyimide ‘Ceramic’ lithium-ion battery separator via SiO2 Nano-encapsulation," Chemical Engineering Journal, vol. 420, p. 129992, 2021.

[89]D. Li, L. Wang, C. Duan, Q. Li, and K. Wang, "Temperature prediction of lithium‐ion batteries based on electrochemical impedance spectrum: A review," International Journal of Energy Research, vol. 46, no. 8, pp. 10372–10388, 2022.

[90]Q. Bai, Q. Li, J. Zan, J. Liu, J. Ou, and J. Liu, "Influence of insulation material thickness on spread of thermal runaway in battery packs," Processes, vol. 11, no. 5, p. 1321, 2023.

[91]F. Liu, J. Wang, N. Yang, F. Wang, Y. Chen, D. Lu, H. Liu, Q. Du, X. Ren, and M. Shi, "Experimental study on the alleviation of thermal runaway propagation from an overcharged lithium-ion battery module using different thermal insulation layers," Energy, vol. 257, p. 124768, 2022.

[92]J. Gong, B. Liu, H. Lian, J. Y. Liu, H. Fu, Y. X. Miao, and J. L. Liu, "Numerical investigation of suppressing thermal runaway propagation in a lithium-ion battery pack using thermal insulators," Process Safety and Environmental Protection, vol. 176, p. 1063–1075, 2023.

[93]R. Y. Ren, Y. H. Zhao, Y. H. Diao, L. Liang, and H. R. Jing, "Active air cooling thermal management system based on U-shaped micro heat pipe array for lithium-ion battery," Journal of Power Sources, vol. 507, pp. 230314, 2021.

[94]O. Kalaf, D. Solyali, M. Asmael, Q. Zeeshan, B. Safaei, and A. Askir, "Experimental and simulation study of liquid coolant battery thermal management system for electric vehicles: A review," International Journal of Energy Research, vol. 45, no. 5, pp. 6495–6517, 2021.

[95]M. Akbarzadeh, T. Kalogiannis, J. Jaguemont, L. Jin, H. Behi, D. Karimi, H. Beheshti, J. Van Mierlo, and M. Berecibar, "A comparative study between air cooling and liquid cooling thermal management systems for a high-energy lithium-ion battery module," Applied Thermal Engineering, vol. 198, p. 117503, 2021.

[96]L. Zhao, W. Li, G. Wang, W. Cheng, and M. Chen, "A novel thermal management system for lithium-ion battery modules combining direct liquid-cooling with forced air-cooling," Applied Thermal Engineering, vol. p. 120992, 2023.

[97]S. Ahmad, Y. Liu, S. A. Khan, M. L. Hao, and X. Y. Huang, "Hybrid battery thermal management by coupling fin intensified phase change material with air cooling," Journal of Energy Storage, vol. 64, p. 107167, 2023.

[98]N. Mao, Z. Wang, T. Gao, and D. Ouyang, W. Yan, "An investigation on thermal runaway behaviours of lithium-ion battery with Li (Ni0.6Co0.2Mn0.2)O2 cathode induced by overcharge under different heat dissipation conditions," International Journal of Heat and Mass Transfer, vol. 217, p. 124677, 2023.

[99]H. Li, D. Zhou, M. Zhang, B. Liu, and C. Zhang, "Multi-field interpretation of internal short circuit and thermal runaway behavior for lithium-ion batteries under mechanical abuse," Energy, vol. 263, p. 126027, 2023.

[100]J. Chen, D. Ren, H. Hsu, L. Wang, X. He, C. Zhang, X. Feng, and M. Ouyang, "Investigating the thermal runaway features of lithium-ion batteries using a thermal resistance network model," Applied Energy, vol. 295, p. 117038, 2021.

[101]C. X. He, Q. L. Yue, Q. Chen, and T. S. Zhao, "Modeling thermal runaway of lithium-ion batteries with a venting process," Applied Energy, vol. 327, p. 120110, 2022.

[102]Y. Wang, D. Ren, X. Feng, L. Wang, and M. Ouyang, "Thermal runaway modeling of large format high-nickel/silicon-graphite lithium-ion batteries based on reaction sequence and kinetics," Applied Energy, vol. 306, p. 117943, 2022.

[103]F. Zhang, X. Feng, C. Xu, F. Jiang, and M. Ouyang, "Thermal runaway front in failure propagation of long-shape lithium-ion battery," International Journal of Heat and Mass Transfer, vol. 182, p. 121928, 2022.

[104]A. Li, J. Weng, A. C. Y. Yuen, W. Wang, H. Liu, E. W. M. Lee, J. Wang, S. Kook, and G. H. Yeoh, "Machine learning assisted advanced battery thermal management system: A state-of-the-art review," Journal of Energy Storage, vol. 60, p. 106688, 2023.

[105]C. Lv, X. Zhou, L. Zhong, C. Yan, M. Srinivasan, Z. W. Seh, C. Liu, H. Pan, S. Li, Y. Wen, and Q. Yan, "Machine learning: an advanced platform for materials development and state prediction in lithium‐ion batteries," Advanced Materials, vol. 34, no. 25, p. 2101474, 2022.

[106]T. Raoofiand and M. Yildiz, "Comprehensive review of battery state estimation strategies using machine learning for battery management systems of aircraft propulsion batteries," Journal of Energy Storage, vol. 59, p. 106486, 2023.

[107]W. Li, H. Cui, T. Nemeth, J. Jansen, C. Ünlübayir, Z. Wei, X. Feng, X. Han, M. Ouyang, H. Dai, X. Z. Wei, and D. U. Sauer, "Cloud-based health-conscious energy management of hybrid battery systems in electric vehicles with deep reinforcement learning," Applied Energy, vol. 293, p. 116977, 2021.

[108]Y. Wang, R. Xu, C. Zhou, X. Kang, and Z. Chen, "Digital twin and cloud-side-end collaboration for intelligent battery management system," Journal of Manufacturing Systems, vol. 62, pp. 124–134, 2022.

[109]Y. Zhang and M. Zhao, "Cloud-based in-situ battery life prediction and classification using machine learning," Energy Storage Materials, vol. 60, p. 106688, 2023.

[110]D. Shi, J. Zhao, C. Eze, Z. Wang, J. Wang, Y. Lian, and A. F. Burke, "Cloud-based artificial intelligence framework for battery management system," Energies, vol. 16, no. 11, p. 4403, 2023.

[111]Z. Wei, X. Yang, Y. Li, H. He, W. Li, and D. U. Sauer, "Machine learning-based fast charging of lithium-ion battery by perceiving and regulating internal microscopic states," Energy Storage Materials, vol. 56, p. 62–75, 2023.

[112]Y. Jia, J. Li, W. Yao, Y. Li, and J. Xu, "Precise and fast safety risk classification of lithium-ion batteries based on machine learning methodology," Journal of Power Sources, vol. 548, p. 232064, 2022.

[113]Y. Zhang, T. Wik, J. Bergström, M. Pecht, and C. Zou, "A machine learning-based framework for online prediction of battery ageing trajectory and lifetime using histogram data," Journal of Power Sources, vol. 526, p. 231110, 2022.

Basic Information:

DOI:10.23919/CHAIN.2024.000004

Chinese Library Classification Number:

Citation Information:

The increasing reliance on batteries in transportation and energy storage sectors plays a pivotal role in addressing the challenges of energy security and grid power instability. However, the recurrent occurrence of battery safety incidents has emerged as the primary obstacle to their more extensive deployment. This necessitates the implementation of precise and efficient battery safety management technology to enhance the safety of batteries throughout their lifecycle, safeguarding the users’ assets and optimizing energy utilization. This article explores battery safety management technologies for power and energy batteries, starting with an overview of battery technology and then reviewing battery applications, failure mechanisms, and the analysis of existing intelligent safety management technologies. Finally, the paper consolidates current advancements, pinpoints gaps, and projects future trends in intelligent safety management technologies for power and energy-storage batteries. The insights presented will serve as a valuable reference and guideline for future research and development of battery safety management technology.

quote

GB/T 7714-2015 [1] Jichao Hong, Jingsong Yang, Fengwei Liang, et al. Intelligent safety management technology for power and energy storage batteries: Advancements and trends[J]. Chain, 2024, 1(3): 203-228. DOI:10.23919/CHAIN.2024.000004.
MLA [1] Jichao Hong, et al., "Intelligent safety management technology for power and energy storage batteries: Advancements and trends." Chain, vol. 1, no. 3, 2024, pp. 203-228, https://doi.org/10.23919/CHAIN.2024.000004.
APA [1] Jichao Hong, Jingsong Yang, Fengwei Liang, Xinyang Zhang, Huaqin Zhang, Haixu Yang, Chi Zhang, Qianqian Yang, Tao Zhu, & Xinyan Huang. (2024). Intelligent safety management technology for power and energy storage batteries: Advancements and trends. Chain, 1(3), 203-228. https://doi.org/10.23919/CHAIN.2024.000004
IEEE [1] Jichao Hong, Jingsong Yang, Fengwei Liang, Xinyang Zhang, Huaqin Zhang, Haixu Yang, Chi Zhang, Qianqian Yang, Tao Zhu, and Xinyan Huang, "Intelligent safety management technology for power and energy storage batteries: Advancements and trends," Chain, vol. 1, no. 3, pp. 203-228, 2024, doi: 10.23919/CHAIN.2024.000004. keywords: {power battery;energy storage battery;fault mechanism;safety management technology;advancement and trend}