daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Conductive Thermoplastic Elastomer Composite Capacitive Strain Sensors and Their Application in a Wearable Device for Quantitative Joint Angle Prediction AITranslate

Simon Fraser University; Simon Fraser University; Simon Fraser University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wearable devices can provide valuable information for the user when completing rehabilitation or attempting to improve athletic performance. Seamlessly incorporated soft strain sensors enable the correlation of strain to more complex metrics such as quantitative multiaxis joint angle motion tracking that is useful for analysis of activities such as walking, running, or cycling. Using a dip-coating technique, a capacitive filament was produced that achieved a relatively high performance with simple materials and fabrication processes. The design of the capacitor produced a sensor with a high baseline capacitance with low noise through the use of a combination of dielectric layers and interfaces between electrodes, good mechanical response through the use of a pristine core filament to support the capacitive sensor components, and a highly stable and reliable signal without requiring exotic or expensive conductive components aided by using specific electronics. The sensor was highly linear within the sensing region required in our proof-of-concept knee brace device, which could predict knee angles to within 1.79° with a simple and easy calibration protocol.

KeyWords AITranslate

capacitive strain sensor fiber sensor wearable devices smart textiles conductive composites dipcoating motion capture Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c00708

Chinese Library Classification Number:

Citation Information:

Wearable devices can provide valuable information for the user when completing rehabilitation or attempting to improve athletic performance. Seamlessly incorporated soft strain sensors enable the correlation of strain to more complex metrics such as quantitative multiaxis joint angle motion tracking that is useful for analysis of activities such as walking, running, or cycling. Using a dip-coating technique, a capacitive filament was produced that achieved a relatively high performance with simple materials and fabrication processes. The design of the capacitor produced a sensor with a high baseline capacitance with low noise through the use of a combination of dielectric layers and interfaces between electrodes, good mechanical response through the use of a pristine core filament to support the capacitive sensor components, and a highly stable and reliable signal without requiring exotic or expensive conductive components aided by using specific electronics. The sensor was highly linear within the sensing region required in our proof-of-concept knee brace device, which could predict knee angles to within 1.79° with a simple and easy calibration protocol.

quote

GB/T 7714-2015 [1] Wanhayoi Geng, Tyler J. Cuthbert, Carlo Menon. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c00708.
MLA [1] Wanhayoi Geng, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c00708.
APA [1] Wanhayoi Geng, Tyler J. Cuthbert, & Carlo Menon. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c00708
IEEE [1] Wanhayoi Geng, Tyler J. Cuthbert, and Carlo Menon, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c00708. keywords: {capacitive strain sensor;fiber sensor;wearable devices;smart textiles;conductive composites;dipcoating;motion capture;Show More}