Highly Permeable Reverse Osmosis Membranes via Molecular Layer-by-Layer Deposition of Trimesoyl Chloride and 3,5-Diaminobenzoic Acid AITranslate
Abstract AITranslate
We present a series of polyamide membranes synthesized via molecular layer-by-layer (mLbL) deposition of trimesoyl chloride (TMC) and 3,5-diaminobenzoic acid (BA). These membranes exhibit superior NaCl rejection compared to previously reported TMC–BA membranes prepared via interfacial polymerization with the improved performance of the mLbL films attributable to higher cross-link density facilitated by the stepwise deposition process in good solvents. We compare the TMC–BA series with membranes synthesized from TMC and m-phenylenediamine (MPD), a conventional reverse osmosis membrane chemistry. At the minimum thickness capable of 90% NaCl rejection, mLbL TMC–BA membranes exhibit 50% greater water permeance than mLbL TMC–MPD.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01199
Chinese Library Classification Number:
Citation Information:
We present a series of polyamide membranes synthesized via molecular layer-by-layer (mLbL) deposition of trimesoyl chloride (TMC) and 3,5-diaminobenzoic acid (BA). These membranes exhibit superior NaCl rejection compared to previously reported TMC–BA membranes prepared via interfacial polymerization with the improved performance of the mLbL films attributable to higher cross-link density facilitated by the stepwise deposition process in good solvents. We compare the TMC–BA series with membranes synthesized from TMC and m-phenylenediamine (MPD), a conventional reverse osmosis membrane chemistry. At the minimum thickness capable of 90% NaCl rejection, mLbL TMC–BA membranes exhibit 50% greater water permeance than mLbL TMC–MPD.
quote
| GB/T 7714-2015 | [1] William D. Mulhearn, Christopher M. Stafford. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01199. |
| MLA | [1] William D. Mulhearn, and Christopher M. Stafford. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01199. |
| APA | [1] William D. Mulhearn, & Christopher M. Stafford. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01199 |
| IEEE | [1] William D. Mulhearn and Christopher M. Stafford, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01199. keywords: {polyamide;membranes;desalination;molecular layerbylayer deposition;solutiondiffusion;permeance} |