Copolymers of Functionalized and Nonfunctionalized Polydicyclopentadiene AITranslate

University of Victoria; University of Victoria
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polydicyclopentadiene (PDCPD) is a thermoset polymer that is valued in industry for its excellent mechanical properties, heat resistance, and chemical tolerance. However, the commercial polymer lacks chemically tunable functionality. Recently, a methyl ester functionalized polydicyclopentadiene (fPDCPD) was shown to offer significantly improved tunability while maintaining the same thermal stability as the unfunctionalized parent polymer. In this report, we describe the synthesis and characterization of poly[(methyl ester functionalized dicyclopentadiene)-stat-(dicyclopentadiene)] copolymers in which the mole fraction of the functionalized, ester-containing monomer, relative to the unfunctionalized dicyclopentadiene monomer, is systematically increased. Our data reveal an ability to tune physical and mechanical properties of the copolymers (e.g., alpha transition and hardness) by changing the monomer ratio and thermal curing time. Importantly, the copolymers retain the same thermal stability as the individual homopolymers, while allowing for increased control over surface energy.

KeyWords AITranslate

polydicyclopentadiene statistical copolymers dynamic mechanical analysis Vickers hardness hydrophobicity Raman Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01196

Chinese Library Classification Number:

Citation Information:

Polydicyclopentadiene (PDCPD) is a thermoset polymer that is valued in industry for its excellent mechanical properties, heat resistance, and chemical tolerance. However, the commercial polymer lacks chemically tunable functionality. Recently, a methyl ester functionalized polydicyclopentadiene (fPDCPD) was shown to offer significantly improved tunability while maintaining the same thermal stability as the unfunctionalized parent polymer. In this report, we describe the synthesis and characterization of poly[(methyl ester functionalized dicyclopentadiene)-stat-(dicyclopentadiene)] copolymers in which the mole fraction of the functionalized, ester-containing monomer, relative to the unfunctionalized dicyclopentadiene monomer, is systematically increased. Our data reveal an ability to tune physical and mechanical properties of the copolymers (e.g., alpha transition and hardness) by changing the monomer ratio and thermal curing time. Importantly, the copolymers retain the same thermal stability as the individual homopolymers, while allowing for increased control over surface energy.

quote

GB/T 7714-2015 [1] Tong Li, Jeremy E. Wulff. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01196.
MLA [1] Tong Li, and Jeremy E. Wulff. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01196.
APA [1] Tong Li, & Jeremy E. Wulff. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01196
IEEE [1] Tong Li and Jeremy E. Wulff, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01196. keywords: {polydicyclopentadiene;statistical copolymers;dynamic mechanical analysis;Vickers hardness;hydrophobicity;Raman;Show More}