Synthesis of Fiber Tubular Nano-sized Manganese Oxide with Cotton Fiber as the Template AITranslate
Abstract AITranslate
Nano-sized manganese oxide micrometer tube was synthesized by liquid infiltration and high temperature calcination with cotton fibre as the template.The structure and morphology of the samples were investigated by SEM,XRD and FTIR.The results show that the obtained manganese oxide particles are spherical with average diameter of 300~600 nm.The aggregate of manganese oxide particles has a tubular shape with a diameter of about 10 μm and a length of about 40 μm.
KeyWords AITranslate
1邹强,李付奎,张之圣,李玲霞,王慧,薛涛,王磊,倪恒侃.高分子自组装Mn_2O_3花瓣状纳米带、纳米线的研究[J].化学学报,2009,67(17):2043-2046. 被引量:4
2黄彩娟.超声波辅助水热合成MnO_2纳米线[J].矿冶工程,2009,29(6):89-91. 被引量:3
3李良超,应桃开,周享春.纳米氧化锰的制备及其电化学性能研究[J].材料科学与工程学报,2005,23(6):836-838. 被引量:4
4刘玲,夏熙.纳米电极材料的制备及其电化学性质研究(Ⅲ)——微乳液中通氧气制备MnO_2及其性能[J].电化学,1998,4(3):328-333. 被引量:18
5李亚栋,李成韦,李龙泉,钱逸泰.γ-MnO_2纳米晶的水热合成及表征[J].高等学校化学学报,1997,18(9):1436-1437. 被引量:25
6Liu Y P,Qian Y T,Zhang Y H. γ-Ray radiation preparation and characterization of nanocrystaline manganese dioxide[J].Materials Research Bulletin,1997,(08):1055-1062.doi:10.1016/S0025-5408(97)00069-X.
7李娟,夏熙,李清文.纳米MnO_2的固相合成及其电化学性能的研究(Ⅰ)──纳米γ-MnO_2的合成及表征[J].高等学校化学学报,1999,20(9):1434-1437. 被引量:45
8张启卫,钟建生,黄行康,黄河宁,杨勇.δ-MnO_2的制备与性能[J].应用化学,2005,22(8):908-911. 被引量:9
9Yuan Changzhou,Gao Bo,Su Linghao. Interface synthesis of mesoporous MnO2 and its electrochemical capacitive behaviors[J].Journal of Colloid and Interface Science,2008.545-550.
1曾建,马年方,李昱,李锦荣,陈瑞荣,梁磊.蔗渣纤维模板法制备纤维状氧化铁[J].广西科学,2016,23(1):56-61. 被引量:1
2刘佳雯,胡钦,刘利琴,马铭婧,祝青,范春霖,来明秀,曹海兵,程正柏,丁明其,刘洪斌,安兴业.以纤维为模板剂制备纳米管状材料的研究进展[J].天津造纸,2020,42(3):1-9.
1曾建,李锦荣,梁磊,陈瑞荣,马年方.蔗渣纤维炭化特性及不同预处理方法的影响研究[J].甘蔗糖业,2017,46(1):29-36. 被引量:1
1郑广伟,杜玉成,侯瑞琴,王利平,孙广兵.硅藻土原位生长纳米氧化锰及吸附性能[J].中国粉体技术,2014,20(5):63-66.
2舒友琴,袁道强,童岩.由室温固相反应路线制备的纳米MnO_2的pH响应[J].郑州牧业工程高等专科学校学报,2000,20(2):94-96. 被引量:2
3陈爽,麦艺炽.亲油性金纳米粒子的合成[J].功能材料,2007,38(6):1019-1021.
4杨超,刘卓钦,田熙科,皮振邦,王圣平.The Composite Effect of Nanometer MnO_2 Mixed with the Electrolytic MnO_2[J].中国地质大学学报:英文版,2007,18(2):172-176.
5李良超,应桃开,周享春.纳米氧化锰的制备及其电化学性能研究[J].材料科学与工程学报,2005,23(6):836-838. 被引量:4
6杨英惠.分立纳米线提高电池的功率密度[J].现代材料动态,2005(5):9-10.
7姜宪凯,顾继友,陈萃,张彦华,白续铎,张岚.碳纳米管/聚氨酯复合材料的制备及其力学性能的研究[J].黑龙江大学自然科学学报,2009,26(6):790-794. 被引量:5
8宋静静,李勇,韩艳星,杨永珍,刘旭光,许并社.碳微球的荧光量子效应[J].太原理工大学学报,2013,44(2):194-198. 被引量:1
9姜宪凯,顾继友,陈萃,张岚,张彦华,白续铎.碳纳米管/聚氨酯复合材料制备方法的研究[J].黑龙江大学自然科学学报,2010,27(2):214-218. 被引量:7
10尤鹤翔,文晓梅,王晓东,黄培.高热稳定性聚酰亚胺抗静电复合薄膜的制备与表征[J].塑料工业,2013,41(1):120-122. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
Nano-sized manganese oxide micrometer tube was synthesized by liquid infiltration and high temperature calcination with cotton fibre as the template.The structure and morphology of the samples were investigated by SEM,XRD and FTIR.The results show that the obtained manganese oxide particles are spherical with average diameter of 300~600 nm.The aggregate of manganese oxide particles has a tubular shape with a diameter of about 10 μm and a length of about 40 μm.
quote
| GB/T 7714-2015 | [1] FENG Na, LI Feng-feng, MA Hua, et al. Synthesis of Fiber Tubular Nano-sized Manganese Oxide with Cotton Fiber as the Template[J]. Rare Metals and Cemented Carbides, 2012(2): 33-35. |
| MLA | [1] FENG Na, et al., "Synthesis of Fiber Tubular Nano-sized Manganese Oxide with Cotton Fiber as the Template." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 33-35. |
| APA | [1] FENG Na, LI Feng-feng, MA Hua, YANG Wei-chao, ZHANG Ning, & YANG Ke-xin. (2012). Synthesis of Fiber Tubular Nano-sized Manganese Oxide with Cotton Fiber as the Template. Rare Metals and Cemented Carbides(2), 33-35. |
| IEEE | [1] FENG Na, LI Feng-feng, MA Hua, YANG Wei-chao, ZHANG Ning, and YANG Ke-xin, "Synthesis of Fiber Tubular Nano-sized Manganese Oxide with Cotton Fiber as the Template," Rare Metals and Cemented Carbides, no. 2, pp. 33-35, 2012. keywords: {nano-sized manganese oxide;micrometre tube;cotton fiber;template} |