Improvement of High-temperature Oxidation Resistance of TiAl-based Alloy by Cr-Si Plasma Surface Alloying AITranslate

Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology;Nanjing University of Aeronautics and Astronautics University of Materials Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cr-Si was permeated into the surface of TiAl-based alloy by plasma surface alloying.Morphology,alloy element content and phase composition of the alloyed layer were characterized by SEM,EDS and XRD.Effects of surface alloying on high-temperature oxidation resistance of TiAl-based alloy were investigated.The results show that the alloyed layer is composed of Cr3Si and TiCr2 Laves phase.The main phases in the transition layer are Al8Cr5 and Al3Ti.Cr and Si concentration of the alloyed layer is of gradient distribution.The alloying surface layer is covered with dense CrO2 after high temperature oxidation,and the inner layer is a continuous Al2O3 barrier.The oxidation kinetics curve of the alloyed layer show a typical parabola.

KeyWords AITranslate

TiAl-based alloy plasma surface technology Cr-Si alloying high-temperature oxidation resistance

1Kim Y M. Ordered intermetallic alloys,part Ⅲ:Gamma titanium aluminides[J].J OM,1990,(07):30-39.

2刘秀波,王华明.TiAl合金激光熔覆复合材料涂层耐磨性研究[J].材料热处理学报,2006,27(1):87-91. 被引量:11

3Chan K,Kim Y W. Rate and environmental efforts on fracture of two-phase TiAl alloy[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1993.113-125.

4刘大响,程荣辉.世界航空动力技术的现状及发展动向[J].北京航空航天大学学报,2002,28(5):490-496. 被引量:90

5Brady M P,Smialek J L,Smith J. The role of Cr in promoting protective alumina scale formation by γ-based Ti-Al-Cr alloys——Ⅰ.Compatibility with alumina and oxidation behavior in oxygen[J].Acta Materialia,1997,(06):2357-2369.doi:10.1016/S1359-6454(96)00362-X.

6Zhou Chungen,Yang Ying,Gong Shengkai. Effects of Ti-Al-Cr coatings on the high temperature oxidation behavior of TiAl alloys[J].Materials Science and Engineering,2001.182-187.

7Yu T H,Koo C H. Phase characterization of a hot-rolled Ti-40Al-10Nb alloy at 1 000 ℃ to 1 200 ℃[J].Scripta Materialia,1998,(07):915-920.doi:10.1016/S1359-6462(98)00279-6.

8董利民,崔玉友,杨锐,王福会.元素Si对TiAl合金抗氧化性能的影响[J].金属学报,2004,40(4):383-387. 被引量:21

9Tang Zhaolin,Wang Fuhui,Wu Weitao. Effects of MCrA1Y overlay coatings on oxidation resistance of TiAl intermetallics[J].Surface and Coatings Technology,1998.248-252.

10张轲,孙超,王福会.扩散铝涂层的制备及其对γ-TiAl基体的防护[J].金属学报,2006,42(4):355-360. 被引量:10

1于修水,梁文萍,缪强,徐一,任蓓蕾,王玲.γ-TiAl合金磁控溅射Al涂层的抗高温氧化性能[J].金属热处理,2013,38(8):21-25. 被引量:8

2党薇,李宏林,董贵荣,史卫朝.TiAl合金高温抗氧化表面防护技术[J].表面工程与再制造,2019,19(4):34-38. 被引量:2

3赖旭平,李天方,刘瑞,孙红亮.不同电介质对制备TiAl合金粉末的影响[J].稀有金属与硬质合金,2021,49(5):35-40.

1王力,梁文萍,缪强,任蓓蕾,潘晓扬.Ti_2AlNb合金不同温度下的高温氧化行为[J].金属热处理,2015,40(3):52-57. 被引量:6

2裴秋旭,梁文萍,缪强,任蓓蕾,王昉,贲能军.TA15合金在不同温度下的氧化行为[J].热处理,2015,30(4):13-17. 被引量:2

3王凯亮,孙勇,郭中正,段永华,孙国琪.磁控共溅射沉积Al-Al_2O_3复合膜的结构与性能[J].金属热处理,2016,41(1):184-189. 被引量:1

4孟德松,付广艳,李雨莎.Al-Si共渗涂层对1Cr18Ni9Ti不锈钢氧化行为的影响[J].沈阳化工大学学报,2015,29(4):347-352. 被引量:1

5付广艳,王子龙,刘群,张小玲,祁泽艳.溅射AlY涂层对Ni基合金抗热腐蚀性能的影响[J].稀土,2017,38(4):88-94.

6石皋莲,吴少华,任佳.Al(Ni)含量对钛合金激光熔覆AlNiMoSi复合涂层摩擦学性能的影响[J].材料保护,2018,51(3):7-10. 被引量:3

7李艳明,李中生,刘欢,卜嘉利,张开阔,韩振宇.镍基高温合金表面Co-Al涂层抗高温氧化性能研究[J].航空发动机,2023,49(1):169-174.

8黄宏军,徐志鹏,袁晓光,林雪健,郑博文.TiAl合金电弧喷涂Al涂层的高温氧化性能[J].沈阳工业大学学报,2023,45(3):270-277.

9章凯,辛丽,程玉贤,彭新,王博.AlCr(Si)N和CrAl(Si)N涂层对TiAl合金900℃循环氧化性能的影响[J].中国表面工程,2023,36(4):185-195.

1李亚非,张平则,许浩.等离子表面Cr-Si合金化改善TiAl基合金高温性能的研究[J].航空材料学报,2011,31(6):43-49. 被引量:1

2魏祥飞,张平则,魏东博,沙李丽,周鹏,张扬.γ-TiAl合金表面双层辉光等离子铬钨共渗层的高温氧化行为[J].机械工程材料,2014,38(5):12-16. 被引量:2

3董璞,胡淑娟,屈红星,宜楠,韩吉庆.热处理工艺对超导阻隔层用铌板力学性能的影响[J].热加工工艺,2016,45(22):163-164.

4刘卫国,刘建东,赵陈龙.水的磁处理防腐蚀机理研究[J].腐蚀与防护,2006,27(4):196-198. 被引量:8

5李咏梅,张敏,范爱兰.Ti6Al4V合金表面钼-氮渗镀复合层的制备及性能[J].机械工程材料,2011,35(10):1-3.

6王振霞,陈丽红,单小林,贺志勇,刘小萍.TC4表面等离子Ni改性层摩擦磨损研究[J].表面技术,2015,44(1):92-95. 被引量:5

7葛继平,陈美玲,陈玉喜,王学芝.热处理对CrO2低铬铸铁组织和性能的影响[J].金属热处理,1997(7):15-17. 被引量:2

8专利信息(Ⅲ)[J].稀有金属快报,2007,26(12):33-33.

9何玉定,曲选辉,黄伯云.合金元素对Laves相TiCr_2力学性能的影响[J].中国有色金属学报,1998,8(4):568-572. 被引量:9

10何玉定,曲选辉,黄伯云,刘志坚.Laves相TiCr_2的相变特征[J].中国有色金属学报,1998,8(A01):115-118. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG174.445[金属学及工艺—金属表面处理]

Citation Information:

Cr-Si was permeated into the surface of TiAl-based alloy by plasma surface alloying.Morphology,alloy element content and phase composition of the alloyed layer were characterized by SEM,EDS and XRD.Effects of surface alloying on high-temperature oxidation resistance of TiAl-based alloy were investigated.The results show that the alloyed layer is composed of Cr3Si and TiCr2 Laves phase.The main phases in the transition layer are Al8Cr5 and Al3Ti.Cr and Si concentration of the alloyed layer is of gradient distribution.The alloying surface layer is covered with dense CrO2 after high temperature oxidation,and the inner layer is a continuous Al2O3 barrier.The oxidation kinetics curve of the alloyed layer show a typical parabola.

quote

GB/T 7714-2015 [1] LI Ya-fei, ZHANG Ping-ze, XU Hao. Improvement of High-temperature Oxidation Resistance of TiAl-based Alloy by Cr-Si Plasma Surface Alloying[J]. Rare Metals and Cemented Carbides, 2012(2): 36-40.
MLA [1] LI Ya-fei, et al., "Improvement of High-temperature Oxidation Resistance of TiAl-based Alloy by Cr-Si Plasma Surface Alloying." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 36-40.
APA [1] LI Ya-fei, ZHANG Ping-ze, & XU Hao. (2012). Improvement of High-temperature Oxidation Resistance of TiAl-based Alloy by Cr-Si Plasma Surface Alloying. Rare Metals and Cemented Carbides(2), 36-40.
IEEE [1] LI Ya-fei, ZHANG Ping-ze, and XU Hao, "Improvement of High-temperature Oxidation Resistance of TiAl-based Alloy by Cr-Si Plasma Surface Alloying," Rare Metals and Cemented Carbides, no. 2, pp. 36-40, 2012. keywords: {TiAl-based alloy;plasma surface technology;Cr-Si alloying;high-temperature oxidation resistance}