daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Investigation of Interfacial Structure and Doping Effect of Ti(C,N)-based Cermet AITranslate

National Key Laboratory of Mold and Materials, Huazhong University of Science and Technology;National Key Laboratory of Mold and Materials, Huazhong University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the theory and method of interfacial study between metal and ceramic,focusing on the interfacial structure?doping effect and active mechanism of various doping elements of Ti(C,N)-based cermet.Process for interfacial design and surface alloying is reported.

KeyWords AITranslate

metal/ceramic interface interface doping effect surface alloying

1李世普.特种陶瓷工艺学[M].武汉工业大学出版社,1993.5.

2张国军.Ti(C、N)基金属陶瓷[J].机械工程材料,1990,14(3):4-9. 被引量:17

3刘韩星,袁润章.金属-陶瓷界面结构的研究[J].化学通报,1994(6):20-28. 被引量:5

4刘韩星,张汉林,欧阳世翕,袁润章.Cu_n、Ag_n、Au_n(n=2,3,4)原子簇结构的理论分析[J].高等学校化学学报,1995,16(2):260-264. 被引量:1

5任海兰,刘韩星,欧阳世翕.Ti/Al_2O_3和Ni/Al_2O_3界面电子结构的量子化学研究[J].硅酸盐学报,1997,25(6):697-704. 被引量:3

6崔万秋,雷鸣.TiC、TiC_(1-x)、(Ti_(1-x)Nb_x)C电子结构的计算[J].物理化学学报,1998,14(3):198-203. 被引量:2

7闵新民,邓志平,李嘉宇,袁润章.碳化钛与氮化钛类陶瓷材料结构、性能与量子化学计算研究[J].计算物理,1997,14(1):1-5. 被引量:5

8Schoenberger U, et al. Bonding at metal - cermnic interfaces, abinitio density - functioaal calculations for Ti and Ag on MgO[J] .Acta Metall Mater, 1992, 40(suppl) : 1.

9Duffy D M, et al. Atomistic modeling of the metal/oxide interface with image interactions [ J ] . Acta Metall Mater, 1992, 40(suppl) : 11.

10Kom D, et al. Influence of interface impurities on the fracture energy of UHF bonded Niobium - Sapphire bictytals[ J ] .Acta Metall Mater, 1992, 40(suppl) :355.

1陈慧,邓莹,李力.Ti(C,N)基金属陶瓷刀具材料的研究现状[J].重庆文理学院学报:自然科学版,2012,31(5):13-16. 被引量:3

1叶小舟.低温制备碳化物的研究进展[J].重庆文理学院学报:社会科学版,2015,34(2):22-28. 被引量:1

2李慧群,韦霄腾.气动端面行星运动式金刚石磨具的制作[J].重庆文理学院学报:社会科学版,2016,35(5):5-7.

3李强,李文戈,赵远涛,王争强,袁东林,张淼.Mo2NiB2基金属陶瓷制备技术及应用的研究进展[J].机械工程材料,2020,44(10):12-16. 被引量:2

1李万明,姜周华,董艳伍,刘辉,郑立春.复合轧辊界面理论研究的现状[J].材料与冶金学报,2011,10(B03):77-80. 被引量:6

2古今.铸件表面合金化技术研究状况[J].四川冶金,2005,27(1):8-10.

3戴星,金山同.石墨电极表面的抗氧化合金保护层[J].应用基础与工程科学学报,1994,2(1):28-34. 被引量:1

4戴星,包燕平,金山同.浸渗─表面合金化技术在石墨电极表面的应用[J].北京科技大学学报,1994,16(3):240-244.

5于贵波,赵忠民,王建江,张龙.镍对重力分离SHS陶瓷内衬复合管的影响[J].军械工程学院学报,2002,14(1):1-6. 被引量:4

6陈大明,张晨,孟国文,韩栋,曾燮榕,康沫狂.粒径与掺杂对ZrO_2纳米粉相结构的影响[J].材料研究学报,1995,9(3):259-262. 被引量:5

7顾正飞,刘正义,罗承萍,曾德长.烧结Nd-Fe-B稀土永磁合金的界面结构与矫顽力[J].电工合金,1999(3):7-17. 被引量:1

8张景林.蓝钨生产技术进展[J].中国钨业,1993,0(5):17-20. 被引量:2

9刘英伟,谈春明,邬海峰.一种X射线冷轧测厚仪的控制系统[J].核电子学与探测技术,2010,30(1):23-26. 被引量:2

10许承惠,吴润,田薇.Fe基-Al_2O_3复合材料的界面研究[J].武汉冶金科技大学学报,1996,19(3):307-311. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF125.41[冶金工程—粉末冶金]

Citation Information:

Description is made of the theory and method of interfacial study between metal and ceramic,focusing on the interfacial structure?doping effect and active mechanism of various doping elements of Ti(C,N)-based cermet.Process for interfacial design and surface alloying is reported.

quote

GB/T 7714-2015 [1] ZHOU Shi-quan, XIONG Wei-hao. Investigation of Interfacial Structure and Doping Effect of Ti(C,N)-based Cermet[J]. Rare Metals and Cemented Carbides, 2003(3): 9-11.
MLA [1] ZHOU Shi-quan, and XIONG Wei-hao. "Investigation of Interfacial Structure and Doping Effect of Ti(C,N)-based Cermet." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 9-11.
APA [1] ZHOU Shi-quan, & XIONG Wei-hao. (2003). Investigation of Interfacial Structure and Doping Effect of Ti(C,N)-based Cermet. Rare Metals and Cemented Carbides(3), 9-11.
IEEE [1] ZHOU Shi-quan and XIONG Wei-hao, "Investigation of Interfacial Structure and Doping Effect of Ti(C,N)-based Cermet," Rare Metals and Cemented Carbides, no. 3, pp. 9-11, 2003. keywords: {metal/ceramic interface;interface doping effect;surface alloying}