daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of New Wearable Alloy Powder Block from Nano-structured WO_3+C Composite Powder AITranslate

Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy;Department of Materials Science and Engineering, Dalian Railway Academy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A new type wearing-resistant alloy powder block was made from nano-structured WO3+C composite powder. Processing performance test is made for the analysis of surfacing layer structure,composition and hardness,etc.The results showed that the powder block has good welding processing performance,high deposition efficiency with tiny structure in the surfacing layer mainly containing W-enriched carbides of (Fe6W6C), acicular martensite and austenite.The hardness of the surfacing layer was over HRC60,max.HRC63.Compared to the micron powder,nano-powder block is characterized by higher W content in matrix,tiny structure,higher hardness,suitable for wearable surfacing.

KeyWords AITranslate

WO3+C nano-structured powder alloy powder block surfacing

1周玉生,于凤福,贺文雄.碳极氩气拘束电弧碳化钨颗粒复合材料堆焊工艺研究[J].机械工程学报,2002,38(8):151-155. 被引量:2

2张长敏.纳米材料在焊接技术中的应用[J].焊接技术,2001,30(1):12-13. 被引量:11

3李希甫,赵璞,张升波,张志发.利用Fe—5耐磨合金粉块堆焊引风机叶轮技术的应用[J].中国甜菜糖业,1997(1):44-44. 被引量:3

4化茂林,郁翔.碳弧堆焊防磨技术在排粉机上的应用[J].西北电力技术,1998(4):31-33. 被引量:2

5李东,陈怀宁,刘刚,卢柯,林泉洪.SS400钢对接接头表面纳米化及其对疲劳强度的影响[J].焊接学报,2002,23(2):18-21. 被引量:44

6任瑞铭 等.机械与热激活合成纳米结构WC/Co复合粉体[J].材料科学与工艺,2001,9:346-346.

7陈春焕,赵秀娟,史春元,杨德新,董雪,马光.用WO_3+C纳米粉末制备新型堆焊焊条[J].大连铁道学院学报,2003,24(1):52-56. 被引量:4

1姚上卫.纳米技术在焊接领域的应用[J].焊接学报,2007,28(3):109-112. 被引量:6

2乔雷,孙海燕.焊接技术中的创新发明[J].山西冶金,2017,40(6):62-64.

1顾玲燕,徐越兰,张霞,汤志宁.颗粒度对E4303电焊条性能影响[J].焊接学报,2008,29(10):50-52.

2王爱华,李建国,姚青虎,杨科伟.纳米稀土氧化物对铁粉焊条焊缝低温冲击韧度的影响[J].热加工工艺,2008,37(21):21-22. 被引量:4

3刘晶晶.纳米技术及其发展浅析[J].科技与生活,2012(14):219-219. 被引量:1

4何鹏,矫震,王君,林铁松.纳米尺度连接技术的研究现状与展望[J].焊接学报,2013,34(2):109-112. 被引量:5

5栗卓新,曹晓涛,Wolfgang TILLMANN.纳米材料在无镀铜焊丝中的研究现状[J].北京工业大学学报,2017,43(10):1582-1589. 被引量:7

6张文毓.纳米技术在焊接领域的应用进展[J].现代焊接,2016,0(10):1-5.

1张玉柱,李东春,燕山大学,邢宏伟,郎建峰.硼镁复合添加剂对烧结矿玻璃相形成的影响[J].烧结球团,2001,26(5):9-11. 被引量:5

2彭天祥,孙敏.耐磨堆焊合金粉末的研究进展及应用[J].黑龙江科技信息,2009(19):26-26. 被引量:3

3杨希,夏立明,何小琴.一种含铌耐磨堆焊药芯焊丝的开发[J].中国冶金,2016,26(12):54-56.

4由升远.回转窑炉筒焊接工艺性探讨[J].中国钼业,2007,31(6):27-28.

5赵春燕,李家宇,高兆先,王善元.连铸辊堆焊用药芯焊带的研究[J].焊接,1997(11):5-8. 被引量:2

6霍.,布D,林燕耆.连铸机辊子的设计,作用和性能[J].大重科技,1997(1):41-47.

7郭林,霍向东,李烈军,黎剑锋,董锋,田振卓.冷却速度对X80管线钢焊接热影响区组织性能的影响[J].钢铁钒钛,2013,34(6):96-100. 被引量:5

8孙东升,王恒.电渣重熔超超临界叶片钢KT5931ASO的质量缺陷与改进[J].金属世界,2009(3):49-53.

9刘士伟.烧结矿中三元铁酸钙固结相形成的探讨[J].烧结球团,1996,21(4):13-17. 被引量:1

10应用离子选择电极控制硫化铜矿生物浸出液萃取过程中第三相形成的工艺[J].有色冶金节能,2011(6):56-56.

Basic Information:

DOI:

Chinese Library Classification Number:TF122.1[冶金工程—粉末冶金]

Citation Information:

A new type wearing-resistant alloy powder block was made from nano-structured WO3+C composite powder. Processing performance test is made for the analysis of surfacing layer structure,composition and hardness,etc.The results showed that the powder block has good welding processing performance,high deposition efficiency with tiny structure in the surfacing layer mainly containing W-enriched carbides of (Fe6W6C), acicular martensite and austenite.The hardness of the surfacing layer was over HRC60,max.HRC63.Compared to the micron powder,nano-powder block is characterized by higher W content in matrix,tiny structure,higher hardness,suitable for wearable surfacing.

quote

GB/T 7714-2015 [1] CHEN Chun-huan, ZHAO Xiu-juan, YANG De-xin. Preparation of New Wearable Alloy Powder Block from Nano-structured WO_3+C Composite Powder[J]. Rare Metals and Cemented Carbides, 2003(3): 5-8.
MLA [1] CHEN Chun-huan, et al., "Preparation of New Wearable Alloy Powder Block from Nano-structured WO_3+C Composite Powder." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 5-8.
APA [1] CHEN Chun-huan, ZHAO Xiu-juan, & YANG De-xin. (2003). Preparation of New Wearable Alloy Powder Block from Nano-structured WO_3+C Composite Powder. Rare Metals and Cemented Carbides(3), 5-8.
IEEE [1] CHEN Chun-huan, ZHAO Xiu-juan, and YANG De-xin, "Preparation of New Wearable Alloy Powder Block from Nano-structured WO_3+C Composite Powder," Rare Metals and Cemented Carbides, no. 3, pp. 5-8, 2003. keywords: {WO3+C;nano-structured powder;alloy powder block;surfacing}