Abstract AITranslate

High-concentration Cr-contaminated wastewater can cause serious environmental and public health problems. Therefore, this study proposed a method that uses ascorbic acid, a cationic copolymer gel-supported reducing agent, to remove hexavalent chromium, Cr(VI), from wastewater. This gel adsorbed Cr(VI) via an ion exchange process that uses N-[3-(dimethylamino) propyl] acrylamide methyl chloride quaternary monomer (DMAPAAQ) (DQ) and trivalent chromium, Cr(III), reduced by l-ascorbic acid (VC) via chelation and insoluble hydroxide formation induced by N,N-dimethylamino propylacrylamide monomer (DMAPAA) (DA). Furthermore, the effects of solution pH, initial Cr(VI) concentration, co-existing anions, contact time, and temperature on the reduction and removal processes facilitated by the DA/DQ and DA/DQ/VC gels were investigated. Both gels maintained a high adsorption efficiency at pH 3–6; however, the DA/DQ gel had a lower efficiency than the DA/DQ/VC gel in acidic, neutral, and weak alkaline environments. Adsorption isotherms suggested that both gels had a structurally homogeneous surface. Kinetics indicated that Cr(VI) adsorption by both gels was dominated by different sorption at low- or high-concentrations of Cr-contaminated wastewater. Thermodynamic parameters calculated using equations and plotting results indicated that the adsorption by both gels was an endothermic, irreversible, and spontaneous process.

KeyWords AITranslate

hydrogel reductant chromium removal pH kinetics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02105

Chinese Library Classification Number:

Citation Information:

High-concentration Cr-contaminated wastewater can cause serious environmental and public health problems. Therefore, this study proposed a method that uses ascorbic acid, a cationic copolymer gel-supported reducing agent, to remove hexavalent chromium, Cr(VI), from wastewater. This gel adsorbed Cr(VI) via an ion exchange process that uses N-[3-(dimethylamino) propyl] acrylamide methyl chloride quaternary monomer (DMAPAAQ) (DQ) and trivalent chromium, Cr(III), reduced by l-ascorbic acid (VC) via chelation and insoluble hydroxide formation induced by N,N-dimethylamino propylacrylamide monomer (DMAPAA) (DA). Furthermore, the effects of solution pH, initial Cr(VI) concentration, co-existing anions, contact time, and temperature on the reduction and removal processes facilitated by the DA/DQ and DA/DQ/VC gels were investigated. Both gels maintained a high adsorption efficiency at pH 3–6; however, the DA/DQ gel had a lower efficiency than the DA/DQ/VC gel in acidic, neutral, and weak alkaline environments. Adsorption isotherms suggested that both gels had a structurally homogeneous surface. Kinetics indicated that Cr(VI) adsorption by both gels was dominated by different sorption at low- or high-concentrations of Cr-contaminated wastewater. Thermodynamic parameters calculated using equations and plotting results indicated that the adsorption by both gels was an endothermic, irreversible, and spontaneous process.

quote

GB/T 7714-2015 [1] Yu Song, Takehiko Gotoh, Satoshi Nakai. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02105.
MLA [1] Yu Song, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02105.