Perylene Diimide-Containing Dynamic Hyper-crosslinked Ionic Porous Organic Polymers: Modulation of Assembly and Gas Storage AITranslate

Indian Institute of Technology Hyderabad; Indian Institute of Technology Hyderabad; Indian Institute of Technology Kharagpur; Indian Institute of Technology Hyderabad; Indian Institute of Technology Kharagpur; Indian Institute of Technology Hyderabad; Indian Institute of Technology Hyderabad
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A strategy to synthesize hyper-crosslinked polymers with strong visible-light absorption and abundant ionic sites is discussed. This is achieved in a one-pot reaction via the simultaneous Friedel–Crafts alkylation and quaternization reaction between α,α′-dibromo-p-xylene (DBX) and perylene diimide (PDI) substituted with N,N-dimethyl ethylene to result in hyper-crosslinked ionic polymers (HIPs). These HIPs display good surface areas with strong visible-light absorption (400–650 nm) and dispersibility in polar solvents like water and DMSO. Importantly, our experimental and theoretical studies indicate that PDI-HIPs possess a dynamic network with good uptake of water up to seven times their weight. Notably, PDI in PDI-HIPs is not only responsible for visible-light absorption but also acts as a probe to study their dynamic nature. Moreover, the presence of ultramicropores and CO2-philic functional groups in PDI-HIPs renders good CO2 uptake up to 2.11 mmol/g at 273 K despite their relatively low surface area.

KeyWords AITranslate

hypercrosslinked polymers dynamic behavior porous materials perylene diimides gas storage
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02102

Chinese Library Classification Number:

Citation Information:

A strategy to synthesize hyper-crosslinked polymers with strong visible-light absorption and abundant ionic sites is discussed. This is achieved in a one-pot reaction via the simultaneous Friedel–Crafts alkylation and quaternization reaction between α,α′-dibromo-p-xylene (DBX) and perylene diimide (PDI) substituted with N,N-dimethyl ethylene to result in hyper-crosslinked ionic polymers (HIPs). These HIPs display good surface areas with strong visible-light absorption (400–650 nm) and dispersibility in polar solvents like water and DMSO. Importantly, our experimental and theoretical studies indicate that PDI-HIPs possess a dynamic network with good uptake of water up to seven times their weight. Notably, PDI in PDI-HIPs is not only responsible for visible-light absorption but also acts as a probe to study their dynamic nature. Moreover, the presence of ultramicropores and CO2-philic functional groups in PDI-HIPs renders good CO2 uptake up to 2.11 mmol/g at 273 K despite their relatively low surface area.

quote

GB/T 7714-2015 [1] Soujanya H. Goudar, Dhiraj S. Ingle, Rahul Sahu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02102.
MLA [1] Soujanya H. Goudar, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02102.
APA [1] Soujanya H. Goudar, Dhiraj S. Ingle, Rahul Sahu, Srinu Kotha, Sandeep K. Reddy, Deepu J. Babu, & Venkata Rao Kotagiri. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02102
IEEE [1] Soujanya H. Goudar, Dhiraj S. Ingle, Rahul Sahu, Srinu Kotha, Sandeep K. Reddy, Deepu J. Babu, and Venkata Rao Kotagiri, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02102. keywords: {hypercrosslinked polymers;dynamic behavior;porous materials;perylene diimides;gas storage}