Determination of Trace Hydrogen in High-purity Titanium Metal AITranslate
Abstract AITranslate
The mass fraction of the hydrogen in high-purity titanium metal was determined by high frequency induction-thermal conductivity method. The influences of induction current, crucible material, fluxing agent,blank value,minimum analysis time and sample weight on the determined result were emphatically discussed. And a method to determine the hydrogen in high-purity titanium metal was established. The results show that the relative standard deviation of the hydrogen mass fraction determined by the above method is 6. 3%, and the recovery of standard addition is 98%-106%. The determination conditions of partial hydrogen content in titanium metal were studied by a combined analysis program. Based on peak separation experiments, each partial hydrogen content was calculated.
KeyWords AITranslate
1张之翔.金属材料中微量氢和氧的分析[J].稀有金属材料与工程,1997,26(1):56-61. 被引量:5
2Joseph J Kreuser, Thomas W Junker, Richard A Fork. Simultaneous measurement of hydrogen, notrogen and oxygen in molten steel[J]. AISTech Proceedings, 2004, 24 ( 1 ): 821-829.
3李婷,刘颂禹.金属中气体分析进展[J].冶金分析,1999,19(6):35-40. 被引量:11
4王蓬,王海舟.金属中氢的分析技术进展[J].冶金分析,2007,27(3):37-44. 被引量:19
1魏欣,董俊华,柯伟.高放射性核废料地质处置环境中钛处置罐腐蚀研究的进展[J].腐蚀科学与防护技术,2013,25(2):160-164. 被引量:5
2王虹.惰性气体中熔样-热导法测定锆中氢的含量[J].理化检验:化学分册,2014,50(6):781-783. 被引量:3
1薛芳,魏欣,董俊华,柯伟.高放废物深地质处置环境中低碳钢腐蚀行为的研究进展[J].腐蚀科学与防护技术,2015,27(5):497-502. 被引量:7
2赵飞,李娟.惰气熔融-红外法测定铪中氢含量[J].有色金属科学与工程,2017,8(6):117-120. 被引量:1
3陆科呈,杨鸿驰,刘俊生,兰标景.热导法测定航空用铝合金中氢含量[J].化学分析计量,2018,27(3):44-47.
4杨瑞杰,蒋永光,石良.微生物与核废料的长期管理[J].地球科学,2018,43(A01):127-135.
5刘灿帅,田朝晖,张志明,王俭秋,韩恩厚.地质处置后期无氧阶段X65低碳钢腐蚀行为研究[J].腐蚀科学与防护技术,2019,31(4):371-378.
6李凤侠,张俊,赵呈刚.基于文献计量学的氢脆研究的演进、热点和趋势分析[J].材料导报,2019,33(S02):488-496. 被引量:4
7张琦超,黄彦良,许勇,杨丹,路东柱.高放射性核废料钛储罐深地质环境中氢吸收及氢脆研究进展[J].中国腐蚀与防护学报,2020,40(6):485-494. 被引量:1
8刘攀,杜丽丽,唐伟,李治亚.无机固态材料中气体元素分析的现状与进展[J].理化检验:化学分册,2015,51(1):131-136. 被引量:9
1卞敏,纪新华,李英秋,武红英.V-5Cr-5Ti合金中杂质元素氧、氮、氢的测定[J].核化学与放射化学,2016,38(4):219-224.
2何丽君,霍彩霞,李生英,姚小军,杨彩玲,徐飞.柚皮苷与人血清白蛋白相互作用的研究[J].化学研究与应用,2014,26(8):1195-1199. 被引量:4
3马浚,唐元明,张勤英,龚有进.固相微萃取-气相色谱联用技术分析混合气体中微量氢[J].分析测试技术与仪器,2007,13(3):182-186. 被引量:1
4周海收,温美娟,辛仁轩.低温堆水样中微量氢的测定[J].分析试验室,1995,14(6):56-59. 被引量:2
5姜镭,辛仁轩.反应堆冷却水中微量氢的顶空气相色谱测定[J].分析试验室,1997,16(3):48-50. 被引量:1
6陈美春,朱杰丽.氢化物原子荧光光谱法测定土壤中的汞的不确定度评定[J].分析试验室,2008,27(B12):432-435. 被引量:3
7汪涛.化学实验计算的新要求[J].中学理科:高中内容,2002(7):35-36.
8张洁,陈俞霖,朱永,骆飞.Photo-induced currents in CNT films/Al large area multiwalled Structure[J].中国光学快报:英文版,2014,0(A01):15-18.
9陈平,任兴碧,肖成建,曹大伟,冉光明,刘云怒,夏修龙,陈晓军,王和义.氧化锆检测器在微量氢同位素色谱分析中的应用研究[J].原子能科学技术,2017,51(4):603-608. 被引量:2
10孟庆强,金之钧,刘文汇,陶成,把立强,杨华敏.MAT253气体同位素质谱仪测定微量氢同位素组成进样方法初探[J].岩矿测试,2010,29(6):639-642. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:O659.33[理学—分析化学]
Citation Information:
The mass fraction of the hydrogen in high-purity titanium metal was determined by high frequency induction-thermal conductivity method. The influences of induction current, crucible material, fluxing agent,blank value,minimum analysis time and sample weight on the determined result were emphatically discussed. And a method to determine the hydrogen in high-purity titanium metal was established. The results show that the relative standard deviation of the hydrogen mass fraction determined by the above method is 6. 3%, and the recovery of standard addition is 98%-106%. The determination conditions of partial hydrogen content in titanium metal were studied by a combined analysis program. Based on peak separation experiments, each partial hydrogen content was calculated.
quote
| GB/T 7714-2015 | [1] BIAN Min, LI Ying-qiu, LIU Jun, et al. Determination of Trace Hydrogen in High-purity Titanium Metal[J]. Rare Metals and Cemented Carbides, 2009(4): 36-40. |
| MLA | [1] BIAN Min, et al., "Determination of Trace Hydrogen in High-purity Titanium Metal." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 36-40. |
| APA | [1] BIAN Min, LI Ying-qiu, LIU Jun, & DUAN Li-mei. (2009). Determination of Trace Hydrogen in High-purity Titanium Metal. Rare Metals and Cemented Carbides(4), 36-40. |
| IEEE | [1] BIAN Min, LI Ying-qiu, LIU Jun, and DUAN Li-mei, "Determination of Trace Hydrogen in High-purity Titanium Metal," Rare Metals and Cemented Carbides, no. 4, pp. 36-40, 2009. keywords: {high-purity titanium metal;trace hydrogen;partial hydrogen content;high frequencyinductionthermal conductivity method} |