Silver Recovery from the Supernatant Produced during Copper Anode Slime Pretreatment AITranslate

Jiangxi Tongye Group Corporation Guixi Metallurgical Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The silver in the supernatant,produced from copper anode slime pretreatment is recovered by silver precipitation with NaI-transformation with Na2 S and then HNO3. And the optimal process conditions are determined. The results show that the silver recovery canreach 96.56% ,the silver content in the precipitated Ag solution is reduced down to 4 mg/L and the purity of crude silver is above 95%.

KeyWords AITranslate

silver recovery copper anode slime supernatant NaI Na2S

1CanahanTG FlynnCM.用碘化物沉淀法从氯化物浸出液中回收银.黄金,1981,(4):20-23.

1吕高平.铜阳极泥湿法处理工艺的改进与优化[J].有色冶炼,2003,32(4):28-30. 被引量:6

2吴月强,黄宇光.锰银精矿及粗银粉中银的容量法快速测定[J].岩矿测试,2004,23(4):315-316. 被引量:5

3赵孝文,吴珂,范庆丽.一种提高NaI能谱仪高能区射线解谱能力的装置[J].科技创新与应用,2015,5(11):66-66.

4莫晓虎,张建勇,张天保,张清江,Achasov Mikhail,傅成栋,Muchnoi Nikolay,秦庆,屈化民,王贻芳,吴靖民,徐金强,俞伯祥.Measurement of radiation dose at the north interaction point of BEPC Ⅱ[J].中国物理C:英文版,2009(10):914-921.

5莫劳.盐:人类不可缺少的矿物质[J].中国食品,2009(19):18-19.

6GONG ChunHui,ZENG GuoQiang,GE LiangQuan,TANG Xiaobin,TAN ChengJun.Minimum detectable activity for NaI(Tl) airborne γ-ray spectrometry based on Monte Carlo simulation[J].中国科学:技术科学英文版,2014,0(9):1840-1845. 被引量:3

7朱耀明,林明贵.宁德核电厂外围环境γ辐射连续监测系统[J].海峡科学,2015,0(6):75-78. 被引量:13

8苏健,马豪,苏耿华,曾志,程建平,李君利,朱立.我国沿海核电站海洋放射性就地伽玛能谱测量研究[J].辐射防护,2013,33(6):329-333. 被引量:7

9张丽.白银回收技术[J].企业科技与发展,1995,0(7):15-15.

10李文杰,鲁学军,陈振飞.样品衰变时间对陶瓷放射性测定的影响及修正[J].环境科学与技术,2015,38(6):99-105.

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

The silver in the supernatant,produced from copper anode slime pretreatment is recovered by silver precipitation with NaI-transformation with Na2 S and then HNO3. And the optimal process conditions are determined. The results show that the silver recovery canreach 96.56% ,the silver content in the precipitated Ag solution is reduced down to 4 mg/L and the purity of crude silver is above 95%.

quote

GB/T 7714-2015 [1] ZHANG Ling-ling. Silver Recovery from the Supernatant Produced during Copper Anode Slime Pretreatment[J]. Rare Metals and Cemented Carbides, 2009(4): 32-35.
MLA [1] ZHANG Ling-ling. "Silver Recovery from the Supernatant Produced during Copper Anode Slime Pretreatment." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 32-35.
APA [1] ZHANG Ling-ling. (2009). Silver Recovery from the Supernatant Produced during Copper Anode Slime Pretreatment. Rare Metals and Cemented Carbides(4), 32-35.
IEEE [1] ZHANG Ling-ling, "Silver Recovery from the Supernatant Produced during Copper Anode Slime Pretreatment," Rare Metals and Cemented Carbides, no. 4, pp. 32-35, 2009. keywords: {silver;recovery;copper anode slime;supernatant;NaI;Na2S}