Effect of Sintering Temperature on Microstructure and Properties of NdFeB Magnet AITranslate
Abstract AITranslate
NdFeB permanent magnet was prepared by rapid solidification strip casting and hydrogenation crushing,and its microstructure and properties were characterized by optical microscopy,scanning electron microscopy and AMT—4magnetic property tester.Investigation was made of the effect of sintering temperature on the microstructure and properties of the magnet.The results show that with sintering temperature increasing,the density of the sintered magnet increases,and its remanence,coercivity and maximum magnetic energy product increase at first and then decrease.The reason is that the major crystalline phase grains grow up and the neodymium-rich phase distribution is more homogeneous with sintering temperature increasing.However,when the sintering temperature reaches a certain value,the magnet microstructure is inhomogeneous and the neodymium-rich phase agglomerates.
KeyWords AITranslate
1贾成厂,孙爱芝.烧结钕铁硼永磁材料[J].金属世界,2013(3):9-14. 被引量:15
2刘小鱼,刘国征,赵明静,鲁富强,武斌.双合金工艺制备钕铁硼永磁体的性能和显微组织的研究[J].金属功能材料,2010,17(6):5-7. 被引量:5
3于濂清,袁永锋.制备工艺对NaFeB磁体力学性能的影响[J].稀有金属快报,2008,27(6):17-20. 被引量:2
4伍尚南,肖方明,黄莉丽.工艺技术对钕铁硼磁体性能影响的研究[J].材料研究与应用,2007,1(3):199-202. 被引量:4
5徐玉磊,刘树峰.使用有机添加剂改进烧结钕铁硼磁体生产工艺[J].内蒙古石油化工,2006,32(5):11-12. 被引量:4
6高汝伟,王标,刘汉强,韩广兵,白岗,孙艳,刘涛.粉末流动性和添加润滑剂对烧结钕铁硼磁体取向度和磁性能的影响[J].自然科学进展,2006,16(4):495-498. 被引量:6
7唐杰,刘颖,张然,杨刚,高升吉,涂铭旌.烧结钕铁硼永磁体矫顽力理论及其影响[J].材料导报,2006,20(4):61-63. 被引量:17
8高汝伟,王标,刘汉强,韩广兵,白岗,孙艳,刘涛.高性能烧结钕铁硼磁体的研究与开发(二)[J].磁性材料及器件,2005,36(1):1-5. 被引量:13
9唐杰,刘颖,高升吉,涂铭旌.烧结钕铁硼粉末粒度对磁性能的影响[J].金属功能材料,2004,11(6):5-8. 被引量:14
10王标,高汝伟,陈蓓新,刘汉强.添加润滑剂对烧结钕铁硼磁体性能的影响[J].材料研究学报,2004,18(6):577-581. 被引量:8
1汪东红.一种磁学特性优良的磁性材料[J].中外技术情报,1996(12):20-20.
2徐玉磊,刘树峰.使用有机添加剂改进烧结钕铁硼磁体生产工艺[J].内蒙古石油化工,2006,32(5):11-12. 被引量:4
3郭峰,高建祥,卓海宇.磁性多层膜的研究进展[J].材料导报:网络版,2006(4):4-7.
4马诺,王新林,李波,赵韦人,林德.钕铁硼母合金速凝薄带的微观结构[J].金属功能材料,2001,8(6):36-38. 被引量:10
5李建,周义,程星华,喻晓军.烧结钕铁硼镀镍防腐性能比较[J].稀土,2011,32(3):19-23. 被引量:13
6王帅,刘湘涟,秦林,杨瑞.烧结工艺对Nd-Fe-B磁体结构、磁性能与温度稳定性的影响[J].磁性材料及器件,2012,43(4):25-30. 被引量:4
7李营,肖勇,王钢.AMT3000相角监测功能的实时数字仿真测试[J].电力自动化设备,2000,20(4):57-59.
8李文彬,刘勇,范育兵.小型化宽频带磁传感器的设计[J].舰船电子工程,2012,32(3):129-130. 被引量:4
9USMTO美国制造技术业订单出炉[J].现代制造,2014(4):24-24.
10李立严.通过破碎和HDDR法制备粘结Sm-Fe-(Ta)-N材料[J].电工合金,2000(2):40-43. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
NdFeB permanent magnet was prepared by rapid solidification strip casting and hydrogenation crushing,and its microstructure and properties were characterized by optical microscopy,scanning electron microscopy and AMT—4magnetic property tester.Investigation was made of the effect of sintering temperature on the microstructure and properties of the magnet.The results show that with sintering temperature increasing,the density of the sintered magnet increases,and its remanence,coercivity and maximum magnetic energy product increase at first and then decrease.The reason is that the major crystalline phase grains grow up and the neodymium-rich phase distribution is more homogeneous with sintering temperature increasing.However,when the sintering temperature reaches a certain value,the magnet microstructure is inhomogeneous and the neodymium-rich phase agglomerates.
quote
| GB/T 7714-2015 | [1] PENG Guang-huai, JIA Xiao-wu, HAN Bao-jun, et al. Effect of Sintering Temperature on Microstructure and Properties of NdFeB Magnet[J]. Rare Metals and Cemented Carbides, 2015(2): 33-35. |
| MLA | [1] PENG Guang-huai, et al., "Effect of Sintering Temperature on Microstructure and Properties of NdFeB Magnet." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 33-35. |
| APA | [1] PENG Guang-huai, JIA Xiao-wu, HAN Bao-jun, GUO Hua-bin, & DU Xi-long. (2015). Effect of Sintering Temperature on Microstructure and Properties of NdFeB Magnet. Rare Metals and Cemented Carbides(2), 33-35. |
| IEEE | [1] PENG Guang-huai, JIA Xiao-wu, HAN Bao-jun, GUO Hua-bin, and DU Xi-long, "Effect of Sintering Temperature on Microstructure and Properties of NdFeB Magnet," Rare Metals and Cemented Carbides, no. 2, pp. 33-35, 2015. keywords: {rapid solidification method;sintered NdFeB magnet;sintering temperature;magnetic property} |