The Influences of Fluoridization Methods on Performance of Fluorine-containing Cerium-based Rare Earth Polishing Powder AITranslate
Abstract AITranslate
The precursor of fluorine-containing cerium-based rare earth polishing powder was obtained by fluoridization of cerium-based rare earth carbonate added with hydrofluoric acid,and then it was roasted at high temperature and ground and graded to prepare fluorine-containing cerium-based rare earth polishing powder.The effects were investigated of two fluoridization methods on phase structure,particle size and distribution and polishing performance of fluorine-containing cerium-based rare earth polishing powder.The results show that fluoridization method has no obvious effect on polishing performance of cerium-based rare earth polishing powder.However,the particle size is significantly reduced of the polishing power and its precursor prepared by fluoridization with hydrofluoric acid at first and then precipitation with ammonium bicarbonate,and their particle size distribution is narrower.
KeyWords AITranslate
1杨国胜,崔凌霄,谢兵,黄绍东,吴文远.铈基稀土抛光粉焙烧过程的研究[J].稀土,2013,34(5):11-15. 被引量:3
2杨来东,李梅,柳召刚,胡艳宏,王觅堂.含氟铈基稀土抛光粉的制备及其抛光性能[J].有色金属:冶炼部分,2013(4):45-48. 被引量:9
3康秋珍,任立华.浅析稀土抛光粉产业的发展现状与前景[J].甘肃冶金,2012,34(2):51-53. 被引量:8
4谢丽英.包头稀土抛光粉产业差距分析[J].稀土信息,2010,16(6):18-20. 被引量:4
5黄绍东,李学舜.稀土抛光粉的应用及发展简介[J].稀土,2008,29(1):59-62. 被引量:15
6黄绍东,刘铃声,李学舜,李培忠,郭殿东.光学玻璃抛光用稀土抛光粉的制备[J].稀土,2002,23(6):46-49. 被引量:21
7N. B. Kirk,J. V. Wood.The effect of the calcination process on the crystallite shape of sol-gel cerium oxide used for glass polishing[J]. Journal of Materials Science . 1995 (8)
1贾慧灵,卢元,吴锦绣,谭心,邵祺,任元.氟、硅掺杂对CeO_(2)(001)表面结构及还原性能影响的第一性原理研究[J].中国稀土学报,2023,41(4):794-801.
1王永和,金彦章,胡石磊,宋在芝,王军.光学玻璃掺氟铈基抛光材料的制备研究[J].中国玻璃,2016,0(5):3-6.
2尹证.环境条件对玻璃钢冷却塔冷却能力影响的初步探索[J].玻璃钢/复合材料,1997(4):35-37. 被引量:1
3氯化钾镀锌低铬彩色钝化选用伺种配方好?[J].表面工程资讯,2010,10(1):37-37.
4张丰胜,杨廷录,沈师孔.正丁烷氧化制顺酐Ce基复合氧化物VPO催化剂研制[J].分子催化,2000,14(4):260-264. 被引量:5
5黄金昌.铈基抛光剂的应用与市场[J].稀有金属快报,1995(4):1-4.
6柳召刚,李梅,胡艳宏,刘铃声,熊晓柏.铈基氧化物粉体的湿化学法制备及用途[J].湿法冶金,2004,23(4):176-181. 被引量:2
7谭文轶,钟秦.铈基固体电解质的燃烧法制备及其导电特性[J].材料导报,2005,19(3):101-103. 被引量:5
8李先柏,喻庆华.晶态镝、钬、铒、钇碳酸盐的制备[J].稀有金属,1994,18(5):360-364. 被引量:1
9闫玉玲,李丽华,张金生,吴限.铈基纳米复合氧化物的研究及其应用进展[J].应用化工,2016,45(11):2125-2129. 被引量:5
10汪卫华.新型铈基非晶结构材料——金属塑料[J].中国基础科学,2006,8(2):7-7.
Basic Information:
DOI:
Chinese Library Classification Number:TQ133.3[化学工程—无机化工]
Citation Information:
The precursor of fluorine-containing cerium-based rare earth polishing powder was obtained by fluoridization of cerium-based rare earth carbonate added with hydrofluoric acid,and then it was roasted at high temperature and ground and graded to prepare fluorine-containing cerium-based rare earth polishing powder.The effects were investigated of two fluoridization methods on phase structure,particle size and distribution and polishing performance of fluorine-containing cerium-based rare earth polishing powder.The results show that fluoridization method has no obvious effect on polishing performance of cerium-based rare earth polishing powder.However,the particle size is significantly reduced of the polishing power and its precursor prepared by fluoridization with hydrofluoric acid at first and then precipitation with ammonium bicarbonate,and their particle size distribution is narrower.
quote
| GB/T 7714-2015 | [1] MI Ning, YANG Lai-dong. The Influences of Fluoridization Methods on Performance of Fluorine-containing Cerium-based Rare Earth Polishing Powder[J]. Rare Metals and Cemented Carbides, 2015(2): 29-32. |
| MLA | [1] MI Ning, and YANG Lai-dong. "The Influences of Fluoridization Methods on Performance of Fluorine-containing Cerium-based Rare Earth Polishing Powder." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 29-32. |
| APA | [1] MI Ning, & YANG Lai-dong. (2015). The Influences of Fluoridization Methods on Performance of Fluorine-containing Cerium-based Rare Earth Polishing Powder. Rare Metals and Cemented Carbides(2), 29-32. |
| IEEE | [1] MI Ning and YANG Lai-dong, "The Influences of Fluoridization Methods on Performance of Fluorine-containing Cerium-based Rare Earth Polishing Powder," Rare Metals and Cemented Carbides, no. 2, pp. 29-32, 2015. keywords: {fluorine-containing cerium-based rare earth polishing powder;cerium-based rare earth carbonate;fluoridization method;polishing performance;particle size} |