daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Magnetocaloric Effect of La(FeMCoSi)13B0.25 Series Alloy at Low Magnetic Field AITranslate

Department of CNC Technology, Baotou Vocational and Technical College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

LaFe11.1-xCrxCo0.8Si1.1B0.25 and LaFe11.1-xTixCo0.8Si1.1B0.25 series alloys were prepared by adding a small amount of Cr and Ti elements into LaFeCoSi-based alloy,and their magnetocaloric effects were measured using directly measuring instrument at 1.5T magnetic field.The experimental results show that both Cr addition and Ti addition have influence on Curie temperature and magnetocaloric effect of the serie alloy.The properties of the material can be adjusted to some extent taking advantage of these alloying elements.

KeyWords AITranslate

LaFeCoSi-based alloy Cr Ti magnetic refrigeration room temperature magnetic refrigeration material adiabatic temperature change

1生利英,黄焦宏,曹朝霞,齐勇田,宋博宇.Gd_3Al_(2-x)Ga_x系合金绝热温变的直接测量[J].金属功能材料,2015,22(2):37-40. 被引量:1

2张鑫,邱万奇,史新伟,李春明.Cr在多弧离子镀(Ti,Cr)N复合膜中的作用[J].真空,2007,44(2):48-50. 被引量:2

3胡兵,潘应君,王晴芳,周慧敏,徐明.添加Cr、V元素对Mo_2FeB_2基金属陶瓷的组织及性能的影响[J].金属热处理,2011,36(6):29-32. 被引量:7

4李爱民,孙康宁,张玉军,李静,尹衍升.Cr对Fe-Al/Al_2O_3复合材料韧性的影响[J].材料工程,2001(9):21-24. 被引量:3

5李祖来,蒋业华,周荣,陈志辉,山泉.Cr的添加对WC_p/铁基表层复合材料三体磨料磨损性能的影响[J].材料热处理学报,2014,35(1):17-21. 被引量:7

6刘肖,李玉龙,沙江波,马朝利.合金元素对Nb-Mo-Si合金相平衡及Nb-Nb_5Si_3共晶组织形态的影响[J].复合材料学报,2008,25(2):16-20. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TB64[一般工业技术—制冷工程]

Citation Information:

LaFe11.1-xCrxCo0.8Si1.1B0.25 and LaFe11.1-xTixCo0.8Si1.1B0.25 series alloys were prepared by adding a small amount of Cr and Ti elements into LaFeCoSi-based alloy,and their magnetocaloric effects were measured using directly measuring instrument at 1.5T magnetic field.The experimental results show that both Cr addition and Ti addition have influence on Curie temperature and magnetocaloric effect of the serie alloy.The properties of the material can be adjusted to some extent taking advantage of these alloying elements.

quote

GB/T 7714-2015 [1] WANG Li-quan. Magnetocaloric Effect of La(FeMCoSi)13B0.25 Series Alloy at Low Magnetic Field[J]. Rare Metals and Cemented Carbides, 2015(2): 36-38.
MLA [1] WANG Li-quan. "Magnetocaloric Effect of La(FeMCoSi)13B0.25 Series Alloy at Low Magnetic Field." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 36-38.
APA [1] WANG Li-quan. (2015). Magnetocaloric Effect of La(FeMCoSi)13B0.25 Series Alloy at Low Magnetic Field. Rare Metals and Cemented Carbides(2), 36-38.
IEEE [1] WANG Li-quan, "Magnetocaloric Effect of La(FeMCoSi)13B0.25 Series Alloy at Low Magnetic Field," Rare Metals and Cemented Carbides, no. 2, pp. 36-38, 2015. keywords: {LaFeCoSi-based alloy;Cr;Ti;magnetic refrigeration;room temperature magnetic refrigeration material;adiabatic temperature change}