Synthesis and Characterization of Cathode Material LiNi1/3Co1/3Mn1/3O_2 for Lithium-ion Battery with Spray Drying Method AITranslate

Suzhou University Shagang Steel College;Suzhou University Shagang Steel College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The cathode material LiNi1/3Co1/3Mn1/3O2 for lithium-ion battery was successfully synthesized with the spray drying method and its crystal structure, morphology and electrochemical performance were characterized by SEM,XRD and charge-discharge experiments. The results show that the cathode material LiNi1/3Co1/3Mn1/3O2 with spherical and evenly distributed particles can be synthesized at 750 ℃ for 12 h. And the cathode material exhibits excellent electrochemical performance for that its initial discharge specific capacity is 154 mA ·h/g under the conditions of 2.8~4.3 V and 0.1C and its discharge specific capacity is maintained at 94.7 % after 25 cycles.

KeyWords AITranslate

lithium-ion battery cathode material LiNi1/3Co1/3Mn1/3O2 spray drying method electrochemicalperformance

1刘云建,胡启阳,李新海,王志兴,郭华军,彭文杰.钴酸锂的再生及其电化学性能[J].中国有色金属学报,2007,17(6):984-989. 被引量:10

2Lee J, Kim T, Park 13. Metal-phosphate coating on LiCoO2 cathodes with high cutoff voltages[J]. Materi- als Research Bulletin,2007,42(7):1 201-1 211.

3黄可龙.锂离子电池原理与关键技术[M].北京:化学工业出版社,2009.

4Zhang S C, Qiu X P, He Z Q, et al. Nanoparticled LiNil/3COl/3MnO2 as cathode material for high- rate lithium-ion batteries[J]. Power Sources, 2006,153 : 350- 353.

5Ding Y H,Zhang P,Jiang Y,et al. The effect of sodium dodecyl sulfate on the conformation of bovine serum al bumin[J]. Solid State Lonics, 2007,298 ( 3 ) : 163-169.

6Hu Y Y,Zhou Y K,Wang J,etal. Preparation and char- acterization of macroporous LiNi1/3 Col/3 Mnl/3 02 using carbon sphere as template[J]. Materials Chemistry and Physics, 2011,129 : 296-300.

7Cao Q,Zhang H P,Wang G,et al. A novel carbon-coated LiCoO2 as cathode material for lithium ion battery[J]. Electrochemistry Communications, 2007, 9 ( 5 ) : 1 228 - 1 232.

8Chen C H, Liu J, Stoll M E, et al. Aluminum-doped lithi- um nickel cobalt oxide electrodes for high power lithium -ion batteries I J]. Journal of Power Sources, 2004, 128 (2) :278-285.

9Fujii Y, Miura H, Suzuki N,et al. Structural and electro- chemical properties of LiCol/a Nil/3 Mnl/3O2 calcination temperature dependence[J]. Journal of Power Sources, 2007,171(2) :894-903.

1董恩华,纪鸿文,刘秉国,宇文超.微波法一步合成LiNi_(1/3)Co_(1/3)Mn_(1/3)O_(2)材料及其性能[J].有色金属工程,2022,12(6):14-22.

2董恩华,纪鸿文,刘秉国,宇文超.氧化石墨烯包覆LiNi_(1/3)Co_(1/3)Mn_(1/3)O_(2)复合正极材料及其性能[J].中国有色冶金,2022,51(3):121-127.

1章守权,葛秀涛.水热法合成LiNi_(1/3)Co_(1/3)Mn_(1/3)O_2及其性能研究[J].材料导报,2014,28(6):37-39. 被引量:4

2李奇峰,朱华丽,刘平礼,张磊,谢添,陈召勇.锂离子电池正极材料LiNi_(1/3)Co_(1/3)Mn_(1/3)O_2的制备及其电化学性能[J].合成化学,2013,21(2):151-156. 被引量:2

3李星,唐水花,瞿美臻,关小旭,康毅力.锂离子电池正极材料LiNi_(1/3)Co_(1/3)Mn_(1/3)O_2的研究现状[J].合成化学,2013,21(2):251-256. 被引量:2

4章守权.共沉淀法合成Zr-Mg掺杂的LiNiO_2及其性能研究[J].滁州学院学报,2008,10(3):83-86. 被引量:1

5郭子龙,吁霁.低温固相法制备球形掺La镍酸锂正极材料及其电化学性能[J].材料导报,2013,27(10):40-44. 被引量:3

6欧阳曦,陈珍华,郑雪琴.电感耦合等离子体原子发射光谱法测定锂离子电池三元正极材料LiNi_(1-x-y)Co_xMn_yO_2中钠[J].冶金分析,2014,34(11):42-45. 被引量:1

7丁燕怀,张平,姜勇,尹久仁,卢其斌,高德淑.Ti,F复合掺杂改进LiNi_(1/3)Co_(1/3)Mn_(1/3)O_2正极材料的电化学性能[J].高等学校化学学报,2007,28(10):1839-1841. 被引量:15

8滑纬博,郭孝东,郑卓,张继斌,钟本和.纳米片LiNi_(1/3)Co_(1/3)Mn_(1/3)O_2正极材料的制备与研究[J].化学研究与应用,2014,26(3):441-444. 被引量:5

9滑纬博,郑卓,李龙燕,郭孝东,刘恒,沈重亨,吴振国,钟本和,黄令.氨蒸发诱导法制备纳米结构LiNi1/3Co1/3Mn1/3O2及其作为高功率型锂离子电池正极材料的性能[J].物理化学学报,2014,30(8):1481-1486. 被引量:3

10宫杰,王春忠,杨景海,王雅新,宗占国.Al掺杂LiNi_(1-x)Al_xO_2固溶体的制备及结构研究[J].吉林大学学报:理学版,2002,40(3):280-283.

Basic Information:

DOI:

Chinese Library Classification Number:O614.111[理学—无机化学]

Citation Information:

The cathode material LiNi1/3Co1/3Mn1/3O2 for lithium-ion battery was successfully synthesized with the spray drying method and its crystal structure, morphology and electrochemical performance were characterized by SEM,XRD and charge-discharge experiments. The results show that the cathode material LiNi1/3Co1/3Mn1/3O2 with spherical and evenly distributed particles can be synthesized at 750 ℃ for 12 h. And the cathode material exhibits excellent electrochemical performance for that its initial discharge specific capacity is 154 mA ·h/g under the conditions of 2.8~4.3 V and 0.1C and its discharge specific capacity is maintained at 94.7 % after 25 cycles.

quote

GB/T 7714-2015 [1] WANG Zheng-guo, ZHONG Sheng-kui. Synthesis and Characterization of Cathode Material LiNi1/3Co1/3Mn1/3O_2 for Lithium-ion Battery with Spray Drying Method[J]. Rare Metals and Cemented Carbides, 2014(4): 59-62.
MLA [1] WANG Zheng-guo, and ZHONG Sheng-kui. "Synthesis and Characterization of Cathode Material LiNi1/3Co1/3Mn1/3O_2 for Lithium-ion Battery with Spray Drying Method." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 59-62.
APA [1] WANG Zheng-guo, & ZHONG Sheng-kui. (2014). Synthesis and Characterization of Cathode Material LiNi1/3Co1/3Mn1/3O_2 for Lithium-ion Battery with Spray Drying Method. Rare Metals and Cemented Carbides(4), 59-62.
IEEE [1] WANG Zheng-guo and ZHONG Sheng-kui, "Synthesis and Characterization of Cathode Material LiNi1/3Co1/3Mn1/3O_2 for Lithium-ion Battery with Spray Drying Method," Rare Metals and Cemented Carbides, no. 4, pp. 59-62, 2014. keywords: {lithium-ion battery;cathode material;LiNi1/3Co1/3Mn1/3O2;spray drying method;electrochemicalperformance}