Effect of Trace Element Boron on the Solidification Microstructure of Single-crystal Nickel-based Superalloy AITranslate
Abstract AITranslate
Single-crystal nickel-based superalloys DD90 with different boron contents were prepared by seed growth technique, and the influences were researched of B element on dendritic structure, eutectic structure and carbide morphology. The results show that with boron content increasing, the secondary dendrites gradually become thicker, the third dendrites become more distinct, and meanwhile, the carbides increase while the eutectic microstructure obviously decreases.
KeyWords AITranslate
1汤晓君,张永军,李建国.超高温度梯度下凝固速率对一种镍基单晶高温合金定向凝固组织的影响[J].稀有金属材料与工程,2012,41(4):738-742. 被引量:7
2McLean M. Directional solidified material for high tem- perature service[M]. London: The Material Society, 1983.4.
3马书伟,李嘉荣,侯淑娥,曾强,郑运荣,颜鸣皋.Re对γ′相粗化行为的影响[J].航空材料学报,2000,20(3):11-15. 被引量:7
4Sammmy Tin. Carbon additions and grain defect forma- tion in direvtionally solidified nickel-base superalloys [D]. American : The University of Michigan, 2001.
5韩利哲,罗震,葛凤,李洋,刘建,赵楠.Inconel 601合金胀形成形的显微结构及其性能[J].中国科技论文在线,2010,5(4):265-268. 被引量:1
6胥国华,焦兰英,张北江,秦鹤勇,赵光普.固溶冷却速度对GH4586合金组织及850℃拉伸性能的影响[J].材料热处理学报,2006,27(2):47-49. 被引量:8
7陈国胜,金鑫,周奠华,王世普,谢伟,王林涛.硼含量对镍基合金GH4049晶界析出相和高温性能的影响[J].金属学报,2005,41(6):622-626. 被引量:21
8张磊,祁峰,张伟红,信昕,孙文儒.B对高W镍基高温合金凝固行为的影响[J].热加工工艺,2011,40(23):33-37. 被引量:6
9张明军,骆宇时,肖程波,唐定中,吴仲棠.抽拉速率对DD6单晶高温合金组织的影响[J].材料工程,2010,38(11):8-10. 被引量:5
10Rutter J W. A prismatic substructure {ormed during so lidification of metals[J]. Can J Phys, 1953,31 (1) : 15- 39.
1韩二锋,黄瑞,刘杨.B对发动机用真空感应熔炼GH600合金凝固组织和力学性能的影响[J].真空科学与技术学报,2020,0(2):153-157. 被引量:2
2刘剑辉,杨树峰,赵跃文.应力时效对发动机用GH4169镍基合金组织演化及蠕变抗力的影响[J].热加工工艺,2018,47(16):196-199.
1谭大庆,姜山,胡韶华,杨洪.载荷对非自耗真空熔炼GC2025高硬刀具的滑动磨损行为的影响[J].真空科学与技术学报,2021,41(5):477-481.
2吴立凡,李涛.RE对真空感应熔炼热轧SA516Gr70钢拉伸和冲击性能的影响[J].锻压技术,2021,46(11):255-259. 被引量:3
1汪圣林,崔丽,贺定勇,周正,蒋建敏.亚共晶Fe-Cr-B-C系堆焊合金的组织及耐磨性[J].热加工工艺,2016,45(1):30-33. 被引量:3
2李宁宁,宋克兴,周延军,张彦敏,何霞.热处理对Cu-0.23Be-0.84Co合金性能和组织的影响[J].河南科技大学学报:自然科学版,2015,36(2):10-13. 被引量:6
3梁福鸿,丛津功,胡昕明.石油储罐用08MnNiVR钢板组织和性能研究[J].鞍钢技术,2009(5):32-35. 被引量:5
4马幼平,李泽宇,刘玉高,赵峰,李俊,杨蕾.复合变质对过共晶高铬铸铁凝固组织的影响[J].兵器材料科学与工程,2007,30(6):35-38. 被引量:2
5晏井利,薛烽,白晶,周健,徐燕芳.Mg-(1-4)Ce合金的组织和性能[J].东南大学学报:自然科学版,2014,44(4):876-880. 被引量:1
6黄安国,王永生,李志远.低合金钢焊缝中先共析铁素体组织数量的控制[J].电焊机,2003,33(10):9-14. 被引量:14
7娄开钧,陈培生,熊振茵,黄旭华.复合变质剂对高铬白口铸铁组织与性能的影响[J].铸造,1996,45(4):15-18. 被引量:1
8陈健,汪兵,胡亮,刘清友,刘翔.高强度管线钢微观组织对氢致裂纹的影响[J].钢铁,2015,50(4):48-52. 被引量:11
9李铁龙,杨新岐.45钢锤头淬火后的组织和硬度[J].热加工工艺,2012,41(4):201-203. 被引量:2
10尹冬松.Nd对Mg-6Zn微观组织影响研究[J].铸造设备与工艺,2010(5):34-36.
Basic Information:
DOI:
Chinese Library Classification Number:TG132.32[一般工业技术—材料科学与工程]
Citation Information:
Single-crystal nickel-based superalloys DD90 with different boron contents were prepared by seed growth technique, and the influences were researched of B element on dendritic structure, eutectic structure and carbide morphology. The results show that with boron content increasing, the secondary dendrites gradually become thicker, the third dendrites become more distinct, and meanwhile, the carbides increase while the eutectic microstructure obviously decreases.
quote
| GB/T 7714-2015 | [1] ZHANG Xin-lei. Effect of Trace Element Boron on the Solidification Microstructure of Single-crystal Nickel-based Superalloy[J]. Rare Metals and Cemented Carbides, 2014(4): 55-58. |
| MLA | [1] ZHANG Xin-lei. "Effect of Trace Element Boron on the Solidification Microstructure of Single-crystal Nickel-based Superalloy." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 55-58. |
| APA | [1] ZHANG Xin-lei. (2014). Effect of Trace Element Boron on the Solidification Microstructure of Single-crystal Nickel-based Superalloy. Rare Metals and Cemented Carbides(4), 55-58. |
| IEEE | [1] ZHANG Xin-lei, "Effect of Trace Element Boron on the Solidification Microstructure of Single-crystal Nickel-based Superalloy," Rare Metals and Cemented Carbides, no. 4, pp. 55-58, 2014. keywords: {boron;single-crystal nickel-based superalloy;solidification microstructure;dendritic microstructure;eutectic microstructure;carbide} |