Characterization and Research on the Influencing Factors of Recycled Cemented Carbide AITranslate
Abstract AITranslate
In view of increased product consumption and scrap accumulation in domestic cemented carbide field and decreased reserves and exploitation of tungsten resources, recycled materials from cemented carbide scrap were chosen as the research subjects. Crystal morphology, chemical composition and phase structure of recycled cobalt powder and tungsten carbide powder were characterized by SEM, EDS and XRD. Hardness of recycled W-Co alloy was tested by Rockwell apparatus. Based on the analysis for the above results,the existing problems in recycled cemented carbide are determined, providing some theoretical support for improvement of recycling technology and process control technology of cemented carbide scrap.
KeyWords AITranslate
1朱丽慧,马学鸣,雷景轩,赵海锋.纳米硬质合金的研究进展[J].稀有金属材料与工程,2004,33(4):349-353. 被引量:23
2Upadhyaya A, Sarathy D,Wagner G. Advances in sinte- ring of hard metals[J]. Materials and Design, 2001,22: 499-506.
3葛启录,肖振声,韩欢庆.高性能难熔材料在尖端领域的应用与发展趋势[J].粉末冶金工业,2000,10(1):7-13. 被引量:49
4王英姿,侯宪钦.带能谱分析的扫描电子显微镜在材料分析中的应用[J].制造技术与机床,2007(9):80-83. 被引量:37
5李继刚,吴希俊,谭洪波,刘金芳.纳米碳化钨粉的制备及其热稳定性研究[J].稀有金属材料与工程,2004,33(7):736-739. 被引量:22
6宁阳.球磨WC-Co纳米复合粉末的合成和成形[J].稀有金属与硬质合金,2003,31(1):53-56. 被引量:5
7张玉华,吴恩熙.硬质合金抗弯强度的研究[J].稀有金属材料与工程,1991(3):31-36. 被引量:6
8易勇,熊继,李懿,沈保罗.硬质合金抗弯强度及其分散性的研究[J].工具技术,2002,36(10):16-19. 被引量:32
9Brookes K. Optimized hard-metals:Pick of the paper at Plansee[J]. Metal Powder Report, 2002,57 ( 1 ) : 30-34.
10Sun J, Zhang F, Shen J. Characterization of ball milled nano-crystalline WC-Co composite powders and subse- quently rapid hot pressing[J]. Materials Letters, 2003, 57(21) :3 140-3 148.
1周新华,王力民,彭英健.我国硬质合金再生产业现状与发展[J].硬质合金,2016,33(5):356-364. 被引量:19
1李亮星,朱志城,贾孟熹,黄茜琳.硬质合金废料电解回收钨及W(Ⅵ)在熔盐中的电化学行为[J].材料导报,2022,36(S01):448-453.
2陈飞,龙坚战,冉丽萍,邱友绪.Al含量对WC-Fe合金的组织与性能的影响[J].硬质合金,2017,34(2):75-82.
3王超,张红梅,李岩,贾宏斌,王渐灵,孟令浩,姜正义.烧结温度对碳化钨/高强钢复合材料界面微观组织和元素扩散的影响[J].功能材料,2019,50(4):4086-4092.
4谭千榆,王鹏,时凯华,曾伟.Co-Ni-Cr复合粘结相矿用合金的研制及生产[J].四川冶金,2019,41(3):29-33. 被引量:1
5邝海,谭敦强,何文,易志强.氧化还原法回收废硬质合金[J].稀有金属与硬质合金,2019,47(4):70-75. 被引量:3
6赵中伟,孙丰龙,杨金洪,方奇,姜文伟,刘旭恒,陈星宇,李江涛.我国钨资源、技术和产业发展现状与展望[J].中国有色金属学报,2019,29(9):1902-1916. 被引量:39
7汪艳亮,王云,谢小豪,陈林芳,陈颢.稀土硬质合金研究进展[J].有色金属科学与工程,2019,10(5):106-112. 被引量:9
8谢小豪,王云,汪艳亮,陈颢.废旧硬质合金回收方法及其研究进展[J].有色金属科学与工程,2020,11(2):64-70. 被引量:11
9李刚,张红梅,赵大东,王超,李洪楠,李娜,孟令浩,姜正义.颗粒粒径对碳化钨/高强钢复合材料界面微观组织和元素扩散的影响[J].功能材料,2021,52(1):1104-1114.
10熊华超,汤昌仁,胡梦云.电解法回收废旧硬质合金的研究现状及展望[J].中国金属通报,2020(24):271-272.
1邝海.锌熔法回收废旧硬质合金的研究进展[J].稀有金属与硬质合金,2016,44(5):79-82. 被引量:13
2程秀兰,洪海侠.钛含量对WC-8Co硬质合金组织和性能的影响[J].凿岩机械气动工具,2016,42(4):43-46.
3张兴华,汪明朴.再生碳化钨性能及应用[J].硬质合金,2008,25(1):58-62. 被引量:7
4钟连生.低压烧结对钨钴合金碳校正的初步探讨[J].硬质合金,1990(3):5-9. 被引量:4
5羊建高,熊继.稀土添加剂对钨钴合金中碳化钨晶粒度影响的研究[J].有色金属与稀土应用,1994(2):36-38.
6廖军,吴翔,江庆.烧结温度对含再生料硬质合金性能的影响[J].四川有色金属,2013(2):45-48. 被引量:3
7王元荪.专利信息[J].上海有色金属,2008,29(4):194-194.
8赵万军,杨海林,阮建明.再生料制备的硬质合金组织与性能研究[J].硬质合金,2008,25(3):169-174. 被引量:17
9王瑶,刘雪梅,宋晓艳,魏崇斌,王海滨,王西龙.高性能再生硬质合金的短流程回收制备[J].金属学报,2014,50(5):633-640. 被引量:8
10杨斌,陈广军,石安红,刘柏雄.废旧硬质合金短流程回收技术的研究现状[J].材料导报,2015,29(3):68-74. 被引量:15
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
In view of increased product consumption and scrap accumulation in domestic cemented carbide field and decreased reserves and exploitation of tungsten resources, recycled materials from cemented carbide scrap were chosen as the research subjects. Crystal morphology, chemical composition and phase structure of recycled cobalt powder and tungsten carbide powder were characterized by SEM, EDS and XRD. Hardness of recycled W-Co alloy was tested by Rockwell apparatus. Based on the analysis for the above results,the existing problems in recycled cemented carbide are determined, providing some theoretical support for improvement of recycling technology and process control technology of cemented carbide scrap.
quote
| GB/T 7714-2015 | [1] LI Shao-xiang, WANG Zhao-feng, LI Wen-qian, et al. Characterization and Research on the Influencing Factors of Recycled Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2014(4): 63-67. |
| MLA | [1] LI Shao-xiang, et al., "Characterization and Research on the Influencing Factors of Recycled Cemented Carbide." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 63-67. |
| APA | [1] LI Shao-xiang, WANG Zhao-feng, LI Wen-qian, ZHOU Gui-zhong, & LIU Guang-zhao. (2014). Characterization and Research on the Influencing Factors of Recycled Cemented Carbide. Rare Metals and Cemented Carbides(4), 63-67. |
| IEEE | [1] LI Shao-xiang, WANG Zhao-feng, LI Wen-qian, ZHOU Gui-zhong, and LIU Guang-zhao, "Characterization and Research on the Influencing Factors of Recycled Cemented Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 63-67, 2014. keywords: {cemented carbide scrap;recycling;crystal morphology;chemical composition;phase structure hardness} |