A new method of constructing physics-based nano-crystalline atomic structures for molecular dynamics simulation AITranslate
Abstract AITranslate
We present a new method of constructing various nano-crystalline structures for molecular dynamics simulations. The basic idea underlying our method is to map the microstructure obtained from the phase field model onto the atomic configuration. As a result, we can construct more realistic nano-crystalline structures compared to the Voronoi construction method that has been widely used for studying nano-structured materials. The new method gives us much freedom in constructing single- or multi-component nano-crystalline structures, single- or multi-phase microstructures, and random packing of nano-particles for use in molecular dynamics simulations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2010.06.005
Chinese Library Classification Number:
Citation Information:
We present a new method of constructing various nano-crystalline structures for molecular dynamics simulations. The basic idea underlying our method is to map the microstructure obtained from the phase field model onto the atomic configuration. As a result, we can construct more realistic nano-crystalline structures compared to the Voronoi construction method that has been widely used for studying nano-structured materials. The new method gives us much freedom in constructing single- or multi-component nano-crystalline structures, single- or multi-phase microstructures, and random packing of nano-particles for use in molecular dynamics simulations.
quote
| GB/T 7714-2015 | [1] NaYoung Park, SeungCheol Lee, PilRyung Cha. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.06.005. |
| MLA | [1] NaYoung Park, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.06.005. |
| APA | [1] NaYoung Park, SeungCheol Lee, & PilRyung Cha. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.06.005 |
| IEEE | [1] NaYoung Park, SeungCheol Lee, and PilRyung Cha, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.06.005. |