Molecular dynamics simulation of porous layer-induced stress in Fe single crystal AITranslate

University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Pipeline steel in soil containing water could induce a macro tensile stress, leading to stress corrosion cracking (SCC). Porous layer-induced stress in Fe single crystal with various vacancy distributions on the surface layer is studied using molecular dynamics. The results show that Fe single crystal with one end fixed and a porous layer on the surface is deflected toward the porous layer during relaxation, resulting in a macro tensile stress. There is a maximum tensile stress in the matrix near the interface between the porous layer and the matrix resulting from the porous layer. The average stress on the porous layer σxx(d), which is calculated based on the measured deflection, increases with the increase of the maximum vacancy concentration CV on the top surface and the relative depth of the porous layer d/B. And the macro tensile stress σxx(B) on the cross section of the sample increases also with the increase of CV and d/B. σxx(B) is approximately four times smaller than σxx(d).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.06.006

Chinese Library Classification Number:

Citation Information:

Pipeline steel in soil containing water could induce a macro tensile stress, leading to stress corrosion cracking (SCC). Porous layer-induced stress in Fe single crystal with various vacancy distributions on the surface layer is studied using molecular dynamics. The results show that Fe single crystal with one end fixed and a porous layer on the surface is deflected toward the porous layer during relaxation, resulting in a macro tensile stress. There is a maximum tensile stress in the matrix near the interface between the porous layer and the matrix resulting from the porous layer. The average stress on the porous layer σxx(d), which is calculated based on the measured deflection, increases with the increase of the maximum vacancy concentration CV on the top surface and the relative depth of the porous layer d/B. And the macro tensile stress σxx(B) on the cross section of the sample increases also with the increase of CV and d/B. σxx(B) is approximately four times smaller than σxx(d).

quote

GB/T 7714-2015 [1] D. Li, F.Y. Meng, X.Q. Ma, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.06.006.
MLA [1] D. Li, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.06.006.
APA [1] D. Li, F.Y. Meng, X.Q. Ma, L.J. Qiao, & W.Y. Chu. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.06.006
IEEE [1] D. Li, F.Y. Meng, X.Q. Ma, L.J. Qiao, and W.Y. Chu, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.06.006.