Preparation of Graphene-based Noble Metal Catalysts and their Effects on the Performance of Lithium-oxygen Batteries AITranslate

Faculty of Metallurgy and Energy Engineering,Kunming University of Science and Technology;Faculty of Metallurgy and Energy Engineering,Kunming University of Science and Technology;Faculty of Metallurgy and Energy Engineering,Kunming University of Science and Technology;Faculty of Metallurgy and Energy Engineering,Kunming University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-oxygen batteries,as a new type of battery system with ultra-high theoretical specific energy density,have good application prospects in the field of electric vehicles.Reduced graphene oxide was prepared by modified Hummers method and thermal expansion method,and different noble metals Ru,Ir,Au and Ag were loaded by impregnation reduction method,and the effect of graphene catalysts with different noble metals on the performance of lithium-oxygen batteries were studied.The results show that the reversibility and charge-discharge cycle stability of lithium-oxygen batteries with Ru/RGO and Ir/RGO catalysts with high catalytic activity for oxygen precipitation are better than those of lithium-oxygen batteries with Ag/RGO and Au/RGO catalysts.

KeyWords AITranslate

reduced graphene oxide noble metal catalyst impregnation reduction method Li-O2 battery

1闻雷,刘成名,宋仁升,罗洪泽,石颖,李峰,成会明.石墨烯材料的储锂行为及其潜在应用[J].化学学报,2014,72(3):333-344. 被引量:49

2陈迎龙,甘卫平,刘晓刚,郭桂全,向锋.太阳能电池正面银浆用高分散超细银粉的制备[J].稀有金属与硬质合金,2013,41(1):35-40. 被引量:8

1赵馨睿,王铮,杜娟,李晓宇.Z机制光催化三元复合材料RGO/WO_3/g-C_3N_4结构及光催化性能[J].人工晶体学报,2019,48(4):598-606.

2叶鸿清,赖木深,朱明芳,梁焕如,梁学彬.银-铜/还原氧化石墨烯修饰的玻碳电极测定当归中的阿魏酸[J].广东药科大学学报,2019,35(2):210-214. 被引量:1

3新型.我国下一代锂离子动力电池正极材料研究取得重要进展[J].化工新型材料,2019,47(2):272-272.

4边洋,徐萍萍,申奥,赵洋强,张子英,张俊婷,侯春宁.α-Fe_2O_3单晶纳米片的制备及其电化学性能研究[J].人工晶体学报,2019,48(2):185-189.

5周梦影,王奖,徐爱菊.高缺陷石墨烯的制备及性能[J].内蒙古师范大学学报:自然科学汉文版,2019,48(3):239-243.

6张志刚,周扬杰,李帅,林琅,蒋晓瑜.钴酸镧掺杂Ti/RuO_2电极材料电化学性能研究[J].湖南师范大学自然科学学报,2019,42(1):70-75. 被引量:3

7吴佳凡,李军,张希,戴永红.高气压型臭氧发生器结构设计与性能研究[J].造纸科学与技术,2019,38(1):76-82.

8宁小娜,严宏,郭辰峻,刘富伟,董茜.谷氧还蛋白2对高氧诱导的人晶状体上皮细胞过度迁移的抑制作用[J].中华实验眼科杂志,2019,37(4):245-251.

9徐士亮,宋兴连,韩卫东,刘涛.升温速度和气氛对MnZn铁氧体材料烧结性能的影响[J].磁性材料及器件,2019,50(3):29-32.

10物理研究所.物理所等高体积和重量能量密度锂-硫电池研究获进展[J].硅酸盐通报,2019,38(4):1067-1067.

Basic Information:

DOI:

Chinese Library Classification Number:TM911.41[电气工程—电力电子与电力传动];TQ426[化学工程]

Citation Information:

Lithium-oxygen batteries,as a new type of battery system with ultra-high theoretical specific energy density,have good application prospects in the field of electric vehicles.Reduced graphene oxide was prepared by modified Hummers method and thermal expansion method,and different noble metals Ru,Ir,Au and Ag were loaded by impregnation reduction method,and the effect of graphene catalysts with different noble metals on the performance of lithium-oxygen batteries were studied.The results show that the reversibility and charge-discharge cycle stability of lithium-oxygen batteries with Ru/RGO and Ir/RGO catalysts with high catalytic activity for oxygen precipitation are better than those of lithium-oxygen batteries with Ag/RGO and Au/RGO catalysts.

quote

GB/T 7714-2015 [1] ZENG Xiao-yuan, ZHANG Ying-jie, LI Xue, et al. Preparation of Graphene-based Noble Metal Catalysts and their Effects on the Performance of Lithium-oxygen Batteries[J]. Rare Metals and Cemented Carbides, 2019(2): 50-56.
MLA [1] ZENG Xiao-yuan, et al., "Preparation of Graphene-based Noble Metal Catalysts and their Effects on the Performance of Lithium-oxygen Batteries." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 50-56.
APA [1] ZENG Xiao-yuan, ZHANG Ying-jie, LI Xue, & DONG Peng. (2019). Preparation of Graphene-based Noble Metal Catalysts and their Effects on the Performance of Lithium-oxygen Batteries. Rare Metals and Cemented Carbides(2), 50-56.
IEEE [1] ZENG Xiao-yuan, ZHANG Ying-jie, LI Xue, and DONG Peng, "Preparation of Graphene-based Noble Metal Catalysts and their Effects on the Performance of Lithium-oxygen Batteries," Rare Metals and Cemented Carbides, no. 2, pp. 50-56, 2019. keywords: {reduced graphene oxide;noble metal;catalyst;impregnation reduction method;Li-O2 battery}