Study on Preparation of Nano-Al_2O_3/Ni-based Superalloy Composite Powder and Laser 3D Printing AITranslate

College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics;College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using polyethylene glycol as dispersants and adhesives,nano-sized Al2O3 ceramic particles were assembled to the surface of Ni-based superalloy spherical particle to prepare Al2O3/Ni-based superalloy powder by the two steps method of ultrasonic dispersion and high speed stirring.Molding Al2O3/Ni-based superalloy composites were prepared by the laser 3 D printing.The results show that the composite powder used for laser 3 D printing technology can be successfully prepared by two steps process of ultrasonic dispersion and high speed stirring.After laser 3 D printing,the microstructure of molding materials is mainly represented by the columnar crystal and isometric crystal structure,uniform and compact,the nano-Al2O3 granules are uniformly distributed in the matrix.The microhardness(HV)of the composites can reach to 405.81.

KeyWords AITranslate

nano-Al2O3 Ni-based superalloy laser 3D printing ultrasonic dispersion high speed stirring

1覃思思,余勇,曾归余,肖明清.3D打印用金属粉末的制备研究[J].粉末冶金工业,2016,26(5):21-24. 被引量:43

2闫岸如,杨恬恬,王燕灵,马志红,杜云,王智勇.选区激光熔化不同层厚镍的热特性与机械性能[J].中国激光,2016,43(2):68-76. 被引量:16

3张升,桂睿智,魏青松,史玉升.选择性激光熔化成形TC4钛合金开裂行为及其机理研究[J].机械工程学报,2013,49(23):21-27. 被引量:69

4于秀平,沈以赴,顾冬冬.激光烧结法制备原位增强型多孔镍基复合材料[J].稀有金属与硬质合金,2009,37(4):11-14. 被引量:7

5温志勋,岳珠峰,朱振涛.镍基单晶合金紧凑拉伸试样高温断裂特性的实验研究[J].材料工程,2007,35(12):15-20. 被引量:1

6姜华,汤海波,王华明.激光熔化沉积DZ408镍基高温合金的组织研究[J].稀有金属与硬质合金,2014,42(1):46-51. 被引量:6

1隆文革.铸造成形工艺中的3D打印激光制备力学性能实验研究[J].应用激光,2021,41(1):148-153.

2霍俊美,何博.Ti_(2)AlNb基合金及其增材制造技术研究进展[J].中国材料进展,2022,41(8):645-652. 被引量:1

1尹先和,周建平,许燕.电极材料对直流短电弧铣削Ti2AlNb加工性能影响的实验研究[J].制造技术与机床,2023(9):39-43.

1章再稳,庞海峰.耐热平滑抗静电锦纶FDY油剂的制备[J].纺织报告,2019,38(2):6-9. 被引量:2

2常川川,张田仓,李菊.Ti-22Al-27Nb合金线性摩擦焊接头组织与显微硬度分析[J].焊接学报,2019,40(3):140-144. 被引量:6

3杨艳萍.两步法处理含参恒成立问题中参数取值范围的问题[J].中学数学研究,2019(5):36-38.

4张晓娟,殷兵,王建朝,李升,刘国彬,胡祖圣,吴卫卫,张英泽.人体下腰椎显微骨硬度分布特征研究[J].中国脊柱脊髓杂志,2019,29(4):343-347. 被引量:4

5何志高,邹旸,邢丽,申科.9Cr18Mo/GH3625异种合金燃油组件激光焊接头的组织分析[J].焊接,2019(4):29-33. 被引量:2

6魏玉顺,罗春丽,闫卫国,刘姝昱,赵世锦.单层胶体晶体及反蛋白质纳米阵列结构的制备研究[J].材料科学,2018,8(12):1119-1128.

7钱建伟.不锈钢A-TIG焊时电弧形貌和熔宽熔深研究[J].江苏船舶,2019,36(1):35-37.

8周川,路新,贾成厂,刘博文.碳纳米管增强铜基复合材料的制备、力学性能及电导率[J].稀有金属材料与工程,2019,48(4):1249-1255. 被引量:8

9薛克敏,孙建辉,纪小虎,郭威威,李萍.高压扭转工艺对TA15钛合金组织和性能的影响[J].稀有金属材料与工程,2019,48(4):1189-1194. 被引量:4

10陈俊,陈晨,罗恒勇.Nb-V微合金化0.15~0.35Mo含量和轧制温度对建筑用耐火钢性能的影响[J].特殊钢,2019,40(3):49-52. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TP391.73[自动化与计算机技术—计算机应用技术];TB383.3[一般工业技术—材料科学与工程]

Citation Information:

Using polyethylene glycol as dispersants and adhesives,nano-sized Al2O3 ceramic particles were assembled to the surface of Ni-based superalloy spherical particle to prepare Al2O3/Ni-based superalloy powder by the two steps method of ultrasonic dispersion and high speed stirring.Molding Al2O3/Ni-based superalloy composites were prepared by the laser 3 D printing.The results show that the composite powder used for laser 3 D printing technology can be successfully prepared by two steps process of ultrasonic dispersion and high speed stirring.After laser 3 D printing,the microstructure of molding materials is mainly represented by the columnar crystal and isometric crystal structure,uniform and compact,the nano-Al2O3 granules are uniformly distributed in the matrix.The microhardness(HV)of the composites can reach to 405.81.

quote

GB/T 7714-2015 [1] PENG Ming-mei, WANG Tao, HE Qing-xian, et al. Study on Preparation of Nano-Al_2O_3/Ni-based Superalloy Composite Powder and Laser 3D Printing[J]. Rare Metals and Cemented Carbides, 2019(2): 57-62.
MLA [1] PENG Ming-mei, et al., "Study on Preparation of Nano-Al_2O_3/Ni-based Superalloy Composite Powder and Laser 3D Printing." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 57-62.
APA [1] PENG Ming-mei, WANG Tao, HE Qing-xian, WU Xin, ZHENG Chang-tian, & WANG Qian. (2019). Study on Preparation of Nano-Al_2O_3/Ni-based Superalloy Composite Powder and Laser 3D Printing. Rare Metals and Cemented Carbides(2), 57-62.
IEEE [1] PENG Ming-mei, WANG Tao, HE Qing-xian, WU Xin, ZHENG Chang-tian, and WANG Qian, "Study on Preparation of Nano-Al_2O_3/Ni-based Superalloy Composite Powder and Laser 3D Printing," Rare Metals and Cemented Carbides, no. 2, pp. 57-62, 2019. keywords: {nano-Al2O3;Ni-based superalloy;laser 3D printing;ultrasonic dispersion;high speed stirring}