daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis and Properties of Yb3+ Co-activated Sr_2MgSi_2O_7∶Eu2+,Dy3+ Long Afterglow Phosphors AITranslate

School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology;School of Materials Science and Engineering,North China University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+long afterglow phosphors were prepared via high-temperature solid state reaction.Microstructure and optical properties of Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+long afterglow phosphors were characterized through XRD,SEM,excitation spectrum,emission spectrum and decay curves.The results show that the crystal structure and microstructure of Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+have not changed significantly.The addition of Yb3+ions shows a remarkable change in fluorescent properties and afterglow performance.The introduction of Yb3+makes Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+have better fluorescence performance and afterglow properties.Different Yb3+doping amounts have a significant effect on the trap depth and electron transport rate of the long afterglow phosphors.When the doping amount of Yb3+equals to 0.03,experiments show that the Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+has the strongest fluorescence intensity and the best afterglow attenuation performance.

KeyWords AITranslate

Sr2MgSi2O7 rare earth element ytterbium high temperature solid phase method long afterglow phosphor material fluorescence performance

1潘文,宁桂玲,林源,杨雪峰.A New Co-Activator Gd_2O_3 to Eu_2O_3 and Dy_2O_3 Doped Alkaline Earth Silicate Phosphors[J].稀土学报:英文版,2007,0(S1):305-309. 被引量:1

2陈将,江国健,周鹏,罗佳文,沈晴昳.燃烧合成Eu^(2+),Eu^(3+),Dy^(3+)掺杂硅酸镁锶材料及其性能研究[J].陶瓷学报,2017,38(1):59-62. 被引量:2

1王乃芹,卢婷.Si掺杂对Ca_(0.8)Zn_(0.2)TiO_(3)∶Pr^(3+)红色长余辉发光材料的影响[J].中国照明电器,2022(11):20-23.

1刘盛意,张金苏,孙佳石,陈宝玖,李香萍,徐赛,程丽红.实验优化设计Sr_2MgSi_2O_7:Eu^(2+),Dy^(3+)的合成及长余辉特性[J].物理学报,2019,68(5):72-78. 被引量:1

2孔丽,乔露,魏奇业,赵明悦,刘莹莹,王文生,于海辉.助熔剂对白光LED用红色荧光粉SrMoO_4:Eu^(3+)的光谱性能影响[J].人工晶体学报,2019,48(4):616-620. 被引量:4

3Nature Photonics报道本刊编委黄维院士团队首例多彩有机“夜明珠”研究新成果[J].南京邮电大学学报:自然科学版,2019,39(2):62-62.

4陈瑞,王维,卜童乐,库治良,钟杰,彭勇,肖生强,尤为,黄福志,程一兵,傅正义.低成本富勒烯衍生物电子传输层在钙钛矿太阳能电池的应用(英文)[J].物理化学学报,2019,35(4):401-407. 被引量:7

5蔡文烨,刘珊珊.一种高温电容器材料的合成方法[J].佛山陶瓷,2019,29(4):9-11.

6钟鑫,牛亚然,朱涛,王亚文,石旻昊,郑学斌.物相组成对硅酸镱涂层显微结构和耐蚀性能的影响研究[J].热喷涂技术,2019,11(1):37-44. 被引量:4

7董竹君,姜鹏程,姚金波,姜会钰.紫苏染料的提取及其对棉织物的染色工艺研究[J].武汉纺织大学学报,2019,32(2):3-7. 被引量:5

8黄彦捷,李成辉,周瑾艳,黄振宇,陈玲,王鑫,关妍.荧光光谱仪的校准方法研究及不确定度评定[J].化学试剂,2019,41(5):495-501. 被引量:2

9稀土[J].金川科技,2019,0(1):56-56.

10杨涵,陈星濛,高俊潇,武晓丽,常津.上转换介孔二氧化硅多功能肝癌诊疗纳米复合体系的构建[J].生物医学工程研究,2019,38(1):1-6. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O482.31[理学—固体物理];TQ422[化学工程]

Citation Information:

Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+long afterglow phosphors were prepared via high-temperature solid state reaction.Microstructure and optical properties of Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+long afterglow phosphors were characterized through XRD,SEM,excitation spectrum,emission spectrum and decay curves.The results show that the crystal structure and microstructure of Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+have not changed significantly.The addition of Yb3+ions shows a remarkable change in fluorescent properties and afterglow performance.The introduction of Yb3+makes Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+have better fluorescence performance and afterglow properties.Different Yb3+doping amounts have a significant effect on the trap depth and electron transport rate of the long afterglow phosphors.When the doping amount of Yb3+equals to 0.03,experiments show that the Sr2MgSi2O7∶Eu2+,Dy3+,Yb3+has the strongest fluorescence intensity and the best afterglow attenuation performance.

quote

GB/T 7714-2015 [1] CAI Yong-feng, LIU Zuo-tao, CHANG Shi-yan, et al. Synthesis and Properties of Yb3+ Co-activated Sr_2MgSi_2O_7∶Eu2+,Dy3+ Long Afterglow Phosphors[J]. Rare Metals and Cemented Carbides, 2019(2): 45-49.
MLA [1] CAI Yong-feng, et al., "Synthesis and Properties of Yb3+ Co-activated Sr_2MgSi_2O_7∶Eu2+,Dy3+ Long Afterglow Phosphors." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 45-49.
APA [1] CAI Yong-feng, LIU Zuo-tao, CHANG Shi-yan, LI Feng-feng, SHEN Yi, CHEN Chen, WU Xin-jiang, WANG Yue, XU Zi-lin, & HUANG Chun-cao. (2019). Synthesis and Properties of Yb3+ Co-activated Sr_2MgSi_2O_7∶Eu2+,Dy3+ Long Afterglow Phosphors. Rare Metals and Cemented Carbides(2), 45-49.
IEEE [1] CAI Yong-feng, LIU Zuo-tao, CHANG Shi-yan, LI Feng-feng, SHEN Yi, CHEN Chen, WU Xin-jiang, WANG Yue, XU Zi-lin, and HUANG Chun-cao, "Synthesis and Properties of Yb3+ Co-activated Sr_2MgSi_2O_7∶Eu2+,Dy3+ Long Afterglow Phosphors," Rare Metals and Cemented Carbides, no. 2, pp. 45-49, 2019. keywords: {Sr2MgSi2O7;rare earth element ytterbium;high temperature solid phase method;long afterglow phosphor material;fluorescence performance}