Theory and Current Research of Strontium and Barium Separation AITranslate
Abstract AITranslate
Sr and Ba separation is a technical difficult problem in the production of high compounds. The principle,characteristics and application of main methods for Sr and Ba viewed,and the study orientation for Sr and Ba separation is also discussed.
KeyWords AITranslate
1刘牡丹,李光辉,董海刚,范晓慧,黄柱成,姜涛.中国碳酸锶工业生产现状与进展[J].无机盐工业,2006,38(1):9-12. 被引量:15
2刘述平.荧光级碳酸锶的制备工艺技术[J].矿产综合利用,2007(6):11-14. 被引量:1
3刘相果,彭晓东,刘江,谢卫东.高纯碳酸锶的制备技术研究进展[J].材料导报,2003,17(9):54-57. 被引量:11
4王树轩,黄宁.高纯碳酸锶生产方法[J].陕西化工,1999,28(2):7-9. 被引量:7
5朱屯.无机盐生产中的锶钡分离[J].无机盐工业,2003,35(2):13-15. 被引量:8
6王日团.从天青石中提取锶和钡[J].有色金属(冶炼部分),1964,(5):55.
7周大俊.由硝酸锶制取分析纯碳酸锶的研究[J].无机盐工业,1994(2):13-15. 被引量:8
8刘恒,周大利,李大成,陈朝珍.电子陶瓷用高纯碳酸锶制备方法[J].电子元件与材料,1998,17(6):18-19. 被引量:8
9贾宗敏,付之正.复分解法从合川天青石中提取碳酸锶[J].中国井矿盐,1983,(3):26-32.
10胡建华.高纯碳酸锶的制备方法[P].中国专利:2009i0305219.i,2011-03-23.
1崔晓莉,李瑞生,蔡仁锁.天青石还原制取粗制硫化锶[J].河北化工,1989(4):6-8.
2刘建明,段东平,钟莉,韩宏亮,周娥.高纯碳酸锶清洁生产国内外研究进展[J].盐湖研究,2013,21(2):66-72. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TQ132.33[化学工程—无机化工]
Citation Information:
Sr and Ba separation is a technical difficult problem in the production of high compounds. The principle,characteristics and application of main methods for Sr and Ba viewed,and the study orientation for Sr and Ba separation is also discussed.
quote
| GB/T 7714-2015 | [1] XIAO Chao, WU Hai-guo. Theory and Current Research of Strontium and Barium Separation[J]. Rare Metals and Cemented Carbides, 2013(5): 10-14. |
| MLA | [1] XIAO Chao, and WU Hai-guo. "Theory and Current Research of Strontium and Barium Separation." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 10-14. |
| APA | [1] XIAO Chao, & WU Hai-guo. (2013). Theory and Current Research of Strontium and Barium Separation. Rare Metals and Cemented Carbides(5), 10-14. |
| IEEE | [1] XIAO Chao and WU Hai-guo, "Theory and Current Research of Strontium and Barium Separation," Rare Metals and Cemented Carbides, no. 5, pp. 10-14, 2013. keywords: {strontium;barium;separation;theory;characteristic purity strontium separation are re} |