Analysis of Causes for High Solid Content of Crude TiCl_4 Produced by Molten Salt Chlorination AITranslate
Abstract AITranslate
The causes are analyzed for high solid content of crude TICl4 produced by molten salt chlorination. It is pointed out the high solid content of crude TICl4 is caused mainly by raw materials,chlorination temperature and molten salt composition in the molten salt chlorination section, the temperature of dust collection chamber and chamber connection pattern in the dust collection section, scrubbing temperature and circulating pump tank allocation in the scrubbing section as well as the stirring rate and settlement time in the settlement section. The related countermeasures are discussed.
KeyWords AITranslate
1莫畏,邓国珠,罗方承.钛冶金[M].北京:冶金工业出版社,2007:164.
2阎守义.谈海绵钛生产的无筛板沸腾氯化与前苏联的熔盐氯化[J].轻金属,2011(S1):307-310. 被引量:6
3居殿春,卿阳,严定鎏,陈志勇,李向阳.氯化物熔盐中钙镁离子固化工艺的热力学分析[J].钢铁钒钛,2011,32(3):25-29. 被引量:9
4黄树杰.高钙镁钛渣熔盐氯化技术的研究与熔盐氯化炉大型化的探讨[J].钢铁钒钛,1989,10(4):45-54. 被引量:9
5李大成,周大利,刘恒.热力学汁算在海绵钛冶金中的应用[M].北京:冶金工业出版社.2009.54-56.
1杨天予,刘诚.我国粗TiCl_4生产工艺的进展[J].石油化工,2016,45(7):880-884. 被引量:3
2张苏新.熔盐氯化生产TiCl_4过程中固含量控制技术研究[J].钛工业进展,2018,35(5):42-46.
1刘汉国.干馏煤替代石油焦用于TiCl4生产的应用研究[J].有色金属:冶炼部分,2020(10):38-42.
2师家安.氯化炉制备四氯化钛综述及应用展望[J].有色金属设计,2021,48(2):34-37.
3马昕,师家安.大型熔盐氯化炉生产实践[J].有色金属设计,2022,49(1):40-44.
1卜相娟.通过对炮泥、泥炮及钻头的改进来改善对高炉出铁口的操作[J].耐火材料,2006,40(4):293-293.
2张苏新,杨仰军,陆平,刘森林,王云.含钛碳化高炉渣为原料制备TiCl_4试验研究[J].钢铁钒钛,2016,37(6):24-28. 被引量:7
3黄海辉,王云.提金渣氯化焙烧提取金银的试验[J].有色金属:冶炼部分,2009(6):46-48. 被引量:13
4王丽敏,薛楠.冶金标准样品的演变与发展[J].中国标准化,2011(4):27-31. 被引量:5
5黏性介质超滤盒系统[J].现代化工,2009(5):94-94.
6范晓慧,申炳昕,陈许玲,孙文东.烧结生产自动控制新技术(上)[J].烧结球团,2002,27(1):28-35. 被引量:14
7郭持皓,袁朝新,刘大学,胡磊.难处理金矿焙砂氯化挥发提金试验研究[J].矿冶,2016,25(3):37-40. 被引量:5
8肖泽辉,罗吉荣.镁合金铸造生产在我国的现状及其发展对策[J].轻金属,2004(2):43-45. 被引量:12
9赵玉龙,袁朝新,郭持皓,徐晓辉,韦其晋.熔融氯化法处理难处理金矿[J].矿冶,2016,25(6):32-34. 被引量:9
10孙明生.硫酸锌溶液冷却结晶除钙镁生产实践[J].中国有色冶金,2012,41(3):13-16. 被引量:13
Basic Information:
DOI:
Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]
Citation Information:
The causes are analyzed for high solid content of crude TICl4 produced by molten salt chlorination. It is pointed out the high solid content of crude TICl4 is caused mainly by raw materials,chlorination temperature and molten salt composition in the molten salt chlorination section, the temperature of dust collection chamber and chamber connection pattern in the dust collection section, scrubbing temperature and circulating pump tank allocation in the scrubbing section as well as the stirring rate and settlement time in the settlement section. The related countermeasures are discussed.
quote
| GB/T 7714-2015 | [1] LU Hui, YANG Ren-mu, MENG Jun, et al. Analysis of Causes for High Solid Content of Crude TiCl_4 Produced by Molten Salt Chlorination[J]. Rare Metals and Cemented Carbides, 2013(5): 5-9. |
| MLA | [1] LU Hui, et al., "Analysis of Causes for High Solid Content of Crude TiCl_4 Produced by Molten Salt Chlorination." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 5-9. |
| APA | [1] LU Hui, YANG Ren-mu, MENG Jun, SHI Sheng-dian, XIE Hong-yan, & XIE Gang. (2013). Analysis of Causes for High Solid Content of Crude TiCl_4 Produced by Molten Salt Chlorination. Rare Metals and Cemented Carbides(5), 5-9. |
| IEEE | [1] LU Hui, YANG Ren-mu, MENG Jun, SHI Sheng-dian, XIE Hong-yan, and XIE Gang, "Analysis of Causes for High Solid Content of Crude TiCl_4 Produced by Molten Salt Chlorination," Rare Metals and Cemented Carbides, no. 5, pp. 5-9, 2013. keywords: {molten salt chlorination;crude TICl4;high solid content;cause;countermeasure} |