Tough Hydrogel Coating on Silicone Rubber with Improved Antifouling and Antibacterial Properties AITranslate

Southeast University; Southeast University; Southeast University; Southeast University; Southeast University; Southeast University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Silicone rubber catheters have a wide range of medical applications. However, silicone rubber is subject to biofouling, biofilm formation, and microbial infection, which can decrease its success and performance because of lipophilicity. In this report, a tough hydrogel was grafted onto the surface of silicone rubber to endow it with antifouling and antibacterial properties. First of all, an acrylamide (AAm)-, 2-methacryloxyethyl phosphorylcholine (MPC)-, and zinc methacrylate (ZMA)-derived poly(AAm-MPC-ZMA) hydrogel was coated on the surface of silicone rubber mediated by a poly(vinyl acetate) (PVAc) primer layer. Second, the composition and hydrophilicity of the hydrogel-coated rubber were evaluated by X-ray photoelectron spectroscopy (XPS) and a contact angle analyzer. The results indicated the success of the poly(AAm-MPC-ZMA) hydrogel coating, inducing a decrease in the contact angle from 107.01 to 23.22°. Bovine serum albumin (BSA) was further used to test the nonspecific protein absorption of the modified silicone rubber. It was found that BSA deposition on the surface of silicone rubber decreased from 0.33 to 0.07 mg/cm2 after coating, indicating an antifouling effect. In addition, the incorporation of ZMA gave silicone rubber significant antibacterial properties against Pseudomonas aeruginosa, Staphylococcus aureus, and Escherichia coli. As a preliminary application test, a silicone rubber catheter was coated with the poly(AAm-MPC-ZMA) hydrogel, which showed improved hydrophilicity and reduced adhesion against biological soft tissues. Taken together, the poly(AAm-MPC-ZMA) hydrogel coating generated a highly hydrophilic silicone rubber with excellent antifouling and antibacterial properties, which has great potential in the application of medical catheters.

KeyWords AITranslate

silicone rubber hydrogel coating surface modification antifouling antibacterial property
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00069

Chinese Library Classification Number:

Citation Information:

Silicone rubber catheters have a wide range of medical applications. However, silicone rubber is subject to biofouling, biofilm formation, and microbial infection, which can decrease its success and performance because of lipophilicity. In this report, a tough hydrogel was grafted onto the surface of silicone rubber to endow it with antifouling and antibacterial properties. First of all, an acrylamide (AAm)-, 2-methacryloxyethyl phosphorylcholine (MPC)-, and zinc methacrylate (ZMA)-derived poly(AAm-MPC-ZMA) hydrogel was coated on the surface of silicone rubber mediated by a poly(vinyl acetate) (PVAc) primer layer. Second, the composition and hydrophilicity of the hydrogel-coated rubber were evaluated by X-ray photoelectron spectroscopy (XPS) and a contact angle analyzer. The results indicated the success of the poly(AAm-MPC-ZMA) hydrogel coating, inducing a decrease in the contact angle from 107.01 to 23.22°. Bovine serum albumin (BSA) was further used to test the nonspecific protein absorption of the modified silicone rubber. It was found that BSA deposition on the surface of silicone rubber decreased from 0.33 to 0.07 mg/cm2 after coating, indicating an antifouling effect. In addition, the incorporation of ZMA gave silicone rubber significant antibacterial properties against Pseudomonas aeruginosa, Staphylococcus aureus, and Escherichia coli. As a preliminary application test, a silicone rubber catheter was coated with the poly(AAm-MPC-ZMA) hydrogel, which showed improved hydrophilicity and reduced adhesion against biological soft tissues. Taken together, the poly(AAm-MPC-ZMA) hydrogel coating generated a highly hydrophilic silicone rubber with excellent antifouling and antibacterial properties, which has great potential in the application of medical catheters.

quote

GB/T 7714-2015 [1] Lei Cheng, Chao Liu, Ji Wang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00069.
MLA [1] Lei Cheng, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00069.
APA [1] Lei Cheng, Chao Liu, Ji Wang, Yang Wang, Wenhui Zha, & Xinsong Li. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00069
IEEE [1] Lei Cheng, Chao Liu, Ji Wang, Yang Wang, Wenhui Zha, and Xinsong Li, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00069. keywords: {silicone rubber;hydrogel coating;surface modification;antifouling;antibacterial property}