Chiral Bishelic[6]arene-Based Supramolecular Gels with Circularly Polarized Luminescence Property AITranslate

China|University of Chinese Academy of Sciences; Institute of Chemistry; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this work, a pair of enantiomeric bishelic[6]arenes (P/M-BH6) was synthesized and utilized to construct chiral supramolecular polymers with achiral luminescent guests through the host–guest interactions. The resulting linear supramolecular polymers could further self-assemble into supramolecular gels with enhanced emission. Moreover, the supramolecular gels with chiral and fluorescence properties exhibited circularly polarized luminescence (CPL) property induced by the chirality transfer from the chiral macrocyclic arene to the achiral guests. Furthermore, a kind of chiral supramolecular gel with white-light emission was conveniently obtained by regulating the ratio of the two achiral guests. This work provides a promising strategy to construct CPL-active supramolecular gels based on the chiral macrocyclic host–guest interactions.

KeyWords AITranslate

bishelic[6]arene host−guest interaction chirality transfer supramolecular gels circularly polarized luminescence
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00080

Chinese Library Classification Number:

Citation Information:

In this work, a pair of enantiomeric bishelic[6]arenes (P/M-BH6) was synthesized and utilized to construct chiral supramolecular polymers with achiral luminescent guests through the host–guest interactions. The resulting linear supramolecular polymers could further self-assemble into supramolecular gels with enhanced emission. Moreover, the supramolecular gels with chiral and fluorescence properties exhibited circularly polarized luminescence (CPL) property induced by the chirality transfer from the chiral macrocyclic arene to the achiral guests. Furthermore, a kind of chiral supramolecular gel with white-light emission was conveniently obtained by regulating the ratio of the two achiral guests. This work provides a promising strategy to construct CPL-active supramolecular gels based on the chiral macrocyclic host–guest interactions.

quote

GB/T 7714-2015 [1] Yan Guo, Ying Han, XuSheng Du, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00080.
MLA [1] Yan Guo, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00080.
APA [1] Yan Guo, Ying Han, XuSheng Du, & ChuanFeng Chen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00080
IEEE [1] Yan Guo, Ying Han, XuSheng Du, and ChuanFeng Chen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00080. keywords: {bishelic[6]arene;host−guest interaction;chirality transfer;supramolecular gels;circularly polarized luminescence}