daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Boron Cage Triggered Micellization of a Neutral–Cationic Block Copolymer and Preparation of Boron-Containing Layer-by-Layer Microparticles AITranslate

Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University; Middle East Technical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation of a polymer carrier for a boron delivery agent is presented through a combination of experimental and computational studies. A dodecahydro-closo-dodecaborate (B12H12)2– (B12) anion was used as a model boron-containing agent due to its high boron content. Quaternized poly(2-vinyl pyridine)-b-poly(ethylene oxide) (QP2VP-b-PEO) was chosen as a model neutral–cationic block copolymer to construct the carrier. The electrostatic association between QP2VP and B12 induced the self-assembly of QP2VP-b-PEO, resulting in micelles with (B12 + QP2VP)-core and PEO-corona. The mechanism of formation of (B12 + QP2VP)-b-PEO micelles was examined through density functional theory (DFT) calculations and classical simulations. (B12 + QP2VP)-b-PEO micelles were found to be undurable in biological medium. To enhance stability, micelles were utilized as building blocks together with poly(N-vinyl caprolactam) (PVCL) and tannic acid (TA) to construct layer-by-layer (LbL) microparticles. Cytotoxicity and cellular association of LbL particles were assessed using the HepG2 cell line. Multilayered particles were found to show no cellular cytotoxicity. Association studies and the boron content of treated cells through inductively coupled plasma optical emission spectroscopy (ICP-OES) showed that LbL microparticles were extensively associated with and successfully delivered boron to HepG2 cells. This study reveals the challenges and possible solutions to obtain stable self-assembled structures in a cell culture medium. These findings contribute to a fundamental understanding of the structure–property relationship in self-assembled micelles/LbL particles and provide a basis for further development of boron-containing polymer vehicles for boron neutron capture therapy.

KeyWords AITranslate

selfassembly layerbylayer technique block copolymer micelle boron delivery multilayer particles
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00060

Chinese Library Classification Number:

Citation Information:

The preparation of a polymer carrier for a boron delivery agent is presented through a combination of experimental and computational studies. A dodecahydro-closo-dodecaborate (B12H12)2– (B12) anion was used as a model boron-containing agent due to its high boron content. Quaternized poly(2-vinyl pyridine)-b-poly(ethylene oxide) (QP2VP-b-PEO) was chosen as a model neutral–cationic block copolymer to construct the carrier. The electrostatic association between QP2VP and B12 induced the self-assembly of QP2VP-b-PEO, resulting in micelles with (B12 + QP2VP)-core and PEO-corona. The mechanism of formation of (B12 + QP2VP)-b-PEO micelles was examined through density functional theory (DFT) calculations and classical simulations. (B12 + QP2VP)-b-PEO micelles were found to be undurable in biological medium. To enhance stability, micelles were utilized as building blocks together with poly(N-vinyl caprolactam) (PVCL) and tannic acid (TA) to construct layer-by-layer (LbL) microparticles. Cytotoxicity and cellular association of LbL particles were assessed using the HepG2 cell line. Multilayered particles were found to show no cellular cytotoxicity. Association studies and the boron content of treated cells through inductively coupled plasma optical emission spectroscopy (ICP-OES) showed that LbL microparticles were extensively associated with and successfully delivered boron to HepG2 cells. This study reveals the challenges and possible solutions to obtain stable self-assembled structures in a cell culture medium. These findings contribute to a fundamental understanding of the structure–property relationship in self-assembled micelles/LbL particles and provide a basis for further development of boron-containing polymer vehicles for boron neutron capture therapy.

quote

GB/T 7714-2015 [1] Umut Aydemir, Esma Ugur, Cagdas Ermis, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00060.
MLA [1] Umut Aydemir, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00060.
APA [1] Umut Aydemir, Esma Ugur, Cagdas Ermis, Fatma Nur Aydemir, Erhan Ozdemir, Sreeparna Banerjee, Erol Yildirim, Akin Akdag, & Irem ErelGoktepe. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00060
IEEE [1] Umut Aydemir, Esma Ugur, Cagdas Ermis, Fatma Nur Aydemir, Erhan Ozdemir, Sreeparna Banerjee, Erol Yildirim, Akin Akdag, and Irem ErelGoktepe, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00060. keywords: {selfassembly;layerbylayer technique;block copolymer micelle;boron delivery;multilayer particles}