Recent Advances in Real-Time Inkjet Monitoring Techniques Based on Piezo Self-Sensing Signals Recent Advances in Real-Time Inkjet Monitoring Techniques Based on Piezo Self-Sensing Signals AITranslate

Soonchunhyang University; Soonchunhyang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Inkjet technology has been used in the manufacturing process due to its high throughput using multiple nozzles for simultaneous jetting. However, not all nozzles are in good condition, and misfiring nozzles should be excluded from the printing process. Moreover, the condition of some nozzles may change even during the printing process. Thus, real-time monitoring of the whole nozzle status is one of the important issues in an inkjet-based manufacturing process. In this Spotlight, we discuss recent advances in real-time inkjet monitoring methods based on piezo self-sensing signals. To improve the monitoring algorithm and verify the proposed method, the analysis results of long-term jet behavior are presented. Based on scatter plots of more than 140,000 jetting cases, the influence of parameters on the reliability of monitoring was also investigated. Finally, the prospects for real-time inkjet monitoring techniques based on our current advances will be discussed.

KeyWords AITranslate

inkjet monitoring jet failures piezo selfsensing inkjet printing inkjet vision monitoring inkjet reliability printed electronics strobe LED
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01142

Chinese Library Classification Number:

Citation Information:

Inkjet technology has been used in the manufacturing process due to its high throughput using multiple nozzles for simultaneous jetting. However, not all nozzles are in good condition, and misfiring nozzles should be excluded from the printing process. Moreover, the condition of some nozzles may change even during the printing process. Thus, real-time monitoring of the whole nozzle status is one of the important issues in an inkjet-based manufacturing process. In this Spotlight, we discuss recent advances in real-time inkjet monitoring methods based on piezo self-sensing signals. To improve the monitoring algorithm and verify the proposed method, the analysis results of long-term jet behavior are presented. Based on scatter plots of more than 140,000 jetting cases, the influence of parameters on the reliability of monitoring was also investigated. Finally, the prospects for real-time inkjet monitoring techniques based on our current advances will be discussed.

quote

GB/T 7714-2015 [1] Sang Hyeon Park, KyeSi Kwon. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01142.
MLA [1] Sang Hyeon Park, and KyeSi Kwon. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01142.
APA [1] Sang Hyeon Park, & KyeSi Kwon. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01142
IEEE [1] Sang Hyeon Park and KyeSi Kwon, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01142. keywords: {inkjet monitoring jet failures piezo selfsensing inkjet printing inkjet vision monitoring inkjet reliability printed electronics strobe LED}