Dual-Band Electrochromic Smart Window Based on Single-Component Nanocrystals Dual-Band Electrochromic Smart Window Based on Single-Component Nanocrystals AITranslate

Guangxi University; Guangxi University; Guangxi University; Guangxi University; Guangxi University; Guangxi University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Building energy consumption has become one of the main sources of social primary energy consumption and global carbon emissions, and the development of building energy-saving technology has become one of the focus issues. Dual-band electrochromic smart windows (DESWs) can independently control the visible (VIS) light and near-infrared (NIR) thermal radiation in the sunlight, so that the indoor lighting and temperature can reach the level of human comfort, which is expected to reduce the energy consumption of buildings in heating, cooling, and artificial lighting systems. In recent years, DESWs based on single-component nanocrystals (NCs) have attracted much attention because of their facile construction method and excellent dual-band electrochromic performance. On the basis of the working mechanism of the DESWs, the spotlight article will first briefly introduce the basic principle and performance evaluation index of DESWs. Then the latest advances in DESWs based on typical single-component NCs are summarized. In addition, the challenges faced by DESWs based on single-component NCs and the potential development direction are also discussed.

KeyWords AITranslate

electrochromism smart windows nanocrystals dualband absorption green building
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01225

Chinese Library Classification Number:

Citation Information:

Building energy consumption has become one of the main sources of social primary energy consumption and global carbon emissions, and the development of building energy-saving technology has become one of the focus issues. Dual-band electrochromic smart windows (DESWs) can independently control the visible (VIS) light and near-infrared (NIR) thermal radiation in the sunlight, so that the indoor lighting and temperature can reach the level of human comfort, which is expected to reduce the energy consumption of buildings in heating, cooling, and artificial lighting systems. In recent years, DESWs based on single-component nanocrystals (NCs) have attracted much attention because of their facile construction method and excellent dual-band electrochromic performance. On the basis of the working mechanism of the DESWs, the spotlight article will first briefly introduce the basic principle and performance evaluation index of DESWs. Then the latest advances in DESWs based on typical single-component NCs are summarized. In addition, the challenges faced by DESWs based on single-component NCs and the potential development direction are also discussed.

quote

GB/T 7714-2015 [1] Yi Liang, Sheng Cao, Juquan Guo, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01225.
MLA [1] Yi Liang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01225.
APA [1] Yi Liang, Sheng Cao, Juquan Guo, Ruosheng Zeng, Jialong Zhao, & Bingsuo Zou. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01225
IEEE [1] Yi Liang, Sheng Cao, Juquan Guo, Ruosheng Zeng, Jialong Zhao, and Bingsuo Zou, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01225. keywords: {electrochromism smart windows nanocrystals dualband absorption green building}