Microtopography-Guided Chessboard-like Structure for a Broadband Terahertz Absorber Microtopography-Guided Chessboard-like Structure for a Broadband Terahertz Absorber AITranslate
Abstract AITranslate
Broadband absorber in the terahertz frequency is highly required for applications in imaging, detecting, and electromagnetic stealth. The limitations for developing the absorber are not only the complex geometric structure and multimaterials themselves but also the time-consuming, expensive, and inaccurate manufacturing. Herein, a chessboard-like structure with an alternate distribution of Ti and Si materials in the plane is proposed. This quite simple microscale structure exhibits a large absorption in the terahertz range, which can work as an efficient broadband absorber. To fabricate the absorber, we have proposed a microtopographic substrate-guided method which possesses low-cost and high accuracy capacities. Finally, the proposed absorber exhibits above 60% absorption in 0.1–4 THz, while larger than 75% absorption is achieved in 2.1–4 THz. The similarity of the experimental and simulated absorption is up to 92%. These performances could fulfill the requirements for the applications in electromagnetic stealth, terahertz imaging, and sensing in the future. It also indicates that the proposed fabrication method can be effectively applied in preparing terahertz microstructures and metamaterials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00325
Chinese Library Classification Number:
Citation Information:
Broadband absorber in the terahertz frequency is highly required for applications in imaging, detecting, and electromagnetic stealth. The limitations for developing the absorber are not only the complex geometric structure and multimaterials themselves but also the time-consuming, expensive, and inaccurate manufacturing. Herein, a chessboard-like structure with an alternate distribution of Ti and Si materials in the plane is proposed. This quite simple microscale structure exhibits a large absorption in the terahertz range, which can work as an efficient broadband absorber. To fabricate the absorber, we have proposed a microtopographic substrate-guided method which possesses low-cost and high accuracy capacities. Finally, the proposed absorber exhibits above 60% absorption in 0.1–4 THz, while larger than 75% absorption is achieved in 2.1–4 THz. The similarity of the experimental and simulated absorption is up to 92%. These performances could fulfill the requirements for the applications in electromagnetic stealth, terahertz imaging, and sensing in the future. It also indicates that the proposed fabrication method can be effectively applied in preparing terahertz microstructures and metamaterials.
quote
| GB/T 7714-2015 | [1] Tong Li, Hang Chen, HongAn Sun, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00325. |
| MLA | [1] Tong Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00325. |
| APA | [1] Tong Li, Hang Chen, HongAn Sun, Xiaotao Yang, Xiaoguang Sun, Yongchun Shangguan, Zhenlong Wang, & Jia Zhang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00325 |
| IEEE | [1] Tong Li, Hang Chen, HongAn Sun, Xiaotao Yang, Xiaoguang Sun, Yongchun Shangguan, Zhenlong Wang, and Jia Zhang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00325. keywords: {terahertz broadband absorber chessboardlike structure microtopographic substrate multimaterial alternate distribution} |