daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hf0.5Zr0.5O2-Based Germanium Ferroelectric p-FETs for Nonvolatile Memory Applications Hf0.5Zr0.5O2-Based Germanium Ferroelectric p-FETs for Nonvolatile Memory Applications AITranslate

National and Kapodistrian University of Athens;National Centre for Scientific Research “Demokritos”, 15310 Athens; National and Kapodistrian University of Athens;National Centre for Scientific Research “Demokritos”, 15310 Athens;National Centre for Scientific Research “Demokritos”, 15310 Athens
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ferroelectric field-effect transistors (FeFETs) with a TiN/Hf0.5Zr0.5O2 (HZO) gate stack on a germanium p-type channel are fabricated as low-voltage nonvolatile memory (NVM) devices. The clean HZO/Ge interfaces and the absence of a typical passivation oxide layer resulted in stable and robust ferroelectricity without a severe wake-up effect. The impact of unpassivated interfacial defect states on a germanium surface on the functionality of transistors is examined. The ferroelectric field effect is clearly observed and remains during electric field cycling at least until 5 × 104 cycles. With the optimum measurement conditions the memory window is 0.55 V. Retention measurements up to 104 s show a small reduction to 0.5 V, and from data projection it is inferred that the devices are not expected to fail before 10 years. These first results of HZO-based Ge-FeFETs are promising for the realization of a gate-first process and reduced total thermal budget. The lower dopant activation annealing of Ge at ∼600 °C in comparison with Si at temperatures greater than 1000 °C is compatible with the crystallization annealing of HZO, and thus the two annealing processes occur simultaneously in one step.

KeyWords AITranslate

ferroelectric fieldeffect transistor germanium pFET hafnium zirconium oxide nonvolatile memory electrical endurance retention
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00324

Chinese Library Classification Number:

Citation Information:

Ferroelectric field-effect transistors (FeFETs) with a TiN/Hf0.5Zr0.5O2 (HZO) gate stack on a germanium p-type channel are fabricated as low-voltage nonvolatile memory (NVM) devices. The clean HZO/Ge interfaces and the absence of a typical passivation oxide layer resulted in stable and robust ferroelectricity without a severe wake-up effect. The impact of unpassivated interfacial defect states on a germanium surface on the functionality of transistors is examined. The ferroelectric field effect is clearly observed and remains during electric field cycling at least until 5 × 104 cycles. With the optimum measurement conditions the memory window is 0.55 V. Retention measurements up to 104 s show a small reduction to 0.5 V, and from data projection it is inferred that the devices are not expected to fail before 10 years. These first results of HZO-based Ge-FeFETs are promising for the realization of a gate-first process and reduced total thermal budget. The lower dopant activation annealing of Ge at ∼600 °C in comparison with Si at temperatures greater than 1000 °C is compatible with the crystallization annealing of HZO, and thus the two annealing processes occur simultaneously in one step.

quote

GB/T 7714-2015 [1] Christina Zacharaki, Stefanos Chaitoglou, Nikitas Siannas, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00324.
MLA [1] Christina Zacharaki, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00324.
APA [1] Christina Zacharaki, Stefanos Chaitoglou, Nikitas Siannas, Polychronis Tsipas, & Athanasios Dimoulas. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00324
IEEE [1] Christina Zacharaki, Stefanos Chaitoglou, Nikitas Siannas, Polychronis Tsipas, and Athanasios Dimoulas, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00324. keywords: {ferroelectric fieldeffect transistor germanium pFET hafnium zirconium oxide nonvolatile memory electrical endurance retention}