Abstract AITranslate

Stretchable conductors are of crucial relevance for emerging technologies such as wearable electronics, low-invasive bioelectronic implants, or soft actuators for robotics. A critical issue for their development regards the understanding of defect formation and fracture of conducting pathways during stress–strain cycles. Here we present a combination of atomic force microscopy (AFM) methods that provides multichannel images of surface morphology, conductivity, and elastic modulus during sample deformation. To develop the method, we investigate in detail the mechanical interactions between the AFM tip and a stretched, free-standing thin film sample. Our findings reveal the conditions to avoid artifacts related to sample bending modes or resonant excitations. As an example, we analyze strain effects in thin gold films deposited on a soft silicone substrate. Our technique allows one to observe the details of microcrack opening during tensile strain and their impact on local current transport and surface mechanics. We find that although the film fractures into separate fragments, at higher strain a current transport is sustained by a tunneling mechanism. The microscopic observation of local defect formation and their correlation to local conductivity will provide insight into the design of more robust and fatigue resistant stretchable conductors.

KeyWords AITranslate

stretchable conductors in situ AFM fracture local conductivity hard on soft
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00328

Chinese Library Classification Number:

Citation Information:

Stretchable conductors are of crucial relevance for emerging technologies such as wearable electronics, low-invasive bioelectronic implants, or soft actuators for robotics. A critical issue for their development regards the understanding of defect formation and fracture of conducting pathways during stress–strain cycles. Here we present a combination of atomic force microscopy (AFM) methods that provides multichannel images of surface morphology, conductivity, and elastic modulus during sample deformation. To develop the method, we investigate in detail the mechanical interactions between the AFM tip and a stretched, free-standing thin film sample. Our findings reveal the conditions to avoid artifacts related to sample bending modes or resonant excitations. As an example, we analyze strain effects in thin gold films deposited on a soft silicone substrate. Our technique allows one to observe the details of microcrack opening during tensile strain and their impact on local current transport and surface mechanics. We find that although the film fractures into separate fragments, at higher strain a current transport is sustained by a tunneling mechanism. The microscopic observation of local defect formation and their correlation to local conductivity will provide insight into the design of more robust and fatigue resistant stretchable conductors.

quote

GB/T 7714-2015 [1] Giorgio Cortelli, Luca Patruno, Tobias Cramer, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00328.
MLA [1] Giorgio Cortelli, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00328.
APA [1] Giorgio Cortelli, Luca Patruno, Tobias Cramer, Beatrice Fraboni, & Stefano de Miranda. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00328
IEEE [1] Giorgio Cortelli, Luca Patruno, Tobias Cramer, Beatrice Fraboni, and Stefano de Miranda, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00328. keywords: {stretchable conductors in situ AFM fracture local conductivity hard on soft}